公开(公告)号:NO128160B
公开(公告)日:1973-10-08
申请号:NO478368
申请日:1968-11-29
Applicant: HOECHST AG
Inventor: OBERST H , EBIGT J , DUVE G , SCHOMMER A
Abstract: 1,245,470. Laminates. FARBWERKE HOECHST A.G. 4 Dec., 1968 [5 Sept., 1967], No. 67605/68. Heading B5N. [Also in Divisions B2 and F2] A vibration damping laminated system comprises two sheets and bonded to the sheets an interlayer comprising a graft polymer of 40 to 80% by weight of methylmethacrylate or a mixture of methylmethacrylate with from 0À1 to 10% by weight of a copolymerizable carboxylic acid, or 60 to 20% by weight of a copolymer formed from a monomer mixture of 30 to 40% by weight of vinyl acetate, 30 to 40% by weight of n-butyl acrylate, 10 to 30% by weight of dibutyl maleate and 5 to 15% by weight of a copolymerizable unsaturated carboxylic acid. Specified carboxylic acids in admixture with methylmethacrylate are acrylic, methacrylic or a mixture thereof and crotonic acid is specified as the carboxylic acid present in the copolymer. The sheets may be of metal. Also disclosed is a plate applied to one surface of which is a layer of a graft polymer as specified above.
-
公开(公告)号:SE360090B
公开(公告)日:1973-09-17
申请号:SE1649368
申请日:1968-12-03
Applicant: HOECHST AG
Inventor: OBERST H , EBIGT J , DUVE G , SCHOMMER A
Abstract: 1,245,470. Laminates. FARBWERKE HOECHST A.G. 4 Dec., 1968 [5 Sept., 1967], No. 67605/68. Heading B5N. [Also in Divisions B2 and F2] A vibration damping laminated system comprises two sheets and bonded to the sheets an interlayer comprising a graft polymer of 40 to 80% by weight of methylmethacrylate or a mixture of methylmethacrylate with from 0À1 to 10% by weight of a copolymerizable carboxylic acid, or 60 to 20% by weight of a copolymer formed from a monomer mixture of 30 to 40% by weight of vinyl acetate, 30 to 40% by weight of n-butyl acrylate, 10 to 30% by weight of dibutyl maleate and 5 to 15% by weight of a copolymerizable unsaturated carboxylic acid. Specified carboxylic acids in admixture with methylmethacrylate are acrylic, methacrylic or a mixture thereof and crotonic acid is specified as the carboxylic acid present in the copolymer. The sheets may be of metal. Also disclosed is a plate applied to one surface of which is a layer of a graft polymer as specified above.
-
公开(公告)号:DK122181B
公开(公告)日:1972-01-31
申请号:DK592868
申请日:1968-12-04
Applicant: HOECHST AG
Inventor: SCHOMMER A , EBIGT J , DUVE G , OBERST H
Abstract: 1,246,996. Vibration damping laminates. FARBWERKE HOECHST A.G. 4 Dec., 1968 [ 6 Dec., 1967], No. 57603/68. Heading B5N. [Also in Divisions B2 and C3] A vibration damping laminated system comprises two plates, e.g. of metal such as steel, bonded together with an interlayer comprising a graft polymer of 40-80% by weight of styrene or a mixture thereof with 0À1-10% by weight based on the styrene of a copolymerizable carboxylic acid, e.g. acrylic and/or methacrylic acid, an 60-20% by weight of a copolymer of 30-40% by weight of vinyl acetate, 30-40% by weight of n-butyl acrylate, 10-30% by weight of di-n-butyl maleate and 5-15% by weight of a copolymerizable unsaturated carboxylic acid, e.g. crotonic acid. The graft polymer may be cross-linked with a compound containing a plurality of epoxide or isocyanate groups. The graft polymer may contain minor amounts of fillers, e.g. heavy spar, silicic acid, graphite, soot or a mixture thereof, and one or more plasticizers. The total thickness of the laminated system may be 1-6 mm., the thickness of the interlayer being 0À1-1 mm. and the ratio of the thickness of the plates being from 1 : 1 to 4 : 1. The graft polymer may be applied to the plates by trowelling, brushing or pouring at an elevated temperature and the system cooled under pressure between rollers. A solution of the copolymer in styrene or styrene and acrylic and/or methacrylic acid mixture containing a polymerization initiator, e.g. tertiary butyl hydroperoxide may be applied between the plates and the laminated system subjected to heating at 60-180‹ C. to effect grafting.
