公开(公告)号:AU2012246194B2
公开(公告)日:2017-10-05
申请号:AU2012246194
申请日:2012-04-18
Applicant: OUTOKUMPU OY
Inventor: OLIVER JAMES , JONSSON JAN Y , TALONEN JUHO , PETTERSSON RACHEL , ANDERSSON JAN-OLOF
Abstract: The invention relates to a method for manufacturing a ferritic-austenitic stainless steel having good formability, good weldability and high elongation. The stainless steel containing the sum of carbon and nitrogen C+N in the range 0,17 - 0,295 in weight % in which sum C+N a lower carbon content to avoid sensitisation during welding is compensated by an increased nitrogen content to maintain formability is heat treated so that the microstructure of the stainless steel contains 45-75 % austenite in the heat treated condition, the remaining microstructure being ferrite, and the measured M
-
公开(公告)号:EA024633B1
公开(公告)日:2016-10-31
申请号:EA201290986
申请日:2011-04-18
Applicant: OUTOKUMPU OY
Inventor: TALONEN JUHO , TAULAVUORI TERO , KODUKULA SURESH
IPC: C22C38/58 , C21C5/00 , C22C38/40 , C22C38/42 , C22C38/44 , C22C38/46 , C22C38/48 , C22C38/50 , C22C38/54
Abstract: Изобретениеотноситсяк аустенитнойнержавеющейсталис низкимсодержаниемникеля, обладающейвысокойстойкостьюк замедленномутрещинообразованию. Изобретениетакжеотноситсяк применениютакойстали. Стальсодержит, мас.%: углерод - 0,02-0,15, марганец - 7-15, хром - 14-19, никель - 0,1-4, медь - 0,1-3, азот - 0,05-0,3, аостатокдо 100% составляютжелезои неизбежныепримеси, приэтомхимическийсоставсталив пересчетенасуммарноесодержаниеуглеродаи азота (C+N) иизмереннаятемпература Mнаходятсявнутриобласти, ограниченнойточками ABCD, которыеимеютследующиезначения:
-
公开(公告)号:AU2011249711B2
公开(公告)日:2016-05-12
申请号:AU2011249711
申请日:2011-04-18
Applicant: OUTOKUMPU OY
Inventor: TALONEN JUHO , TAULAVUORI TERO , KODUKULA SURESH
IPC: C22C38/58 , C21C5/00 , C22C38/40 , C22C38/42 , C22C38/44 , C22C38/46 , C22C38/48 , C22C38/50 , C22C38/54
Abstract: The invention relates to a low-nickel austenitic stainless steel with high resistance to delayed cracking and the use of the steel. The steel contains in weight % 0,02 - 0,15 % carbon, 7 - 15 % manganese, 14 - 19 % chromium, 0,1 - 4 % nickel, 0,1 - 3 % copper, 0,05 - 0,3 % nitrogen, the balance of the steel being iron and inevitable impurities, and the chemical composition range in terms of the sum of carbon and nitrogen contents (C+N) and the measured Md3o-temperature is inside the area defined by the points ABCD which have the following values Point M
-
公开(公告)号:MX2015017548A
公开(公告)日:2016-04-26
申请号:MX2015017548
申请日:2014-06-19
Applicant: OUTOKUMPU OY
Inventor: TALONEN JUHO
Abstract: La invención se relaciona con un acero inoxidable que muestra efecto de plasticidad inducido por transformación (TRIP) y que es resistente al agrietamiento retardado; así como también al método para producir el acero inoxidable. La resistencia al agrietamiento retardado en el acero inoxidable se logra al limitar el contenido de hidrogeno total del acero inoxidable medido por el método de fusión de gas inerte por debajo de 4 ppm en peso, preferiblemente debajo de 3 ppm en peso, por medio de un tratamiento con calor llevado a cabo a un rango de temperatura de entre 100 °C y 700 °C por 0.1-300 horas, preferiblemente a 200-600 °C por 1-100 horas, y más preferiblemente a 250-500 °C por 1-100 horas.
-
25.
