미끄럼방지용 포장재 조성물
    21.
    发明授权
    미끄럼방지용 포장재 조성물 失效
    防滑组合物

    公开(公告)号:KR101022197B1

    公开(公告)日:2011-03-16

    申请号:KR1020100049041

    申请日:2010-05-26

    Inventor: 설태윤

    CPC classification number: C09D133/12 C08L23/00 C08L23/26 C09D1/00 E01C11/24

    Abstract: PURPOSE: An anti-slip pavement composition is provided to ensure excellent skid resistance and penetrability inside pores of concrete, and to prevent accidents and the degradation of shock resistance, discoloration by ultraviolet rays. CONSTITUTION: An anti-slip pavement composition comprises 25-45 weight% of modified methyl methacrylate resin, 30-45 weight% of one or more aggregates, 15-30 weight% of at least one filler, 3-10 weight% of functional filler, 2-5 weight% of sieved pigment, and 1-2 weight% of wax. The modified methyl methacrylate resin is prepared by mixing 3-15 weight% of thermoplastic elastomer and/or modified polypropylene to a resin in which 80-20 weight% of methylmethacrylate and 20-80 weight% of ethylacrylate are mixed; and adding .5-2 weight% of curing accelerators to the mixture.

    Abstract translation: 目的:提供防滑路面组合物,以确保混凝土孔隙内优异的抗滑性和渗透性,并防止事故和抗震性降解,紫外线变色。 构成:防滑路面组合物包含25-45重量%的改性甲基丙烯酸甲酯树脂,30-45重量%的一种或多种聚集体,15-30重量%的至少一种填料,3-10重量%的功能填料 ,2-5重量%的过筛颜料和1-2重量%的蜡。 通过将3-15重量%的热塑性弹性体和/或改性聚丙烯与80-20重量%的甲基丙烯酸甲酯和20-80重量%的丙烯酸乙酯混合的树脂混合来制备改性的甲基丙烯酸甲酯树脂; 并将0.5-2重量%的固化促进剂加入到混合物中。

    자전거 전용 도로용 포장재 조성물
    22.
    发明授权
    자전거 전용 도로용 포장재 조성물 有权
    BICYCLE路径的组合

    公开(公告)号:KR100937181B1

    公开(公告)日:2010-01-19

    申请号:KR1020090068584

    申请日:2009-07-27

    Inventor: 전상무 설태윤

    CPC classification number: E01C15/00 E01C7/30 E01C7/356 E01C13/065

    Abstract: PURPOSE: Paving composition for a bicycle path is provided to improve the shock resistance and the durability without a crack or omission. CONSTITUTION: Paving composition for a bicycle path is composed of quick-hardening resin 30~60 weight%, aggregate 20~30 weight%, filler 15~25 weight%, paint 2~5%, anti-foaming agent 1~3 weight%, UV blocking agent 1~4 weight%, and oxygen barrier agent 1~3 weight%. The quick-hardening resin is manufactured by mixing low-viscosity methyl methacrylate resin 50~80 weight%, thermosetting resin or synthetic resin selected from high-viscosity methyl methacrylate 19.5~48 weight%, and hardening accelerator 0.5~2%.

    Abstract translation: 目的:提供用于自行车路径的铺路组合物,以提高抗冲击性和耐久性,而不会产生裂缝或遗漏。 规定:自行车路径的铺路组合物由快硬硬化树脂30〜60重量%,骨料20〜30重量%,填料15〜25重量%,涂料2〜5%,消泡剂1〜3重量% ,紫外线阻断剂1〜4重量%,氧气阻隔剂1〜3重量%。 通过混合低粘度甲基丙烯酸甲酯树脂50〜80重量%,热固性树脂或选自高粘度甲基丙烯酸甲酯19.5〜48重量%的合成树脂和硬化促进剂0.5〜2%制造快速硬化树脂。