-
公开(公告)号:DK122179B
公开(公告)日:1972-01-31
申请号:DK593268
申请日:1968-12-04
Applicant: HOECHST AG
Inventor: SCHOMMER A , EBIGT J , DUVE G , OBERST H
IPC: C08F291/00 , E04B1/98 , C08F29/00 , B32B15/08 , C08J1/40
Abstract: 1,245,470. Laminates. FARBWERKE HOECHST A.G. 4 Dec., 1968 [5 Sept., 1967], No. 67605/68. Heading B5N. [Also in Divisions B2 and F2] A vibration damping laminated system comprises two sheets and bonded to the sheets an interlayer comprising a graft polymer of 40 to 80% by weight of methylmethacrylate or a mixture of methylmethacrylate with from 0À1 to 10% by weight of a copolymerizable carboxylic acid, or 60 to 20% by weight of a copolymer formed from a monomer mixture of 30 to 40% by weight of vinyl acetate, 30 to 40% by weight of n-butyl acrylate, 10 to 30% by weight of dibutyl maleate and 5 to 15% by weight of a copolymerizable unsaturated carboxylic acid. Specified carboxylic acids in admixture with methylmethacrylate are acrylic, methacrylic or a mixture thereof and crotonic acid is specified as the carboxylic acid present in the copolymer. The sheets may be of metal. Also disclosed is a plate applied to one surface of which is a layer of a graft polymer as specified above.
-
公开(公告)号:SE337933B
公开(公告)日:1971-08-23
申请号:SE1609667
申请日:1967-11-23
Applicant: HOECHST AG
Inventor: OBERST H , EBIGT J , DUVE G , SCHOMMER A
IPC: C09J131/04 , C09J133/08 , C08J1/40 , E04B1/90 , F16F15/04
-
公开(公告)号:SE330988B
公开(公告)日:1970-12-07
申请号:SE558767
申请日:1967-04-20
Applicant: HOECHST AG
Inventor: OBERST H , DUVE G , SCHOMMER A , REIHS L , EBIGT J
-
-
公开(公告)号:SE360099B
公开(公告)日:1973-09-17
申请号:SE1650268
申请日:1968-12-03
Applicant: HOECHST AG
Inventor: OBERST H , EBIGT J , DUVE G , SCHOMMER A
IPC: C08F291/00 , F16K11/052 , B32B15/08 , C08J1/40 , E04B1/86 , F16F15/00 , G10K11/00
Abstract: 1,246,997. Vibration damping laminates. FARBWERKE HOECHST A.G. 4 Dec., 1968 [6 Dec., 1967], No. 57606/68. Heading B5N. [Also in Divisions B2 and C3] A vibration damping laminated system comprises two plates, e.g. of metal such as steel, bonded together with an interlayer comprising a graft polymer of 40-80% by weight of a equimolar mixture of styrene and acrylonitrile on 60-20% by weight of a copolymer of 30-40% by weight of vinyl acetate, 30-40% by weight of 2-ethylhexyl acrylate, 10-30% by weight di-n-butyl maleate and 5-15% by weight of a copolymerizable unsaturated caroxylic acid, e.g. crotonic acid. The graft polymer may be cross-linked with a compound containing a plurality of epoxide or isocyanate groups. The graft polymer may contain minor amounts of fillers, e.g. heavy spar, silicic acid, graphite, soot or a mixture thereof, and one or more plasticizers. The total thickness of the laminated system may be 1-6 mm., the thickness of the interlayer being 0À1-1 mm. and the ratio of the thickness of the plates being from 1 : 1 to 4 : 1. The graft polymer may be applied to the plates by trowelling, brushing or pouring at an elevated temperature and the system cooled under pressure between rollers. A solution of the copolymer in the mixture of styrene and acrylonitrile containing a polymerization initiator, e.g. tertiary butyl hydroperoxide, may be applied between the plates and the laminated system subjected to heating at 60-180 C. to effect grafting.
