다공성 유무기혼성체를 함유하는 흡착제
    21.
    发明公开
    다공성 유무기혼성체를 함유하는 흡착제 有权
    包含多孔有机无机混合材料的吸收

    公开(公告)号:KR1020090011999A

    公开(公告)日:2009-02-02

    申请号:KR1020070077335

    申请日:2007-08-01

    CPC classification number: Y02A50/235

    Abstract: An adsorber containing porosity organic/inorganic hybrid is provided to remove impurities of organic/inorganic mixture nanoporous materials and to increase surface area the organic/inorganic mixture nanoporous materials by processing it using ammonium chloride or potassium fluoride. An adsorber containing porosity organic/inorganic hybrid comprises steps of: mixing metal precursor, organic compound acting on ligand, acid and solvent and manufacturing a reactant mixed solution; irradiating microwave to the reactant mixed solution over 100°C; processing the porosity organic/inorganic hybrid using an inorganic salt or solvent. The acid is inorganic acid except for hydrofluoric acid.

    Abstract translation: 提供含有孔隙有机/无机杂化物的吸附剂,以除去有机/无机混合物纳米多孔材料的杂质,并通过使用氯化铵或氟化钾处理有机/无机混合物纳米多孔材料来增加表面积。 含有孔隙性有机/无机杂化物的吸附剂包括以下步骤:混合金属前体,作用于配体,酸和溶剂的有机化合物,制备反应物混合溶液; 在100℃下向反应混合溶液中照射微波; 使用无机盐或溶剂处理孔隙有机/无机混合物。 酸是除氢氟酸以外的无机酸。

    다공성 유무기혼성체의 제조방법, 상기 방법에 의하여수득되는 유무기혼성체 및 이의 촉매적 용도
    22.
    发明公开
    다공성 유무기혼성체의 제조방법, 상기 방법에 의하여수득되는 유무기혼성체 및 이의 촉매적 용도 有权
    一种制备多孔有机无机材料的方法和方法获得的多孔有机无机杂化材料和材料的催化用途

    公开(公告)号:KR1020080114380A

    公开(公告)日:2008-12-31

    申请号:KR1020070063881

    申请日:2007-06-27

    Abstract: A manufacturing method of porosity organic and inorganic hybrid is provided to manufacture and refine porosity organic and inorganic hybrid by an eco-friendly method using a new manufacturing process which does not use a hydrofluoric acid at all. A manufacturing method of porosity organic and inorganic hybrid comprises steps of: 1) manufacturing the reactant mixed solution by mixing a metal precursor, an organic compound acting on a ligand, an acid and a solvent; 2) heating the reactant mixed solution over 100‹C by electric heating or irradiating a microwave; 3) refining the porosity organic and inorganic hybrid by processing obtained the porosity organic and inorganic hybrid in the step 2) as inorganic salts.

    Abstract translation: 提供孔隙有机和无机混合物的制造方法,通过使用不使用氢氟酸的新制造方法的环保方法来制造和精制孔隙有机和无机杂化物。 孔隙有机和无机杂化物的制造方法包括以下步骤:1)通过混合金属前体,作用于配体的有机化合物,酸和溶剂来制备反应混合溶液; 2)通过电加热或照射微波将反应物混合溶液加热至100℃以上; 3)通过加工精制孔隙有机和无机杂化物,得到在步骤2)中的无机杂化物作为无机盐。

    불포화 금속자리를 갖는 다공성 유-무기 혼성체 또는메조세공체의 표면 기능화 및 그의 응용
    23.
    发明授权
    불포화 금속자리를 갖는 다공성 유-무기 혼성체 또는메조세공체의 표면 기능화 및 그의 응용 有权
    表面官能化有机无机混合材料或具有协调不饱和金属矿物的多孔材料及其催化应用的制备

