公开(公告)号:DE2967445D1
公开(公告)日:1985-06-13
申请号:DE2967445
申请日:1979-02-19
Applicant: BASF AG
Inventor: GAUSEPOHL HERMANN DR , REFFERT RUDI WILHELM , WILD HANS DR , ECHTE ADOLF DR
IPC: C08F4/04 , C08F212/12
-
公开(公告)号:DE3332326A1
公开(公告)日:1985-03-28
申请号:DE3332326
申请日:1983-09-08
Applicant: BASF AG
-
公开(公告)号:DE3331010A1
公开(公告)日:1985-03-14
申请号:DE3331010
申请日:1983-08-27
Applicant: BASF AG
Inventor: MITULLA KONRAD DR , SWOBODA JOHANN DR , ECHTE ADOLF DR , SCHMITT BURGHARD DR
-
公开(公告)号:DE3168499D1
公开(公告)日:1985-03-07
申请号:DE3168499
申请日:1981-09-09
Applicant: BASF AG
Inventor: ECHTE ADOLF DR , GAUSEPOHL HERMANN DR
IPC: C08L51/04
-
公开(公告)号:DE3234660A1
公开(公告)日:1984-03-22
申请号:DE3234660
申请日:1982-09-18
Applicant: BASF AG
Inventor: HAHN KLAUS DR , WITTMER PAUL DR , DE GRAVE ISIDOOR DR , SCHICK RUPERT DR , ECHTE ADOLF DR
IPC: C08J9/16 , C08F2/38 , C08F12/08 , C08F112/08 , C08J9/20
-
公开(公告)号:DE3234034A1
公开(公告)日:1984-03-15
申请号:DE3234034
申请日:1982-09-14
Applicant: BASF AG
Inventor: HAMBRECHT JUERGEN DR , REFFERT RUDI WILHELM , ECHTE ADOLF DR , SWOBODA JOHANN DR
Abstract: A process for the preparation of high molecular weight polyphenylene ethers from alkyl-substituted monohydric phenols by an oxidative coupling reaction with oxygen in the presence of a catalyst complex of a copper salt and an organic amine, subsequent stopping of the reaction and removal of the metal component of the catalyst by addition of chelating and/or salt-forming agents, wherein the polymer solution is treated with a compound having the general structure: where R2 and R3 can be identical or different and each is OH, NH2, NHR5, where R5 is alkyl or cycloalkyl, or SH, and where R1 and R4 are identical or different, being hydrogen, alkyl, cycloalkyl, aryl, carbonyl, carboxyl, carboxyalkyl or nitrile, and can be linked to form a ring, advantageously in an amount of from 0.1 to 100 mmoles and advantageously in from 1 to 20% strength aqueous solutions.
-
公开(公告)号:DE3228662A1
公开(公告)日:1984-02-02
申请号:DE3228662
申请日:1982-07-31
Applicant: BASF AG
Inventor: HAMBRECHT JUERGEN DR , REFFERT RUDI WILHELM , MUENCH VOLKER DR , ECHTE ADOLF DR , SWOBODA JOHANN DR
Abstract: High molecular weight polyphenylene ethers are prepared from monohydric phenols by an oxidative coupling reaction with oxygen in the presence of a catalyst complex obtained from a copper salt and an organic amine by a method wherein the metal component of the catalyst is separated off, after the polymerization, by the addition of a polymeric polycarboxylic acid which is essentially composed of unsaturated monofunctional or difunctional carboxylic acids and/or their anhydrides. Advantageously, the polymeric polycarboxylic acids used are homopolymers or copolymers of (a) from 50 to 100% by weight of one or more unsaturated monofunctional acids of 3 to 10 carbon atoms and/or one or more difunctional acids or their anhydrides of 4 to 6 carbon atoms and from 0 to 50% by weight of one or more monomers which do not possess an acid function and can be copolymerized with (a).
-
公开(公告)号:DE2208922A1
公开(公告)日:1973-09-06
申请号:DE2208922
申请日:1972-02-25
Applicant: BASF AG
Inventor: SIMAK PETER DR , ADLER HANSJOERG DR , ECHTE ADOLF DR
Abstract: In the polymsn. of styrene stabilised with t.-butyl-pyrocatechol as prepolymsn. inhibitor, in the presence of salts of higher fatty acids as mould release agent, 0.001-1wt.% dialkyl or diaryl phosphite is added to prevent discolouration. Diphenyl, dibenzyl, dibutyl and diisopropyl phosphites are prefd.
-
公开(公告)号:CH478854A
公开(公告)日:1969-09-30
申请号:CH1227767
申请日:1967-09-01
Applicant: BASF AG
Inventor: SCHOTT OTTO DR , BRONSTERT KLAUS DR , ECHTE ADOLF DR , JUERGEN HOFMANN , STEIN DIETER DR
IPC: C08F2/18 , C08F279/04 , C08F19/18
-
公开(公告)号:DE3785743D1
公开(公告)日:1993-06-09
申请号:DE3785743
申请日:1987-12-22
Applicant: BASF AG
Inventor: SCHWABEN HANS-DIETER DR , ECHTE ADOLF DR , BUESCHL RAINER DR , SCHLICHTMANN RAINER , KLAERNER PETER DR , KINDLER HUBERT DR
IPC: C08F2/18 , C08F287/00 , C08L25/06 , C08L51/00
Abstract: Thermoplastic moulding compsn. contains w.r.t. (A+B), (A) 80-60 (wt.)% rigid polystyrene matrix and (B) 20-40% soft phase, obtd. by polymerising styrene in the presence of a linear styrene-butadiene block copolymer with indistinct transition, which contains 35-45% styrene and 65-55% butadiene with a block polystyrene content of 25-35%. (B) is uniformly distributed in (A) and has a particle dia. of less than 0.8 micron. The average particle dia., d50 value (by vol.) of (B) is 0.252-0.38 micron, the particle size distribution range (d95-d5) value, is 0.2-0.6 micron, the d60 value, is in the 0.26-0.40 micron range and the d90 value is 0.40-0.75. (B) pref. contains 38-42% styrene and 62-58% butadiene with 25-35, esp. 30-32% block polystyrene. The average mol.wt. of (B) is 180000-250000 and the mol.wt. of the styrene block 50000-70000.
-
-
-
-
-
-
-
-
-