    발수기능 및 내오염기능을 증대시키고, 기계적 물성을 향상시킨 고기능성 미끄럼 방지 포장재 조성물 및 이를 이용한 시공방법

    公开(公告)号:KR101889270B1

    公开(公告)日:2018-08-20

    申请号:KR1020170137419

    申请日:2017-10-23

    Inventor: 설태윤

    Abstract: 본발명은발수기능및 내오염기능을증대시키고, 기계적물성을향상시킨고기능성미끄럼방지포장재조성물및 이를이용한시공방법에관한것으로, 테레프탈산변성폴리아마이드수지(acid modified polyamide resin) 30~40 중량%, 열가소성하이브리드수지 35~45 중량%, 로진에스테르수지 15~25 중량% 및석유수지 5~10 중량%를포함하는기재및; 상기기재 100 중량부에대하여, 건설용폐골재분말 120~140 중량부, 제강슬래그분말 110~130 중량부, 충진제 50~60 중량부, 세라믹분말 10~20 중량부, 발수제 10~20 중량부, 유리알 1~1.5 중량부및 착색안료 1~1.5 중량부를포함하며, 상기로진에스테르수지는수소첨가탄화수소로진에스테르(hydrogenated hydrocarbon rosin esters), 아크릴릭로진에스테르수지(acrylic rosin esters), 불균화로진에스테르(disproportionated rosin esters), 2염기산변성로진에스테르(dibasic acid modified rosin esters), 중합로진에스테르(polymerized rosin esters), 및페놀변성로진에스테르(phenol modified rosin esters)로이루어진군에서선택된하나이상인것을기술적요지로한다.

    에폭시-폴리우레아 하이브리드 수지를 이용한 미끄럼방지 포장재 조성물
    27.
    发明授权
    에폭시-폴리우레아 하이브리드 수지를 이용한 미끄럼방지 포장재 조성물 有权
    使用环氧树脂混合树脂防止滑动的道路填充材料组合物

    公开(公告)号:KR101148963B1

    公开(公告)日:2012-05-22

    申请号:KR1020110146202

    申请日:2011-12-29

    Inventor: 설태윤

    Abstract: PURPOSE: An anti-slip paving composition using epoxy-polyurea hybrid resin and a manufacturing method thereof are provided to improve drug resistance, cohesive property, corrosiveness. CONSTITUTION: An anti-slip paving composition using epoxy-polyurea hybrid resin comprises 35-44 weight% of epoxy polyurethane hybrid resin, 25-35 weight% of aggregate, 20-25 weight% of filler, 5-10 weight% of reactive aggregate, 2-5 weight% of additive, and 4-7 weight% of pigment. A manufacturing method of the anti-slip paving composition using epoxy-polyurea hybrid resin comprises the following steps: mixing and stirring rkat5-10 weight% of amine-terminated urea prepolymer resin with 80-90 weight% of bisphenol A type epoxy resin and 10-20 weight% of non-halogen flame-retarding epoxy resin; manufacturing the mixture at 80-120 deg. Celsius for 3-5 hours.

    Abstract translation: 目的:提供一种使用环氧 - 聚脲杂化树脂的防滑铺路组合物及其制造方法,以提高耐药性,内聚性,腐蚀性。 构成:使用环氧 - 聚脲杂化树脂的防滑铺路组合物包含35-44重量%的环氧聚氨酯混合树脂,25-35重量%的聚集体,20-25重量%的填料,5-10重量%的反应性聚集体 ,2-5重量%的添加剂和4-7重量%的颜料。 使用环氧 - 聚脲杂化树脂的防滑铺路组合物的制造方法包括以下步骤:将80重量%的双酚A型环氧树脂和10重量%的胺封端的脲预聚物树脂混合搅拌 -20重量%的无卤阻燃环氧树脂; 制造混合物在80-120度。 摄氏3-5小时。

    고탄성 폴리우레아 도료 조성물 및 이를 이용한 시공방법
    28.
    发明授权
    고탄성 폴리우레아 도료 조성물 및 이를 이용한 시공방법 有权
    具有高弹性的环境友好的聚氨酯涂料组合物和使用它的方法

    公开(公告)号:KR101141511B1

    公开(公告)日:2012-05-08

    申请号:KR1020110115367

    申请日:2011-11-07

    Inventor: 설태윤

    CPC classification number: C09D175/02 B05D1/02 C08G18/28 C09D5/00

    Abstract: PURPOSE: A highly elastic polyurea paint composition is provided to improve physical properties because of obtaining strength and tenacity in molecular structure, and to absorb or to release external impact or vibration. CONSTITUTION: A highly elastic polyurea paint composition comprises a base material part and a hardener part with volume ratio of 1:1. The base material part consists of a resin mixture which comprises 20-40 weight% of amine-terminated epoxy prepolymer, 20-40 weight% of polymer mixture, 15-25 weight% of a crosslinking agent, 2-8 weight% of pigment, and 2-8 weight% of additives. The hardener part consists of 70-130 parts by weight of polymer polyol on the basis of 100.0 parts by weight of isocyanate mixture, and is manufactured by maintaining isocyanate mixture and the polymer at 60-120 °C for 3-5 hours.

