Abstract:
PURPOSE: A polymer/carbon nanotube complex is provided to have an environment-friendly property including carbon dioxide reduction and biodegradation property, and to have an excellent mechanical property with a high conductivity by a selective dispersion of conductive filler. CONSTITUTION: A polymer/carbon nanotube complex comprises: polymer mixed with polypropylene carbonate and polylactic acid. The carbon nanotube is dispersed in the polymer. The polypropylene carbonate and polylactic acid are comprised in a ratio of 2-4:1 wt%. The content of propylene carbon nanotube is 1-10 wt% based on the entire complex. A manufacturing method of the polymer/carbon nanotube comprises the steps of: melting and mixing the polypropylene carbonate, polylactic acid, and carbon nano tube; and thermocompressing the mixture.
Abstract:
본 발명은 재활용 폴리프로필렌 복합체 및 이를 포함한 재활용 소재 기반 열가소성 성형품에 관한 것으로서, 재활용 폴리프로필렌 수지와 아크릴로니트릴-부타디엔-스티렌 공중합체 (ABS, acrylonitrile-butadiene-styrene copolymer, 이하 'ABS'로 칭한다) 및 말레산 무수물 그래프트 스티렌-에틸렌-부틸렌-스티렌 공중합체(SEBS-g-MAH, styrene ethylene butylene styrene grafted maleic anhydride, 이하 'SEBS-g-MAH'로 칭한다.)를 포함하는 것을 특징으로 한다. 본 발명에 따른 상기 재활용 폴리프로필렌 복합체는 SEBS-g-MAH를 상용화제로 도입함으로써, 기존의 재활용 폴리프로필렌 복합체보다 분산상의 크기가 감소하여 분산성이 향상되는 등 물성이 우수하고, 상기 재활용 폴리프로필렌 복합체로 제조한 열가소성 소재는 기계적 물성, 특히 충격강도가 우수하다.
Abstract:
PURPOSE: A polymer/carbon nanotube composite is provided to have excellent electrical conductivity and biodegradability, while maintaining properties of polycarbonate like excellent strength and high heat resistance by using carbon nanotube-lactic acid as a compatibilizer. CONSTITUTION: A manufacturing method of a polymer/carbon nanotube composite comprises: a step of obtaining neutralized liquid by acid treating carbon nanotubes by hydroperoxide water, and adding distilled water into the outcome; a step adding L-lactic acid into the acid-treated multi-wall carbon nanotubes, conduct ultrasonic wave treatment, and removing non-reacted L-lactic acid and water. The polymer/carbon nanotube composite comprises polycarbonate, a biodegradable polymer selected from polylactic acid or polycaprolactone, carbon nanotube-lactic acid compatibilizer, and carbon nanotube.
Abstract:
폴리우레탄 나노 복합체 제조방법 및 이에 의하여 제조된 폴리우레탄 나노 복합체가 제공된다. 본 발명에 따른 폴리우레탄 나노 복합체 제조방법은 (a) 폴리올 함유 화합물에 액상 실란계 핵제를 혼합하는 단계; (b) 상기 (a) 단계의 혼합 용액을 교반하는 단계; 및 (c) 상기 (b) 단계에서 얻어진 용액에 디이소시아네이트기 함유 화합물을 혼합하여 폴리우레탄을 수득하는 단계를 포함하며, 본 발명에 따른 폴리우레탄 나노 복합체 제조방법은 종래의 폴리우레탄 나노 복합체에 비하여 작은 셀 크기를 가지며, 열적 특성이 통상적인 폴리우레탄 폼보다 우수하다.
Abstract:
연료전지 분리판용 조성물, 그 제조방법, 이를 포함하는 연료전지 분리판 및 연료전지가 제공된다. 본 발명에 따른 연료전지 분리판용 조성물은 제 1 전도성 첨가제; 및 상기 제 1 첨가제보다 작은 크기의 제 2 전도성 첨가제를 포함하며, 제 1 전도성 첨가제는 전체 조성물의 10 내지 70중량%이고, 제 2 전도성 첨가제는 0.1 내지 10중량%인 것을 특징으로 하며, 기존의 흑연 분리판보다 가격이 저렴하고, 제작이 용이할 뿐만 아니라, 가벼운 무게를 갖는 장점이 있으며, 다른 제조 방법에 의하여 제조된 분리판에 비하여 전기전도도를 향상시키는 효과를 갖는다.
Abstract:
PURPOSE: A fabrication method of a polymer/carbon nanotube composite is provided to synthesize the polymer/carbon nanotube composite with excellent electromagnetic-wave shielding efficiency and conductivity by uniformly dispersing carbon nanotube in a polymer resin. CONSTITUTION: A fabrication method of a polymer/carbon nanotube composite comprises the steps of: dissolving a first polymer resin and carbon nanotube in a solvent and applying ultrasonic waves to prepare a pre-composite; and mixing the pre-composite with a second polymer resin in an extruder. Carbon nanotubes coagulated in the first step is uniformly dispersed in the first polymer resin by sonication. The first polymer resin and/or the second polymer resin are polycarbonate.
Abstract:
A method of pre-treating a carbon nanotube for a polymer/carbon nanotube composite is provided to use no acid injuring a surface of the carbon nanotube, to improve dispersibility of the carbon nanotube and to disperse the carbon nanotube uniformly in a polymer matrix. A method of pre-treating a carbon nanotube for a polymer/carbon nanotube composite comprises steps of: mixing the carbon nanotube into a solvent; and processing the carbon nanotube in the solvent with an ultrasonic wave at a frequency range of 20,000Hz to 60,000Hz and for 30 to 180 minutes and obtaining a carbon nanotube dispersion solution.
Abstract:
A method for pre-treating carbon nanotubes for carbon nanotube/polymer composites is provided to increase dispersibility of carbon nanotubes for carbon nanotube/polymer composites and allow the production of carbon nanotube/polymer composites having excellent electrical and rheological characteristics. A method for pre-treating carbon nanotubes for carbon nanotube/polymer composites includes the steps of: (1) ultrasonically treating carbon nanotubes in a hydrogen peroxide solution at the temperature of 30-70 ‹C for 50-130 minutes; (2) adjusting pH of the product obtained in the step (1) to 5.0-7.0; and (3) freeze-drying the product obtained in the step (2). The carbon nanotubes are multi-walled carbon nanotubes or single-walled carbon nanotubes.
Abstract:
클레이-폴리우레탄 나노복합재가 제공된다. 본 발명에 따른 클레이-폴리우레탄 나노복합재는 디이소시아네이트 화합물을 기준으로 클레이 0.5∼5중량%를 포함하며, 상기 디이소시아네이트 화합물과 상기 클레이의 실란올 작용기가 공유결합으로 연결되어 있는 클레이 함유-디이소시아네이트 화합물과; 폴리올을 반응시켜 제조되는 것을 특징으로 한다. 본 발명에 따른 클레이-폴리우레탄 나노 복합재는 폴리우레탄이 상기 클레이의 층상에 삽입된 구조인 것이 아니라, 층상을 완전히 박리시킨 구조이기 때문에, 순수한 폴리우레탄에 비하여 물성이 우수하며, 발포시킨 경우에도 기계적 강도, 난연성 등의 물성이 통상적인 폴리우레탄 폼보다 현저히 향상된다. 클레이-폴리우레탄 나노복합재