公开(公告)号:JPH05138784A
公开(公告)日:1993-06-08
申请号:JP34089691
申请日:1991-12-24
Applicant: BASF AG
Inventor: HAARDT UDO , SEILER ERHARD , TATZEL HERMANN , SCHWAGER HARALD , DOMAS FRIEDRICH
Abstract: PURPOSE: To make it possible to recycled use as well as obtain good durability, shock resistance, mechanical properties and surface property by constituting a composite molding using a propylene polymer as a main body and making a polymer adhere to both sides of a foamed core with a hot-melt adhesive layer. CONSTITUTION: This shock-absorbing propylene polymer composite molding comprises: (a) a layer with a thickness of 0.5 to 10 mm containing a propylene polymer having a melting point of 130 to 165 deg.C, (b) an intermediate layer with a thickness of 0.05 to 0.5 mm containing a hot-melt adhesive of olefin copolymer having a melting point of 90 to 140 deg.C as a main body, (c) a foamed layer with a thickness of 3 to 200 mm containing a propylene copolymer having a melting point of 125 to 155 deg.C as a main body and a density of 0.015 to 0.1 g/cm , (d) an intermediate layer with a thickness of 0.05 to 0.5 mm containing a hot-melt adhesive of olefin copolymer having a melting point of 90 to 140 deg.C as a main body, and (e) a layer with a thickness of 0.5 to 10 mm containing a propylene polymer having a melting point of 130 to 165 deg.C.
-
公开(公告)号:NO177341B
公开(公告)日:1995-05-22
申请号:NO920295
申请日:1992-01-22
Applicant: BASF AG
Inventor: HAARDT UDO , SEILER ERHARD , TATZEL HERMANN , SCHWAGER HARALD , DOMAS FRIEDRICH
Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …
-
公开(公告)号:DE59103836D1
公开(公告)日:1995-01-26
申请号:DE59103836
申请日:1991-03-02
Applicant: BASF AG
Inventor: LENZ WERNER , DOMAS FRIEDRICH , HAARDT UDO
Abstract: A construction element having a virtually rectangular force-movement characteristic, consisting of an elongated polymer foam body (1) of rectangular cross-section having the rectangular sides a and b, and having a recess (2), which extends over the complete longitudinal extent and on one side of the body, of width d and of height c, the said dimensions satisfying specific equations. … …
-
公开(公告)号:NO920295L
公开(公告)日:1992-07-24
申请号:NO920295
申请日:1992-01-22
Applicant: BASF AG
Inventor: HAARDT UDO , SEILER ERHARD , TATZEL HERMANN , SCHWAGER HARALD , DOMAS FRIEDRICH
Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …
-
公开(公告)号:DE4401579A1
公开(公告)日:1995-07-27
申请号:DE4401579
申请日:1994-01-20
Applicant: BASF AG
Inventor: TATZEL HERMANN , HAARDT UDO , DOMAS FRIEDRICH
-
公开(公告)号:MX9200249A
公开(公告)日:1992-10-01
申请号:MX9200249
申请日:1992-01-21
Applicant: BASF AG
Inventor: HAARDT UDO , SEILER ERHARD , TATZEL HERMANN , SCHWAGER HARALD , DOMAS FRIEDRICH
Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …
-
公开(公告)号:CA2059257A1
公开(公告)日:1992-07-24
申请号:CA2059257
申请日:1992-01-15
Applicant: BASF AG
Inventor: TATZEL HERMANN , DOMAS FRIEDRICH , SCHWAGER HARALD , SEILER ERHARD , HAARDT UDO
Abstract: O.Z. 0050/42154 A shock-absorbing propylene polymer composite molding contains a. a layer with a thickness of from 0.5 to 10 mm which contains a propylene polymer having a melting point of from 130 to 165.degree.C, b. an intermediate layer with a thickness of from 0.05 to 0.5 mm comprising a hot-melt adhesive based on an olefin copolymer having a melting point of from 90 to 140.degree.C, c. a foam layer with a thickness of from 3 to 200 mm and a density of from 0.015 to 0.1 g/cm3 based on a propylene copolymer having a melting point of from 125 to 155.degree.C, d. an intermediate layer with a thickness of from 0.05 to 0.5 mm comprising a hot-melt adhesive based on an olefin copolymer having a melting point of from 90 to 140.degree.C, e. a layer with a thickness of from 0.5 to 10 mm which contains a propylene polymer having a melting point of from 130 to 165.degree.C.
-
公开(公告)号:DE3800197A1
公开(公告)日:1989-07-20
申请号:DE3800197
申请日:1988-01-07
Applicant: BASF AG
Inventor: LOESER WERNER DR , DOMAS FRIEDRICH , ZISSEL GEORG , KUERTEN HERIBERT DR , BENDER RAINER DR
Abstract: The substrate plates, after facing, are finished with lapping discs, with the addition of a polishing fluid composed of an aqueous solution with aluminium oxide powder and organic additives, the lapping discs being provided with a covering made from an elastic material.
-
公开(公告)号:ES2120638T3
公开(公告)日:1998-11-01
申请号:ES95100237
申请日:1995-01-10
Applicant: BASF AG
Inventor: TATZEL HERMANN , HAARDT UDO , DOMAS FRIEDRICH
-
公开(公告)号:AT164345T
公开(公告)日:1998-04-15
申请号:AT91122249
申请日:1991-12-27
Applicant: BASF AG
Inventor: HAARDT UDO , SEILER ERHARD , TATZEL HERMANN , SCHWAGER HARALD , DOMAS FRIEDRICH
Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …
-
-
-
-
-
-
-
-
-