21.
    发明专利
    未知

    公开(公告)号:DE59108958D1

    公开(公告)日:1998-04-30

    申请号:DE59108958

    申请日:1991-12-27

    Applicant: BASF AG

    Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …

    SHOCK-ABSORBING PROPYLENE POLYMER COMPOSITE MOLDINGS

    公开(公告)号:AU1038792A

    公开(公告)日:1992-08-06

    申请号:AU1038792

    申请日:1992-01-22

    Applicant: BASF AG

    Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …

    27.
    发明专利
    未知

    公开(公告)号:NO177341C

    公开(公告)日:1995-08-30

    申请号:NO920295

    申请日:1992-01-22

    Applicant: BASF AG

    Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …

    29.
    发明专利
    未知

    公开(公告)号:ES2066246T3

    公开(公告)日:1995-03-01

    申请号:ES91103171

    申请日:1991-03-02

    Applicant: BASF AG

    Abstract: A construction element having a virtually rectangular force-movement characteristic, consisting of an elongated polymer foam body (1) of rectangular cross-section having the rectangular sides a and b, and having a recess (2), which extends over the complete longitudinal extent and on one side of the body, of width d and of height c, the said dimensions satisfying specific equations. … …

    30.
    发明专利
    未知

    公开(公告)号:NO920295D0

    公开(公告)日:1992-01-22

    申请号:NO920295

    申请日:1992-01-22

    Applicant: BASF AG

    Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …