    Abstract: Copper-containing catalysts for low-temperature conversion at temperatures of from 150 to 300 DEG C and at from 10 to 40 bar which additionally contain aluminium, and zinc, if desired in the form of the compounds or oxides, and are prepared by joint precipitation, the copper-containing catalysts containing potassium and having a BET surface area matched to the potassium content, the potassium content being set to from 0.1 to 3.0% by weight at a BET surface area of from 30 to 160 m /g, and their use for the production of hydrogen and carbon dioxide from carbon monoxide and water.

    29.
    发明专利
    未知

    公开(公告)号:DE59506904D1

    公开(公告)日:1999-10-28

    申请号:DE59506904

    申请日:1995-07-04

    Applicant: BASF AG

    Abstract: PCT No. PCT/EP95/02592 Sec. 371 Date Mar. 20, 1997 Sec. 102(e) Date Mar. 20, 1997 PCT Filed Jul. 4, 1995 PCT Pub. No. WO96/01242 PCT Pub. Date Jan. 18, 1996A process is disclosed for the selective hydrogenation of butynediol to 2-butene-1,4-diol using a palladium catalyst to which either copper and zinc, or silver and zinc, or copper, silver and zinc are added as doping agents. In the preferred embodiment, it has been possible, by optimizing the composition of the catalyst, to improve the activity and selectivity of the catalysts in question while also eliminating the need to handle toxic substances during the catalyst manufacturing process.

    30.
    发明专利
    未知

    公开(公告)号:BR9507072A

    公开(公告)日:1997-09-09

    申请号:BR9507072

    申请日:1995-03-04

    Applicant: BASF AG

    Abstract: Catalyst suitable for hydrogenation of organic cpds., comprises (all based on total wt. of catalyst); (a) 80 wt.% nickel (calculated as nickel oxide); (b) 10-25 wt.% of silicon (calculated as zirconium oxide; and (d) 0-10 wt.% of aluminium (calculated as aluminium oxide). The amt. of silicon dioxide and aluminium oxide is at least 15 wt.%. The catalyst is prepd. by; (2) adding an acidic aq. soln. of nickel-, zirconium- and opt. aluminium salts to a basic aq. soln. or suspension of silicon cpds. (and opt. aluminium cpds.), so that the pH of the resulting mixt. drops to at least 6.5; (2) adding a further basic soln. to bring the pH to 7-8; and (3) isolating the pptd. solid, which is then dried, formed and calcined.