    公开(公告)号:KR100864313B1

    公开(公告)日:2008-10-20

    申请号:KR1020070049415

    申请日:2007-05-21

    CPC classification number: B01J31/1691 B01J31/069 B01J2531/18 B01J2531/824

    Abstract: A preparation method of surface functionalized porous organic-inorganic hybrid materials that can be used in adsorbents, gas storage bodies, sensors, membranes, functional thin films, catalysts, and catalyst carriers is provided, and a catalyst composition for an acid or base reaction, hydrogenation, dehydrogeneration, a carbon-carbon bonding reaction, or an oxidation reaction by using the surface functionalized porous organic-inorganic hybrid materials or porous organic-inorganic mesoporous materials is provided. A preparation method of surface modified porous organic-inorganic hybrid materials is characterized in that the surface modified porous organic-inorganic hybrid materials are prepared by bonding organic materials, polyoxometalates, ionic liquids, organometallic compounds, or mixtures thereof having functional groups selected from an amino group(-NH2), a thiol group(-SH) and a phosphoric group(-PO(OH)2) to porous organic-inorganic hybrid materials with coordinatively unsaturated metal sites or to coordinatively unsaturated metal sites of porous organic-inorganic mesoporous materials. The porous organic-inorganic hybrid materials are polymer compounds formed by bonding core metal ions to organic ligands and have molecular-sized or mamo-sized pore structures, and the porous organic-inorganic mesoporous materials have coordinatively unsaturated metal sites and pores with a pore size of 2 to 50 nm by substituting dissimilar metals. Core metal precursors of the porous organic-inorganic hybrid materials are one or more metals selected from Ti, Zr, Hf, V, Nb, Ta, Cr, Mo, W, Mn, Re, Fe, Ru, Os, Co, Rh, Ir, Ni, Pd, Pt, Cu, Ag, Au, Zn, Cd, Hg, Mg, Ca, Sr, Ba, Sc, Y, Al, Ga, In, Tl, Si, Ge, Sn, Pb, As, Sb and Bi, or compounds thereof.

    Abstract translation: 提供了可用于吸附剂,储气体,传感器,膜,功能薄膜,催化剂和催化剂载体的表面官能化多孔有机 - 无机混合材料的制备方法,以及用于酸或碱反应的催化剂组合物, 提供氢化,脱氢生成,碳 - 碳键合反应或通过使用表面官能化的多孔有机 - 无机杂化材料或多孔有机 - 无机介孔材料的氧化反应。 表面改性多孔有机 - 无机杂化材料的制备方法的特征在于表面改性的多孔有机 - 无机杂化材料是通过键合具有选自以下的官能团的有机材料,多金属氧酸盐,离子液体,有机金属化合物或其混合物制备的: 基团(-NH 2),硫醇基(-SH)和磷酸基(-PO(OH)2)与具有配位不饱和金属位点的多孔有机 - 无机杂化材料或多孔有机 - 无机介孔材料的配位不饱和金属部位 。 多孔有机 - 无机杂化材料是通过将核心金属离子与有机配体键合而形成的聚合物化合物,并且具有分子尺寸或mamo尺寸的孔结构,并且多孔有机 - 无机介孔材料具有配位不饱和金属部位和孔径 通过取代异种金属2〜50nm。 多孔有机 - 无机杂化材料的核心金属前体是选自Ti,Zr,Hf,V,Nb,Ta,Cr,Mo,W,Mn,Re,Fe,Ru,Os,Co,Rh中的一种或多种金属, Ir,Ni,Pd,Pt,Cu,Ag,Au,Zn,Cd,Hg,Mg,Ca,Sr,Ba,Sc,Y,Al,Ga,In,Tl,Si,Ge,Sn,Pb, Sb和Bi,或其化合物。

    철이 포함된 다공성 유무기 혼성체의 제조방법
    24.
    发明授权
    철이 포함된 다공성 유무기 혼성체의 제조방법 有权
    多孔有机无机杂化材料的合成方法

