    Abstract: The present invention provides a method for connecting rounded members between planar members comprising the steps of providing a rounded member having an outer layer having a first melting temperature range and an inner layer concentrically disposed within the outer layer and having a second melting temperature range, the second melting temperature range being warmer than the first melting temperature range, providing a pair of opposed planar members, the planar members each having a melting temperature within the first melting temperature range, positioning an end portion of the rounded member between perimeter edges of the pair of planar members to define an interface area, applying pressure to the interface area to collapse the end portion of the rounded member to essentially a flattened position, applying sealing energy to the interface area to heat the rounded member to a temperature within the first melting temperature range but below the second melting temperature range, thereby forming a weld between the planar members, and the rounded member in the interface area, and, releasing the pressure to the interface area wherein the end portion of the rounded member returns to an open position.

    3.
    发明专利
    未知

    公开(公告)号:DE69713051T2

    公开(公告)日:2003-01-23

    申请号:DE69713051

    申请日:1997-07-01

    Applicant: BAXTER INT

    Abstract: The present invention provides a method for connecting rounded members between planar members comprising the steps of providing a rounded member having an outer layer having a first melting temperature range and an inner layer concentrically disposed within the outer layer and having a second melting temperature range, the second melting temperature range being warmer than the first melting temperature range, providing a pair of opposed planar members, the planar members each having a melting temperature within the first melting temperature range, positioning an end portion of the rounded member between perimeter edges of the pair of planar members to define an interface area, applying pressure to the interface area to collapse the end portion of the rounded member to essentially a flattened position, applying sealing energy to the interface area to heat the rounded member to a temperature within the first melting temperature range but below the second melting temperature range, thereby forming a weld between the planar members, and the rounded member in the interface area, and, releasing the pressure to the interface area wherein the end portion of the rounded member returns to an open position.

    7.
    发明专利
    未知

    公开(公告)号:DE69425649T2

    公开(公告)日:2001-04-19

    申请号:DE69425649

    申请日:1994-11-16

    Applicant: BAXTER INT

    Abstract: A polymer based composition for fabricating into articles is described. The composition comprises: a polypropylene in an amount by weight from 40-90% of the composition and having a melting temperature greater than 130 DEG C; a radio frequency susceptible polymer in an amount by weight from 5-50% of the composition and having a dielectric loss greater than 0.05 at 1-60 MHz and ambient temperature to 250 DEG C, the susceptible polymer being selected from (1) polymers containing at least one segment selected from the group consisting of urethanes, esters, ureas, imides, sulfones, and amides, and (2) ethylene copolymers having 50-85% ethylene content copolymerized with at least one monomer selected from the group consisting of acrylic acid, methacrylic acid, ester derivatives of acrylic acid with alcohols having 1-10 carbons, vinyl acetate, and vinyl alcohol; a compatibilizing polymer in an amount by weight from 5-30% of the composition, the compatibilizing polymer conferring compatibility between the radio frequency susceptible polymer, and the polypropylene, the compatibilizing polymer being a styrenic block copolymer with hydrocarbon soft segments, and wherein the composition has an optical haze value of less than 30% for the composition processed into a film of about 0.299 mm in thickness measured in accordance to ASTM D-1003, a mechanical modulus of less than 2758x10 Pa when measured according to ASTM D-882 and the composition exhibits no strain whitening after being strained at moderate speeds of about 50 cm per minute to about 100% elongation.

    10.
    发明专利
    未知

    公开(公告)号:DE69425649D1

    公开(公告)日:2000-09-28

    申请号:DE69425649

    申请日:1994-11-16

    Applicant: BAXTER INT

    Abstract: A polymer based composition for fabricating into articles is described. The composition comprises: a polypropylene in an amount by weight from 40-90% of the composition and having a melting temperature greater than 130 DEG C; a radio frequency susceptible polymer in an amount by weight from 5-50% of the composition and having a dielectric loss greater than 0.05 at 1-60 MHz and ambient temperature to 250 DEG C, the susceptible polymer being selected from (1) polymers containing at least one segment selected from the group consisting of urethanes, esters, ureas, imides, sulfones, and amides, and (2) ethylene copolymers having 50-85% ethylene content copolymerized with at least one monomer selected from the group consisting of acrylic acid, methacrylic acid, ester derivatives of acrylic acid with alcohols having 1-10 carbons, vinyl acetate, and vinyl alcohol; a compatibilizing polymer in an amount by weight from 5-30% of the composition, the compatibilizing polymer conferring compatibility between the radio frequency susceptible polymer, and the polypropylene, the compatibilizing polymer being a styrenic block copolymer with hydrocarbon soft segments, and wherein the composition has an optical haze value of less than 30% for the composition processed into a film of about 0.299 mm in thickness measured in accordance to ASTM D-1003, a mechanical modulus of less than 2758x10 Pa when measured according to ASTM D-882 and the composition exhibits no strain whitening after being strained at moderate speeds of about 50 cm per minute to about 100% elongation.

Patent Agency Ranking