公开(公告)号:FI20136077A
公开(公告)日:2015-05-05
申请号:FI20136077
申请日:2013-11-04
Applicant: OUTOKUMPU OY
Inventor: TALONEN JUHO , HÄNNINEN HANNU , FORSSTRÖM ANTTI
-
公开(公告)号:MX2012012874A
公开(公告)日:2012-11-29
申请号:MX2012012874
申请日:2011-04-18
Applicant: OUTOKUMPU OY
Inventor: TALONEN JUHO , KODUKULA SURESH , TAULAVUORI TERO
IPC: C22C38/58 , C21C5/00 , C22C38/40 , C22C38/42 , C22C38/44 , C22C38/46 , C22C38/48 , C22C38/50 , C22C38/54
Abstract: La invención se refiere a un acero inoxidable austenítico, al bajo níquel, con elevada resistencia al agrietamiento retardado, y al uso de este acero. El acero contiene en % peso 0.02 - 0.15% de carbono; 7 -15% de manganeso; 14 - 19% de cromo; 0.1 - 4% de níquel; 0.1- 3% de cobre; 0.05 - 0.3% de nitrógeno, el resto del acero siendo fierro e impurezas inevitables, y el intervalo de la composición química en términos de la suma de los contenidos de carbono y nitrógeno (C+N) y la temperatura Md30 medida está dentro del área definida por los puntos ABCD que tienen los siguientes valores: Punto Md30 °C C+N % A -80 0.1 B +7 0.1 C -40 0.40 D -80 0.40.
-
公开(公告)号:CA2832921A1
公开(公告)日:2012-10-26
申请号:CA2832921
申请日:2012-04-18
Applicant: OUTOKUMPU OY
Inventor: OLIVER JAMES , JONSSON JAN Y , TALONEN JUHO , PETTERSSON RACHEL , ANDERSSON JAN-OLOF
Abstract: The invention relates to a method for manufacturing a ferritic-austenitic stainless steel having good formability, good weldability and high elongation. The stainless steel containing the sum of carbon and nitrogen C+N in the range 0,17 - 0,295 in weight % in which sum C+N a lower carbon content to avoid sensitisation during welding is compensated by an increased nitrogen content to maintain formability is heat treated so that the microstructure of the stainless steel contains 45-75 % austenite in the heat treated condition, the remaining microstructure being ferrite, and the measured Md30 temperature of the stainless steel is adjusted between 0 and 50 °C in order to utilize the transformation induced plasticity (TRIP) for improving the formability of the stainless steel.
-
28.
公开(公告)号:ES2781864T3
公开(公告)日:2020-09-08
申请号:ES11774473
申请日:2011-04-18
Applicant: OUTOKUMPU OY
Inventor: OLIVER JAMES , JONSSON JAN Y , TALONEN JUHO
Abstract: Método para fabricar un acero inoxidable ferrítico-austenítico que tiene buena conformabilidad y alto alargamiento, en donde el acero inoxidable contiene % en peso, de menos de 0,05% de C, 0,2-0,7% de Si, 2-5% de Mn, 19 -20,5% de Cr, 0,8- 1,35% de Ni, menos de 0,6% de Mo, menos de 1% de Cu, 0,16-0,24% de N, el resto Fe e impurezas inevitables 0-50 ppm de O, 0-50 ppm de S y 0-0,04% de P, que contiene opcionalmente uno o más elementos añadidos; 0-0,5% de W, 0-0,2% de Nb, 0-0,1% de Ti, 0-0,2% de V, 0-0,5% de Co, 0-50 ppm de B y 0-0,04% de Al, en donde el método comprende el tratamiento térmico del acero inoxidable a una temperatura en el intervalo de 900 - 1200 °C, de modo que la microestructura del acero inoxidable contenga 45 - 75% de austenita en la condición tratada térmicamente, siendo la microestructura restante ferrita y por lo que se ajusta la temperatura Md30 medida del acero inoxidable, y por lo que el acero tiene temperatura Md30 medida entre 0 y 50 °C después del tratamiento térmico con el fin de utilizar la plasticidad inducida por transformación (TRIP) para mejorar la conformabilidad del acero inoxidable, en donde temperatura Md30 se mide como se describe en la descripción.
-
29.
公开(公告)号:CA2796417C
公开(公告)日:2019-05-21
申请号:CA2796417
申请日:2011-04-18
Applicant: OUTOKUMPU OY
Inventor: OLIVER JAMES , JONSSON JAN Y , TALONEN JUHO
Abstract: The invention relates to a method for manufacturing a ferritic-austenitic stainless steel having good formability and high elongation. The stainless steel is heat treated so that the microstructure of the stainless steel contains 45 - 75 % austenite in the heat treated condition, the remaining microstructure being ferrite, and the measured Md30 temperature of the stainless steel is adjusted between 0 and 50 °C in order to utilize the transformation induced plasticity (TRIP) for improving the formability of the stainless steel.
-
公开(公告)号:SI2699704T1
公开(公告)日:2019-04-30
申请号:SI201231546
申请日:2012-04-18
Applicant: OUTOKUMPU OY
Inventor: OLIVER JAMES , JONSSON JAN Y , TALONEN JUHO , PETTERSSON RACHEL , ANDERSSON JAN-OLOF
-
-
-
-
-
-
-
-
-