    公开(公告)号:KR100816547B1

    公开(公告)日:2008-03-25

    申请号:KR1020060117549

    申请日:2006-11-27

    Abstract: A method of preparing an iron-containing porous organic/inorganic hybrid material is provided to prepare an organic/inorganic hybrid material through a batch or continuous reaction process for a short reaction time and prepare an organic/inorganic hybrid material having a special crystal structure within a short time, and an iron-containing porous organic/inorganic hybrid material prepared by the method is provided. In a method of preparing a porous organic/inorganic hybrid material using metal material and coordination compound as reaction raw materials, a method of preparing an iron-containing porous organic/inorganic hybrid material comprises: a pretreatment step of stirring iron or an iron salt as the metal material, and benzene tricarboxylic acid as the coordination compound at a rotation speed of 50 to 2000 revolutions per minute for 5 to 600 minutes in the presence of a solvent, and a mixed acid as a reaction promoter in which nitric acid is mixed with hydrofluoric acid at a molar ratio of 0.1 to 1:1 to 0.1, or irradiating ultrasonic waves of 15000 Hz to 30 MHz onto the iron or an iron salt and the benzene tricarboxylic acid for 1 to 600 minutes to form a crystal nucleus; and a step of irradiating a microwave of 1 to 30 GHz onto the crystal nucleus-formed reaction solution to prepare an organic/inorganic hybrid material in a temperature range of 100 to 250 deg.C. The solvent is an alcohol having 1 to 10 carbon atoms, a ketone having 2 to 10 carbon atoms, a hydrocarbon having 5 to 20 carbon atoms, or mixtures thereof. Further, the iron-containing porous organic/inorganic hybrid material has a structure of Materials of Institut Lavoisier-100.

    Abstract translation: 提供一种制备含铁多孔有机/无机混合材料的方法,通过间歇或连续反应方法制备有机/无机混合材料,反应时间短,并制备具有特殊晶体结构的有机/无机混合材料 提供了通过该方法制备的含铁多孔有机/无机混合材料。 在使用金属材料和配位化合物作为反应原料制备多孔有机/无机混合材料的方法中,制备含铁多孔有机/无机混合材料的方法包括:将铁或铁盐搅拌的预处理步骤 金属材料和苯三羧酸作为配位化合物,在溶剂存在下,以旋转速度为50〜2000转每分钟5〜600分钟,作为反应促进剂,将硝酸与 氢氟酸的摩尔比为0.1-1:1至0.1,或将15000Hz至30MHz的超声波照射到铁或铁盐和苯三羧酸上1至600分钟以形成晶核; 以及将1〜30GHz的微波照射到晶核形成的反应溶液上以在100〜250℃的温度范围内制备有机/无机混合材料的工序。 溶剂是具有1至10个碳原子的醇,具有2至10个碳原子的酮,具有5至20个碳原子的烃或其混合物。 此外,含铁多孔有机/无机混合材料具有Institut Lavoisier-100的材料结构。

    결정성 다공성 유무기혼성체를 함유하는 흡착제
    27.
    发明授权
    결정성 다공성 유무기혼성체를 함유하는 흡착제 有权
    含有结晶多孔有机 - 无机杂化材料的吸附剂