-
公开(公告)号:SE360098B
公开(公告)日:1973-09-17
申请号:SE1650168
申请日:1968-12-03
Applicant: HOECHST AG
Inventor: OBERST H , EBIGT J , DUVE G , SCHOMMER A
Abstract: 1,246,996. Vibration damping laminates. FARBWERKE HOECHST A.G. 4 Dec., 1968 [ 6 Dec., 1967], No. 57603/68. Heading B5N. [Also in Divisions B2 and C3] A vibration damping laminated system comprises two plates, e.g. of metal such as steel, bonded together with an interlayer comprising a graft polymer of 40-80% by weight of styrene or a mixture thereof with 0À1-10% by weight based on the styrene of a copolymerizable carboxylic acid, e.g. acrylic and/or methacrylic acid, an 60-20% by weight of a copolymer of 30-40% by weight of vinyl acetate, 30-40% by weight of n-butyl acrylate, 10-30% by weight of di-n-butyl maleate and 5-15% by weight of a copolymerizable unsaturated carboxylic acid, e.g. crotonic acid. The graft polymer may be cross-linked with a compound containing a plurality of epoxide or isocyanate groups. The graft polymer may contain minor amounts of fillers, e.g. heavy spar, silicic acid, graphite, soot or a mixture thereof, and one or more plasticizers. The total thickness of the laminated system may be 1-6 mm., the thickness of the interlayer being 0À1-1 mm. and the ratio of the thickness of the plates being from 1 : 1 to 4 : 1. The graft polymer may be applied to the plates by trowelling, brushing or pouring at an elevated temperature and the system cooled under pressure between rollers. A solution of the copolymer in styrene or styrene and acrylic and/or methacrylic acid mixture containing a polymerization initiator, e.g. tertiary butyl hydroperoxide may be applied between the plates and the laminated system subjected to heating at 60-180‹ C. to effect grafting.
-
公开(公告)号:SE360097B
公开(公告)日:1973-09-17
申请号:SE1650068
申请日:1968-12-03
Applicant: HOECHST AG
Inventor: OBERST H , EBIGT J , DUVE G , SCHOMMER A
Abstract: 1,247,196. Vibration damping laminates. FARBWERKE HOECHST A.G. 5 Dec., 1968 [6 Dec., 1967], No. 57842/68. Heading B5N. [Also in Divisions B2 and C3] A vibration damping laminated system comprises two plates, e.g. of metal such as steel, bonded together with an interlayer comprising a graft polymer of 40-80% by weight of methyl methacrylate or a mixture thereof with 0À1- 10% by weight based on the methyl methacrylate of a copolymerizable carboxylic acid, e.g. acrylic and/or methacrylic acid, or 60- 20% by weight of a copolymer of 30-40% by weight of vinyl acetate, 30-40% by weight of 2-ethyl hexyl acrylate, 10-30% by weight of di-n-butyl maleate and 5-15% by weight of a copolymerizable unsaturated carboxylic acid, e.g. crotonic acid. The graft polymer may be cross-linked with a compound containing a plurality of epoxide or isocyanate groups. The graft polymer may contain minor amounts of fillers, e.g. heavy spar, silicic acid, graphite, soot or a mixture thereof, and one or more plasticizers. The total thickness of the laminated system may be 1-6 mm., the thickness of the interlayer being 0À1-1 mm. and the ratio of the thickness of the plates being from 1 : 1 to 4 : 1. The graft polymer may be applied to the plates by travelling, brushing or pouring at an elevated temperature and the system cooled under pressure between rollers. A solution of the copolymer in methyl methacrylate or methyl methacrylate and acrylic and/or methacrylic acid mixture containing a polymerization initiator, e.g. tertiary butyl hydroperoxide, may be applied between the plates and the laminated system subjected to heating at 60-180 C. to effect grafting.
-
-
-
-
-
-
-
-
-