26.
    发明专利
    未知

    公开(公告)号:DK150989D0

    公开(公告)日:1989-03-29

    申请号:DK150989

    申请日:1989-03-29

    Applicant: LUBRIZOL CORP

    Abstract: A process for preparing a lower alkene polymer from a lower alkene feedstream, including the steps of: (A) contacting the lower alkene monomer with a catalyst system comprising boron trifluoride and at least one acid selected from the group consisting of sulfuric acid, sulfurous acid, phosphoric acids and strong acid resins and (B) polymerizing the lower alkene monomer in the presence of the catalyst system at a temperature of about -3 DEG C. to about -30 DEG C. thereby obtaining a lower alkene polymer having a molecular weight of about 250 to about 500.

    27.
    发明专利
    未知

    公开(公告)号:NO891120D0

    公开(公告)日:1989-03-15

    申请号:NO891120

    申请日:1989-03-15

    Applicant: LUBRIZOL CORP

    Abstract: A process for preparing a lower alkene polymer from a lower alkene feedstream, including the steps of: (A) contacting the lower alkene monomer with a catalyst system comprising boron trifluoride and at least one acid selected from the group consisting of sulfuric acid, sulfurous acid, phosphoric acids and strong acid resins and (B) polymerizing the lower alkene monomer in the presence of the catalyst system at a temperature of about -3 DEG C. to about -30 DEG C. thereby obtaining a lower alkene polymer having a molecular weight of about 250 to about 500.

    LOWER ALKENE POLYMERS
    28.
    发明专利

    公开(公告)号:AU2138288A

    公开(公告)日:1989-03-01

    申请号:AU2138288

    申请日:1988-06-29

    Applicant: LUBRIZOL CORP

    Abstract: A process for preparing a lower alkene polymer from a lower alkene feedstream, including the steps of: (A) contacting the lower alkene monomer with a catalyst system comprising boron trifluoride and at least one acid selected from the group consisting of sulfuric acid, sulfurous acid, phosphoric acids and strong acid resins and (B) polymerizing the lower alkene monomer in the presence of the catalyst system at a temperature of about -3 DEG C. to about -30 DEG C. thereby obtaining a lower alkene polymer having a molecular weight of about 250 to about 500.