公开(公告)号:DK0679170T3
公开(公告)日:2000-09-18
申请号:DK95901945
申请日:1994-11-16
Applicant: BAXTER INT
Inventor: LING MICHAEL T K , LAURIN DEAN , ROSENBAUM LARRY A , ANDERSON WILLIAM , BUAN ANGELES LILLIAN , DING YUAN-PANG SAMUEL , HAYWARD DENISE S , HOPPESCH JOSEPH P , NEBGEN GREGG , WESTPHAL STANLEY , WOO LECON
IPC: A61L27/00 , A61L31/00 , C08L23/02 , C08L23/06 , C08L23/08 , C08L23/10 , C08L23/16 , C08L23/20 , C08L23/26 , C08L29/04 , C08L31/04 , C08L51/06 , C08L53/00 , C08L53/02 , C08L67/00 , C08L75/00 , C08L77/00 , C08L101/00 , C08L101/12
Abstract: A polymer based composition for fabricating into articles is described. The composition comprises: a polypropylene in an amount by weight from 40-90% of the composition and having a melting temperature greater than 130 DEG C; a radio frequency susceptible polymer in an amount by weight from 5-50% of the composition and having a dielectric loss greater than 0.05 at 1-60 MHz and ambient temperature to 250 DEG C, the susceptible polymer being selected from (1) polymers containing at least one segment selected from the group consisting of urethanes, esters, ureas, imides, sulfones, and amides, and (2) ethylene copolymers having 50-85% ethylene content copolymerized with at least one monomer selected from the group consisting of acrylic acid, methacrylic acid, ester derivatives of acrylic acid with alcohols having 1-10 carbons, vinyl acetate, and vinyl alcohol; a compatibilizing polymer in an amount by weight from 5-30% of the composition, the compatibilizing polymer conferring compatibility between the radio frequency susceptible polymer, and the polypropylene, the compatibilizing polymer being a styrenic block copolymer with hydrocarbon soft segments, and wherein the composition has an optical haze value of less than 30% for the composition processed into a film of about 0.299 mm in thickness measured in accordance to ASTM D-1003, a mechanical modulus of less than 2758x10 Pa when measured according to ASTM D-882 and the composition exhibits no strain whitening after being strained at moderate speeds of about 50 cm per minute to about 100% elongation.
-
公开(公告)号:DK0679124T3
公开(公告)日:1999-08-30
申请号:DK95902620
申请日:1994-11-16
Applicant: BAXTER INT
Inventor: WOO LECON , LING MICHAEL T K , LAURIN DEAN , ROSENBAUM LARRY A , ANDERSON WILLIAM , BUAN ANGELES LILLIAN , DING YUAN-PANG SAMUEL , HAYWARD DENISE S , HOPPESCH JOSEPH P , NEBGEN GREGG , WESTPHAL STANLEY
IPC: A23L7/10 , A23L7/196 , A61L31/00 , B32B27/08 , B32B27/32 , C08L23/08 , C08L23/10 , C08L25/04 , C08L53/00 , C08L53/02
Abstract: A multiple layer structure comprising a skin layer composed of a polypropylene copolymer with styrene ethylene-butene styrene block copolymer within a range of 0-20% by weight skin layer, and, a radio frequency ("RF") susceptible layer adhered to the skin layer. The RF layer has a first component of a propylene based polymer, a second component of a nonpropylene polyolefin, a third component of a radio frequency susceptible polymer, and a fourth component of a polymeric compatibilizing agent.
-
公开(公告)号:DE69415792T2
公开(公告)日:1999-08-19
申请号:DE69415792
申请日:1994-11-16
Applicant: BAXTER INT
Inventor: ROSENBAUM LARRY , ANDERSON WILLIAM , WOO LECON , LAURIN DEAN , BUAN ANGELES , LING MICHAEL , DING YUAN-PANG , HAYWARD DENISE , HOPPESCH JOSEPH , NEBGEN GREGG , WESTPHAL STANLEY
IPC: A23L7/10 , A23L7/196 , A61L31/00 , B32B27/08 , B32B27/32 , C08L23/08 , C08L23/10 , C08L25/04 , C08L53/00 , C08L53/02
Abstract: A multiple layer structure comprising a skin layer composed of a polypropylene copolymer with styrene ethylene-butene styrene block copolymer within a range of 0-20% by weight skin layer, and, a radio frequency ("RF") susceptible layer adhered to the skin layer. The RF layer has a first component of a propylene based polymer, a second component of a nonpropylene polyolefin, a third component of a radio frequency susceptible polymer, and a fourth component of a polymeric compatibilizing agent.
