Abstract:
A thermoplastic polyester composition suitable for producing films or fibers excellent in wear resistance, and a biaxially oriented polyester film made therefrom. The composition comprises (A) a thermoplastic polyester and (B) monoclinic and/or tetragonal zirconium oxide particles.
Abstract:
A polyester resin composition which exhibits a reduced amount of production of the acid component monomer and/or oligomers of the polyester is provided. In other words, the object of the present invention is achieved by the following means. (1) A polyester resin composition, wherein the surface roughness Ra of a capture plate is less than 0.150 ?m, as measured when a sample of the polyester resin composition is melt at 300?C for 60 minutes under a nitrogen atmosphere, quickly cooled and thermally treated at 220?C for 8 hours to form scattered products which are then attached to the capture plate. (2) A polyester resin composition, wherein the production rate of an acid component monomer and/or the production rate of oligomers is/are less than 0.70, as defined by the following formulas ( I) and (II): Production rate of acid component monomer = (amount of produced acid component monomer)/(acid component monomer content) (I) Production rate of oligomers = (amount of produced oligomers)/(oligomer content) (II). (3) A method for producing a polyester resin composition, wherein an ionic liquid is added. [Selected Drawing] None
Abstract:
Provided is a polyester resin composition in which the amount of acid-component monomer and/or oligomer produced in the polyester is reduced. That is to say, the purpose of the present invention is achieved by the following means: (1) a polyester resin composition characterized in that, after rapidly cooling a sample that has been melted in a nitrogen atmosphere at 300oC for 60 minutes, the surface roughness Ra of a collecting plate to which scattered matter has attached during 8 hours of heat treatment at 220oC is less than 0.150 mm; (2) a polyester resin composition characterized in that the acid-component monomer production rate and/or the oligomer production rate defined by formulas (I) and (II) below is less than 0.70; and (3) a method of producing a polyester resin composition characterized by adding an ionic liquid. Formula (I): acid-component monomer production rate = (amount of acid-component monomer produced)/(acid-component monomer content) Formula (II): oligomer production rate = (amount of oligomer produced)/(oligomer content)
Abstract:
Una composición de resina de poliéster que comprende un fosfato de metal alcalino en una cantidad de 1,5 mol/t a 3,0 mol/t, y ácido fosfórico en una cantidad de 0,4 a 1,5 veces (en moles) la del fosfato de metal alcalino, en donde el poliéster de la composición de resina de poliéster es poli(tereftalato de etileno).
Abstract:
A thermoplastic polyester composition suitable for producing films or fibers excellent in wear resistance, and a biaxially oriented polyester film made therefrom. The composition comprises (A) a thermoplastic polyester and (B) monoclinic and/or tetragonal zirconium oxide particles.
Abstract:
Provided is a polylactic acid-based film composed of a composition comprising a resin (A), a resin (B) and a plasticizer (C), wherein the resin (A) is a polylactic acid-based resin and the resin (B) is an aliphatic polyester-based resin that are not polylactic acid-based resins and/or an aliphatic-aromatic polyester-based resin, which polylactic acid-based film exhibits at least one crystallization peak in the temperature range of 105°C to 160°C when cooled from a molten state at a rate of 20°C/min by a differential scanning calorimeter and satisfies the following condition when the total calorific value of the crystallization peak(s) in the temperature range of 105°C to 160°C is defined as ”Hmc A :
Abstract:
A polyester resin composition having an equivalent spherical diameter of 1 mm to 50 mm, a degree of crystallization of not less than 65% and less than 99%, an intrinsic viscosity of not more than 0.7 dl/g and a cyclic trimer content of not more than 0.4% by weight. This polymer resin composition has an excellent color tone, causes no significant viscosity lowering or viscosity rise, and can withstand a process which is exposed to a long-term thermal history. A polyester resin composition having a viscosity suitable for extrusion in a general-purpose manner, a production process thereof, and a polyester film are also provided.
Abstract:
The invention provides a porous film including a polylactic acid based resin (A), a thermoplastic resin (B) that is not a polylactic acid based resin, and a filler (C), wherein resin (A) and resin (B) account for 10 to 95 mass% and 5 to 90 mass%, respectively, of the sum total 100 mass% of resin (A) and resin (B), while the filler (C) accounts for 1 to 400 parts by mass of the sum total 100 parts by mass of resin (A) and resin (B), with the porosity being 1 to 80%. The present invention provides a polylactic acid based porous film that has high flexibility, moisture permeability, heat resistance, and bleed-out resistance.
Abstract:
The present invention relates to a retardation film using polyester having a photoelastic coefficient of -40×10 -12 Pa -1 to 40×10 -12 Pa -1 . The present invention also relates to a polyester resin for optical use which contains a phosphorus compound, and an alicyclic component and a fluorene derivative component as constituents, and satisfies the following equations (6) and (7): 100 �¢ °C ‰ glass transition temperature ‰ 150 �¢ °C and 1.0 ‰ Ma / 2 + Mb + Mc / P ‰ 5.0 wherein Ma is the number of moles of an alkali metal element contained in 1 ton of the polyester resin, Mb is the number of moles of an alkaline earth metal element contained in 1 ton of the polyester resin, Mc is the sum of the number of moles of a zinc element (Zn), a cobalt element (Co) and a manganese element (Mn) contained in 1 ton of the polyester resin, and P is the number of moles of a phosphorus element contained in 1 ton of the polyester resin.