公开(公告)号:KR101026531B1
公开(公告)日:2011-04-01
申请号:KR1020080085996
申请日:2008-09-01
Applicant: 한국화학연구원
Inventor: 박인환
IPC: C09J125/06 , C09J125/08 , C09J125/00
Abstract: 본 발명은 할로겐프리형 난연성 접착제 조성물에 관한 것으로서, 더욱 상세하게는 화학식 1로 표시되는 고분자 수지를 접착제 조성물의 난연제로 사용하여 양호한 난연성, 접착성 및 내블리딩성 등을 유지하면서도 고유의 접착능력을 저하시키는 않으므로, 폴리이미드 기재 필름을 사용하는 동박 적층판은 물론, 유연기판의 폴리이미드 커버레이 필름 등에 활용 가능한 난연화 접착제 조성물에 관한 것이다.
할로겐프리형, 난연성, 접착제-
公开(公告)号:KR1020100027078A
公开(公告)日:2010-03-10
申请号:KR1020090081454
申请日:2009-08-31
Inventor: 박인환
IPC: C09J133/08
Abstract: PURPOSE: An environment-friendly water-based acrylic adhesive is provided to control adhesive strength, coatability, viscosity and chemical resistance and to ensure viscosity, coatability, adhesive force and drug resistance. CONSTITUTION: An environment-friendly water-based acrylic adhesive comprises 30~70 parts by weight of acrylic emulsion with 35~55 weight% solid portion, 2~10 parts by weight of acrylamide-based water-soluble resin with 3~12 weight% solid portion, 0.1~6 parts by weight of cellulose-based resin, and 20~40 parts by weight of additives.
Abstract translation: 目的:提供环保型水性丙烯酸粘合剂,以控制粘合强度,涂布性,粘度和耐化学性,并确保粘度,涂布性,粘合力和耐药性。 构成:环保型水性丙烯酸粘合剂包括30〜70重量份的丙烯酸乳液,35〜55重量%的固体部分,2〜10重量份的丙烯酰胺类水溶性树脂,3〜12重量% 固体部分,0.1〜6重量份的纤维素类树脂和20〜40重量份的添加剂。
-
公开(公告)号:KR1020100026472A
公开(公告)日:2010-03-10
申请号:KR1020080085491
申请日:2008-08-29
Inventor: 박인환
IPC: C09J133/08
CPC classification number: C09J133/08 , C09J9/00 , C09J11/08
Abstract: PURPOSE: A method for preparing water-resistant acrylic adhesives is provided to prepare water-resistant acrylic adhesives with lipophilic property used as a coating agent or adhesive requiring water resistance and salty water resistance. CONSTITUTION: A method for preparing acrylic emulsion adhesives through emulsion polymerization of acrylic monomers comprises the steps of: adding a water-soluble radical initiator to a monomer with a glass transition temperature of 20~70 °C, emulsifying the monomer mixture with a surfactant, and stirring the emulsion to perform core-shell reaction; and adding a lipophilic monomer with a glass transition temperature of -60 ~ -15 °C, a monomer with adhesive functional groups, and a tackifying resin to the reactant to perform copolymerization.
Abstract translation: 目的:提供一种制备耐水丙烯酸粘合剂的方法,以制备具有亲油性的防水丙烯酸粘合剂,用作涂层剂或需要耐水性和耐咸水性的粘合剂。 构成:通过丙烯酸单体的乳液聚合制备丙烯酸乳液粘合剂的方法包括以下步骤:向玻璃化转变温度为20〜70℃的单体中加入水溶性自由基引发剂,用表面活性剂乳化单体混合物, 并搅拌乳液进行核 - 壳反应; 并加入玻璃化转变温度为-60〜-15℃的亲油性单体,具有粘合官能团的单体和增粘树脂进行共聚反应。
-
公开(公告)号:KR1020090023317A
公开(公告)日:2009-03-04
申请号:KR1020080085996
申请日:2008-09-01
Applicant: 한국화학연구원
Inventor: 박인환
IPC: C09J125/06 , C09J125/08 , C09J125/00
CPC classification number: C09J125/08 , C08L63/00 , C09J9/00 , C09J11/08 , C09J125/06
Abstract: A halogen free type flame retardant adhesive composition is provided to maintain a high flame retardant and bleeding resistance property while not reducing a specific adhesive property for a polyimide and copper-clad lamination film. A halogen free type flame retardant adhesive composition has a structure represented by the formula 1. In the formula 1, m, o, p, q and r show the number of moles of each component; and R indicates a C1-C6 alkyl, phenyl, and benzyl group. When a mole fraction(m) of styrene is restricted to 1, a mole fraction(o+p) of a triphenylphosphite bonding group is 0.7-0.95; a mole fraction(o+q) of an amide bonding group is 0.7-0.98; and a mole fraction(p+q+2r) of a carboxyl bonding group is 0.01-0.15.