-
公开(公告)号:HK1002389A1
公开(公告)日:1998-08-21
申请号:HK98101229
申请日:1998-02-17
Applicant: BAXTER INT
Inventor: ROSENBAUM LARRY A , ANDERSON WILLIAM , WOO LECON , LAURIN DEAN , BUAN ANGELES LILLIAN , LING MICHAEL T K , DING YUAN-PANG SAMUEL , HAYWARD DENISE S , HOPPESCH JOSEPH P , NEBGEN GREGG , WESTPHAL STANLEY
IPC: A23L7/10 , A61L31/00 , A23L7/196 , B32B27/08 , B32B27/32 , C08L23/08 , C08L23/10 , C08L25/04 , C08L53/00 , C08L53/02 , B32B
Abstract: A multiple layer structure comprising a skin layer composed of a polypropylene copolymer with styrene ethylene-butene styrene block copolymer within a range of 0-20% by weight skin layer, and, a radio frequency ("RF") susceptible layer adhered to the skin layer. The RF layer has a first component of a propylene based polymer, a second component of a nonpropylene polyolefin, a third component of a radio frequency susceptible polymer, and a fourth component of a polymeric compatibilizing agent.
-
公开(公告)号:NO952802L
公开(公告)日:1995-09-15
申请号:NO952802
申请日:1995-07-14
Applicant: BAXTER INT
Inventor: LAURIN DEAN , BUAN ANGELES LILLIAN , WOO LECON , LING MICHAEL T K , DING YUAN-PANG SAMUEL , ANDERSON WILLIAM , ROSENBAUM LARRY A , HAYWARD DENISE S , HOPPESCH JOSEPH P , NEBGEN GREGG , WESTPHAL STANLEY
IPC: A23L7/10 , A23L7/196 , A61L31/00 , B32B27/08 , B32B27/32 , C08L23/08 , C08L23/10 , C08L25/04 , C08L53/00 , C08L53/02
Abstract: A multiple layer structure comprising a skin layer composed of a polypropylene copolymer with styrene ethylene-butene styrene block copolymer within a range of 0-20% by weight skin layer, and, a radio frequency ("RF") susceptible layer adhered to the skin layer. The RF layer has a first component of a propylene based polymer, a second component of a nonpropylene polyolefin, a third component of a radio frequency susceptible polymer, and a fourth component of a polymeric compatibilizing agent.
-
公开(公告)号:ZA9408816B
公开(公告)日:1995-07-11
申请号:ZA9408816
申请日:1994-11-08
Applicant: BAXTER INT
Inventor: LAURIN DEAN , BUAN ANGELA LILLIAN , WOO LECON , LING MICHAEL T K , DING YUAN-PANG SAMUEL , ANDERSON WILLIAM , ROSENBAUM LARRY A , HAYWARD DENISE S , HOPPESCH JOSEPH P , NEBGEN GREGG , WESTPHAL STANLEY
IPC: A61L27/00 , A61L31/00 , C08L23/02 , C08L23/06 , C08L23/08 , C08L23/10 , C08L23/16 , C08L23/20 , C08L23/26 , C08L29/04 , C08L31/04 , C08L51/06 , C08L53/00 , C08L53/02 , C08L67/00 , C08L75/00 , C08L77/00 , C08L101/00 , C08L101/12 , C08L
CPC classification number: C08L23/02 , C08L23/0815 , C08L23/0846 , C08L23/0853 , C08L23/0869 , C08L23/10 , C08L51/06 , C08L53/00 , C08L53/02 , C08L77/00 , C08L101/00 , C08L2203/02 , C08L2205/08 , C08L2666/04 , C08L2666/20 , C08L2666/14 , C08L2666/24 , C08L2666/02
-
公开(公告)号:DE69425649T2
公开(公告)日:2001-04-19
申请号:DE69425649
申请日:1994-11-16
Applicant: BAXTER INT
Inventor: LAURIN DEAN , BUAN LILLIAN , WOO LECON , LING T , DING SAMUEL , ANDERSON WILLIAM , ROSENBAUM A , HAYWARD S , HOPPESCH P , NEBGEN GREGG , WESTPHAL STANLEY
IPC: A61L27/00 , A61L31/00 , C08L23/02 , C08L23/06 , C08L23/08 , C08L23/10 , C08L23/16 , C08L23/20 , C08L23/26 , C08L29/04 , C08L31/04 , C08L51/06 , C08L53/00 , C08L53/02 , C08L67/00 , C08L75/00 , C08L77/00 , C08L101/00 , C08L101/12
Abstract: A polymer based composition for fabricating into articles is described. The composition comprises: a polypropylene in an amount by weight from 40-90% of the composition and having a melting temperature greater than 130 DEG C; a radio frequency susceptible polymer in an amount by weight from 5-50% of the composition and having a dielectric loss greater than 0.05 at 1-60 MHz and ambient temperature to 250 DEG C, the susceptible polymer being selected from (1) polymers containing at least one segment selected from the group consisting of urethanes, esters, ureas, imides, sulfones, and amides, and (2) ethylene copolymers having 50-85% ethylene content copolymerized with at least one monomer selected from the group consisting of acrylic acid, methacrylic acid, ester derivatives of acrylic acid with alcohols having 1-10 carbons, vinyl acetate, and vinyl alcohol; a compatibilizing polymer in an amount by weight from 5-30% of the composition, the compatibilizing polymer conferring compatibility between the radio frequency susceptible polymer, and the polypropylene, the compatibilizing polymer being a styrenic block copolymer with hydrocarbon soft segments, and wherein the composition has an optical haze value of less than 30% for the composition processed into a film of about 0.299 mm in thickness measured in accordance to ASTM D-1003, a mechanical modulus of less than 2758x10 Pa when measured according to ASTM D-882 and the composition exhibits no strain whitening after being strained at moderate speeds of about 50 cm per minute to about 100% elongation.