    Abstract translation: 目的:提供高弹性聚脲漆组合物,以改善物理性能,因为在分子结构中获得强度和韧性,并吸收或释放外部冲击或振动。 构成:高弹性聚脲漆组合物包含基体部分和体积比为1:1的硬化剂部分。 基材部分由树脂混合物组成,其包含20-40重量%的胺封端的环氧预聚物,20-40重量%的聚合物混合物,15-25重量%的交联剂,2-8重量%的颜料, 和2-8重量%的添加剂。 固化剂部分由70〜130重量份的聚合物多元醇组成,基于100.0重量份的异氰酸酯混合物,并通过将异氰酸酯混合物和聚合物保持在60-120℃下制备3-5小时。

    작업성이 우수하고 견고한 폴리우레아 도료 조성물 및 그 시공방법
    29.
    发明授权
    작업성이 우수하고 견고한 폴리우레아 도료 조성물 및 그 시공방법 有权
    具有优异的可加工性和超强韧性的聚氨酯涂料组合物及其使用方法

    公开(公告)号:KR101029660B1

    公开(公告)日:2011-04-15

    申请号:KR1020110007107

    申请日:2011-01-25

    Inventor: 설태윤

    CPC classification number: C09D175/02 C08L63/00 C09D5/08

    Abstract: PURPOSE: A two-part type polyurea paint composition is provided to impart strength and toughness in molecules, and to ensure excellent mechanical properties and abrasion resistance. CONSTITUTION: A two-part type polyurea paint composition comprises a first-part resin compound and a second-part hardener. The resin compound includes 25.0-45.0 weight% of epoxy prepolymer, 25.0-45.0 weight% of amine functional resin, 5.0-15.0 weight% of corsslinking agent, 2.0-8.0 weight% of pigment, and 2.0-8.0 weight% of additives. The hardener is a mixture of 100 parts by weight of IPDI(Isophorone Diisocyanate) or HDT(Hexamethylene diisocyanate trimer) with 50-150 parts by weight of polypropylene glycol or polyoxypropylenediamine.

    Abstract translation: 目的:提供两部分型聚脲漆组合物,以赋予分子强度和韧性,并确保优异的机械性能和耐磨性。 构成:两部分型聚脲漆组合物包含第一部分树脂化合物和第二部分硬化剂。 树脂化合物包括25.0-45.0重量%的环氧预聚物,25.0-45.0重量%的胺官能树脂,5.0-15.0重量%的连接剂,2.0-8.0重量%的颜料和2.0-8.0重量%的添加剂。 硬化剂是100重量份IPDI(异佛尔酮二异氰酸酯)或HDT(六亚甲基二异氰酸酯三聚体)与50-150重量份聚丙二醇或聚氧丙烯二胺的混合物。

    콘크리트 구조물 보호용 방수 코팅제 조성물
    30.
    发明授权
    콘크리트 구조물 보호용 방수 코팅제 조성물 有权
    防水涂料组合物,用于保护混凝土结构

    公开(公告)号:KR100978451B1

    公开(公告)日:2010-08-26

    申请号:KR1020100034406

    申请日:2010-04-14

    Inventor: 설태윤

    Abstract: PURPOSE: A waterproof coating composition is provided to improve the workability of the composition by the rapid cooling property of a resin, and to prevent the corrosion of an inside steel reinforcing rod. CONSTITUTION: A waterproof coating composition for protecting a concrete structure contains the following: 45~60wt% of methyl methacrylate resin; 20~35wt% of functional filler including one element selected from charcoal powder, hollow material powder, and inhibitive pigment; 2~7wt% of coloring pigment; 15~25wt% of extender pigment; and 1~10wt% of additive. The hollow material powder is alumino silicate. The composition additionally contains more than one curing accelerator selected from the group consisting of metallic salt based cobalt, dimethyl acrylamide, and amine-based compound.

    Abstract translation: 目的:提供防水涂料组合物,以通过树脂的快速冷却性能来改善组合物的可加工性,并防止内部钢筋的腐蚀。 构成:用于保护混凝土结构的防水涂料组合物含有:甲基丙烯酸甲酯树脂45〜60重量% 20〜35wt%的功能性填料,包括一种选自木炭粉,中空材料粉末和抑制性颜料的元素; 2〜7重量%着色颜料; 15〜25wt%增量颜料; 和1〜10wt%的添加剂。 中空材料粉末是铝硅酸盐。 该组合物另外含有多于一种选自金属盐基的钴,二甲基丙烯酰胺和胺类化合物的固化促进剂。