Abstract translation: 提供无卤阻燃粘合剂组合物以在不降低聚酰亚胺和覆铜层压膜的特定粘合性的同时保持高阻燃性和耐渗血性。 无卤阻燃型粘合剂组合物具有由式1表示的结构。在式1中,m,o,p,q和r表示各组分的摩尔数; 并且R表示C1-C6烷基,苯基和苄基。 当苯乙烯的摩尔分数(μm)限制为1时,亚磷酸三苯酯键合基团的摩尔分数(o + p)为0.7-0.95; 酰胺键合基团的摩尔分数(o + q)为0.7-0.98; 羧基键合基团的摩尔分数(p + q + 2r)为0.01-0.15。
-
公开(公告)号:KR1020090023316A
公开(公告)日:2009-03-04
申请号:KR1020080085995
申请日:2008-09-01
Applicant: 한국화학연구원
Inventor: 박인환
IPC: C08F230/02 , C08F222/22 , C08F222/00 , C08F293/00
CPC classification number: C08F230/02 , C08F8/32 , C08F222/22 , C08L43/02 , C08L2201/02
Abstract: A halogen free type specific polymeric flame retardant is provided to realize a flame retardant effect by using a phosphoric acid and a nitrogen gas to generate a synergistic effect of a liquid and gas phase. A halogen free type specific polymeric flame retardant has a structure represented by the formula 1. In the formula 1, m, o, p, q and r show the number of moles of each component; and R indicates a C1-C6 alkyl, phenyl, and benzyl group. When a mole fraction(m) of isobutylene is restricted to 1, a mole fraction(o+p) of a triphenylphosphite bonding group is 0.7-0.95; a mole fraction(o+q) of an amide bonding group is 0.7-0.95; and a mole fraction(p+q+2r) of a carboxylic acid bonding group is 0.01-0.15.
Abstract translation: 提供无卤型特定的聚合物阻燃剂以通过使用磷酸和氮气来产生液相和气相的协同效应来实现阻燃效果。 无卤型特定聚合物阻燃剂具有由式1表示的结构。在式1中,m,o,p,q和r表示各组分的摩尔数; 并且R表示C1-C6烷基,苯基和苄基。 当异丁烯的摩尔分数(μm)限制为1时,亚磷酸三苯酯键合基团的摩尔分数(o + p)为0.7-0.95; 酰胺键合基团的摩尔分数(o + q)为0.7-0.95; 羧酸键合基团的摩尔分数(p + q + 2r)为0.01-0.15。
-
公开(公告)号:KR100837376B1
公开(公告)日:2008-06-12
申请号:KR1020060075233
申请日:2006-08-09
Applicant: 한국화학연구원
Abstract: 본 발명은 정전하상 현상용 토너의 제조에 활용되는 구상수지 조성물에 관한 것으로서, 더욱 상세하게는 착색제, 전하제어제, 이형제 등의 배합성분을 함유하는 토너(toner) 중 상기 배합성분을 담지하는 기본 소재인 구상수지 조성물로 중합하여 대전특성을 주는 친유성 단량체에, 중합되는 구상입자 표면에 극성을 부여하기 위하여 소량의 극성 단량체를 단독 혹은 공간 넓힘용 단량체를 선택적으로 포함하고, 점착성과 내구성을 향상시키는 가교제 등을 조합하고, 이들 조성물을 분산안정제가 함유된 수상 매체에서 중합할 경우에, 구상수지의 평균 입경이 작아지고, 입도 분포의 폭이 적어지므로 균일한 크기의 입자를 얻을 수 있고, 구상입자 내ㆍ외부가 친유와 친수로 구분이 확실하게 되어 함수율이 적어, 고습 하에 있어서도 높은 대전량을 유지하고, 구상입자 표면의 극성관능기에 의해 양호한 저온 정착성을 나타내기에, 이렇게 얻어진 구상수지에 토너용 배합성분을 담지하게 되면, 인쇄 시 흐려짐을 낮게 하고, 보다 향상된 화상농도가 얻어질 수 있도록 대전효과를 효율적으로 향상시키도록 개선한 정전하상 현상용 토너에 사용되는 구상수지 조성물 및 그의 제조방법에 관한 것이다.
정전하상, 현상용, 구상수지, 토너, 대전성
-
-
-
-
-
-
-
-
-