-
公开(公告)号:AT195754T
公开(公告)日:2000-09-15
申请号:AT95901945
申请日:1994-11-16
Applicant: BAXTER INT
Inventor: LAURIN DEAN , BUAN ANGELES LILLIAN , WOO LECON , LING MICHAEL T K , DING YUAN-PANG SAMUEL , ANDERSON WILLIAM , ROSENBAUM LARRY A , HAYWARD DENISE S , HOPPESCH JOSEPH P , NEBGEN GREGG , WESTPHAL STANLEY
IPC: A61L27/00 , A61L31/00 , C08L23/02 , C08L23/06 , C08L23/08 , C08L23/10 , C08L23/16 , C08L23/20 , C08L23/26 , C08L29/04 , C08L31/04 , C08L51/06 , C08L53/00 , C08L53/02 , C08L67/00 , C08L75/00 , C08L77/00 , C08L101/00 , C08L101/12
Abstract: A polymer based composition for fabricating into articles is described. The composition comprises: a polypropylene in an amount by weight from 40-90% of the composition and having a melting temperature greater than 130 DEG C; a radio frequency susceptible polymer in an amount by weight from 5-50% of the composition and having a dielectric loss greater than 0.05 at 1-60 MHz and ambient temperature to 250 DEG C, the susceptible polymer being selected from (1) polymers containing at least one segment selected from the group consisting of urethanes, esters, ureas, imides, sulfones, and amides, and (2) ethylene copolymers having 50-85% ethylene content copolymerized with at least one monomer selected from the group consisting of acrylic acid, methacrylic acid, ester derivatives of acrylic acid with alcohols having 1-10 carbons, vinyl acetate, and vinyl alcohol; a compatibilizing polymer in an amount by weight from 5-30% of the composition, the compatibilizing polymer conferring compatibility between the radio frequency susceptible polymer, and the polypropylene, the compatibilizing polymer being a styrenic block copolymer with hydrocarbon soft segments, and wherein the composition has an optical haze value of less than 30% for the composition processed into a film of about 0.299 mm in thickness measured in accordance to ASTM D-1003, a mechanical modulus of less than 2758x10 Pa when measured according to ASTM D-882 and the composition exhibits no strain whitening after being strained at moderate speeds of about 50 cm per minute to about 100% elongation.
-
公开(公告)号:GR3029456T3
公开(公告)日:1999-05-28
申请号:GR990400541
申请日:1999-02-19
Applicant: BAXTER INT
Inventor: ROSENBAUM LARRY A , ANDERSON WILLIAM , WOO LECON , LAURIN DEAN , BUAN ANGELES LILLIAN , LING MICHAEL T K , DING YUAN-PANG SAMUEL , HAYWARD DENISE S , HOPPESCH JOSEPH P , NEBGEN GREGG , WESTPHAL STANLEY
IPC: A23L7/10 , A23L7/196 , A61L31/00 , B32B27/08 , B32B27/32 , C08L23/08 , C08L23/10 , C08L25/04 , C08L53/00 , C08L53/02
Abstract: A multiple layer structure comprising a skin layer composed of a polypropylene copolymer with styrene ethylene-butene styrene block copolymer within a range of 0-20% by weight skin layer, and, a radio frequency ("RF") susceptible layer adhered to the skin layer. The RF layer has a first component of a propylene based polymer, a second component of a nonpropylene polyolefin, a third component of a radio frequency susceptible polymer, and a fourth component of a polymeric compatibilizing agent.
-
公开(公告)号:AT175383T
公开(公告)日:1999-01-15
申请号:AT95902620
申请日:1994-11-16
Applicant: BAXTER INT
Inventor: ROSENBAUM LARRY A , ANDERSON WILLIAM , WOO LECON , LAURIN DEAN , BUAN ANGELES LILLIAN , LING MICHAEL T K , DING YUAN-PANG SAMUEL , HAYWARD DENISE S , HOPPESCH JOSEPH P , NEBGEN GREGG , WESTPHAL STANLEY
IPC: A61L31/00 , A23L7/10 , A23L7/196 , B32B27/08 , B32B27/32 , C08L23/08 , C08L23/10 , C08L25/04 , C08L53/00 , C08L53/02
Abstract: A multiple layer structure comprising a skin layer composed of a polypropylene copolymer with styrene ethylene-butene styrene block copolymer within a range of 0-20% by weight skin layer, and, a radio frequency ("RF") susceptible layer adhered to the skin layer. The RF layer has a first component of a propylene based polymer, a second component of a nonpropylene polyolefin, a third component of a radio frequency susceptible polymer, and a fourth component of a polymeric compatibilizing agent.
-
-
-
-
-
-
-
-
-