    公开(公告)号:KR100982641B1

    公开(公告)日:2010-09-16

    申请号:KR1020080124810

    申请日:2008-12-09

    Abstract: 본 발명은 결정성 다공성 유무기혼성체를 함유하는 흡착제에 관한 것으로서, 구체적으로는 염화물을 포함하는 무기산의 금속전구체, 리간드로 작용할 수 있는 유기 화합물 및 용매를 혼합하여 반응물혼합액을 제조하는 단계(단계 1); 상기 반응물 혼합액을 전기가열 또는 마이크로파를 조사하여 80 ℃이상으로 가열하여 유무기 혼성체를 형성하는 단계(단계 2);및 상기 단계 2에서 수득된 다공성 유무기혼성체를 무기염, 산도조절제 또는 용매로 처리함으로써 정제하는 단계(단계 3)를 포함하는 제조방법에의해서 제조된 결정성 다공성 유무기혼성체를 함유하는 흡착제에 관한 것이다. 본 발명에 따른 흡착제는 높은 결정성을 갖는 균일한 입도분포를 갖는 나노 다공성 유무기혼성체를 포함하고 있어, 본 발명을 수분 흡착제로서 사용하는 경우, 100 ℃이하의 저온에서 탈착이 용이하여 가습제 또는 제습제로 유용하게 사용할 수 있다. 또한 본 발명을 휘발성유기화합물(VOC) 등을 제거를 위한 흡착제로서 사용하는 경우 특정유해물질을 효과적으로 제거할 수 있어 새집증후군 방지, 각종 유해물질 제거에 유용하게 사용할 수 있다.
    유무기혼성체, 수열합성, 나노입자, 세공물질, 흡착제, 마이크로파 합성, 휘발성유기혼합물(VOC)

    Abstract translation: 本发明是晶体多孔上含有杂化无机 - 有机材料的吸附剂,具体而言,通过混合的有机化合物和可以作为金属前体作用的溶剂,含有氯化物的无机酸的配位体(步骤1制备的反应混合物 ); A和无机盐在上述步骤2中得到的多孔杂化无机 - 有机材料,pH调节剂或溶剂,在80℃以上反应混合物中的电加热或步骤通过微波辐射加热,形成有机 - 无机混合材料(步骤2) (步骤3)本发明还涉及含有结晶多孔杂化无机 - 有机材料的吸附剂。 根据本发明的吸着剂,它包括具有具有高结晶性的均匀的粒度分布,在使用本发明的作为水分吸附剂的情况下,纳米多孔杂化无机 - 有机材料,并且解吸很容易在低于100℃的加湿剂或的低温下 它可以有效地用作干燥剂。 它能够除去某些物质有效地防止病屋综合症,作为用于去除有机化合物(VOC)挥发性的本发明的吸附剂一起使用时除去各种有害物质,也可以是有用的。

    결정성 다공성 유무기혼성체를 함유하는 흡착제
    28.
    发明公开
    결정성 다공성 유무기혼성체를 함유하는 흡착제 有权
    吸附剂包括结晶多孔有机无机混合材料

    公开(公告)号:KR1020100066140A

    公开(公告)日:2010-06-17

    申请号:KR1020080124810

    申请日:2008-12-09

    CPC classification number: B01J20/30 B01J19/08 B01J20/02 B01J20/22 B01J20/28014

    Abstract: PURPOSE: An adsorbent containing crystalline porous organic and inorganic hybrid materials, and a moisture absorbent are provided to eliminate the trace amount of a volatile organic compound in an indoor space, and to be used as a dehumidifier or a humidifier in a low temperature of 100 °C or less. CONSTITUTION: A manufacturing method of an adsorbent containing crystalline porous organic and inorganic hybrid materials comprises the following steps; manufacturing reactant mixed solution by mixing a metal precursor of inorganic acid including chloride, an organic compound used as ligand and a solvent; forming organic and inorganic hybrid by heating the reactant mixed solution with electricity or irradiating with the heat of over 80 °C; and refining the porous organic inorganic hybrid material by inorganic salt or an acidity control agent, or the solvent. The metal precursor is Ti, Zr, Hf, V, Nb, Ta, Cr, Mo, W, Mn, Re, Fe, Ru, Os, Co, Rh, Ir, Ni, Pd, Pt, Cu, Ag, Au, Zn, Cd, Hg, Mg, Ca, Sr, Ba, Sc, Y, Al, Ga, In, Tl, Si, Ge, Sn, Pb, As, Sb or Bi.

    Abstract translation: 目的:提供含有结晶多孔有机和无机混合材料和吸湿剂的吸附剂,以消除室内空气中痕量的挥发性有机化合物,并在低温100℃下用作除湿机或加湿器 ℃以下。 构成:含有结晶多孔有机和无机混合材料的吸附剂的制造方法包括以下步骤: 通过混合包括氯化物的无机酸的金属前体,用作配体的有机化合物和溶剂来制备反应物混合溶液; 通过用电加热反应物混合溶液或用超过80℃的热照射形成有机和无机杂化物; 并通过无机盐或酸度控制剂或溶剂对多孔有机无机杂化材料进行精制。 金属前体是Ti,Zr,Hf,V,Nb,Ta,Cr,Mo,W,Mn,Re,Fe,Ru,Os,Co,Rh,Ir,Ni,Pd,Pt,Cu,Ag,Au, Zn,Cd,Hg,Mg,Ca,Sr,Ba,Sc,Y,Al,Ga,In,Tl,Si,Ge,Sn,Pb,As,Sb或Bi。

    다공성 유무기혼성체를 함유하는 흡착제
    29.
    发明授权
    다공성 유무기혼성체를 함유하는 흡착제 有权
    吸收剂包括多孔有机 - 无机杂化材料

    公开(公告)号:KR100890347B1

    公开(公告)日:2009-03-25

    申请号:KR1020070077335

    申请日:2007-08-01

    CPC classification number: Y02A50/235

    Abstract: 본 발명은 다공성 유무기혼성체 (porous organic inorganic hybrid materials)의 신규 제조방법, 특히, 불산을 사용하지 않는 것을 특징으로 하는 제조 방법, 상기 제조 방법에 의하여 제조된 다공성 유무기혼성체 및 이의 흡착제로서의 용도에 관한 것으로서, 상기 다공성 유무기혼성체는 높은 표면적과 분자크기 또는 나노크기의 세공을 갖고 있어 흡착제, 기체 저장, 센서, 멤브레인, 기능성 박막, 촉매 및 촉매 담체, 가스 및 수분의 흡착제 등에 사용될 수 있으며 세공크기보다 작은 게스트 분자를 포집하거나 세공크기를 이용하여 분자들을 분리하는데 사용될 수 있다.
    유무기혼성체, 수열합성, 나노입자, 세공물질, 흡착제, 마이크로파 합성

    금속 담지 유-무기 메조세공체의 제조 방법
    30.
    发明授权
    금속 담지 유-무기 메조세공체의 제조 방법 失效
    贵金属掺杂的有机 - 无机介孔材料

    公开(公告)号:KR100830840B1

    公开(公告)日:2008-05-20

    申请号:KR1020060059331

    申请日:2006-06-29

    Abstract: 본 발명은 유해물질 제거용 다공성 유-무기 메조세공체의 제조 방법에 관한 것으로서, 더욱 상세하게는 메조세공체의 골격 내에 친유성기를 포함하고, 활성금속이 세공체 동공 내에 고분산되어 특정유해 물질을 선택적으로 흡착하여 저온에서 분해시킬 수 있는 귀금속 담지 유-무기 메조세공체 촉매의 제조 방법에 관한 것으로서, a) 금속염과 킬레이트 화합물의 혼합 용액; 실리카 전구체; 및 고분자 계면활성제 혼합물;을 혼합하여 메조구조체를 형성하는 단계; b) 상기 메조구조체로부터 킬레이트제 및 계면활성제를 제거하는 단계;를 포함하는 것을 특징으로 한다. 본 발명에 따른 제조방법에 의하여 제조된 다공성 유-무기 메조세공체는 휘발성 유기 화합물, 니트로소아민류, 폴리사이클릭아로마틱하이드로카본류 등과 같은 증기상 특정유해물질에 대한 제거능력이 우수하며, 담배 유해물질 제거용 촉매, 방독마스크용 필터로 응용가능하다.
    유-무기 메조세공체, 저온산화촉매, 하이브리드, 휘발성 유기 화합물, 나이트로소아민류, 귀금속