公开(公告)号:JPH10329411A
公开(公告)日:1998-12-15
申请号:JP14382297
申请日:1997-06-02
Applicant: TORAY INDUSTRIES
Inventor: NAKAHARA KATSUJI , IKEDA MIKITO
Abstract: PROBLEM TO BE SOLVED: To obtain a good ink absorption property, water resistivity, and moisture proof making the ratio of glossiness of yellow, cyan, and magenta after printing relative to the glossiness of an ink receptacle layer before printing in JIS 88741, larger than a specific value. SOLUTION: The relation between the glossiness G1 of a receptacle layer before printing and the glossiness G2 of yellow, cyan, and magenta after printing is preferably to be G2/G1>=0.5 (preferably 0.6), and if it is less than 0.5, the coloring property (glossiness) of printing pictures tends to lower. In addition, each glossiness G2 of yellow, cyan, and magenta after printing is preferable to be 50% or more, and more preferably, to be 55% or more. Furthermore, the relation between the thickness d1 of a lower layer consisting mainly of a cationic copolymer and cross-linked polyalkylene oxide resin and the thickness d2 of an upper layer consisting mainly of hydrophilic polymeric resin is preferable to be d1>=d2, and as d2 exceeds d1, water resistiveness or moisture preventiveness becomes low.
-
公开(公告)号:JPH10263133A
公开(公告)日:1998-10-06
申请号:JP7819097
申请日:1997-03-28
Applicant: TORAY INDUSTRIES
Inventor: SHIMIZU KUNIMITSU , NAKAHARA KATSUJI , IKEDA MIKITO
Abstract: PROBLEM TO BE SOLVED: To make snow and soil be easily removable and to reduce damage, etc., of a ski board at a low temperature to make the ski board be excellent in sliding on snow, soilproof, easily washing, and weather resistance by forming an adhesive layer on a fluororesin film. SOLUTION: This protective film for a ski board is made by laminating an adhesive layer 2 on a fluororesin film 1. The reason why the fluororesin film is used is because the film has proper flexibility to make the film be easily and quickly adhered on a ski board and is hard to be adhered by snow and ice at a low temperature to slip them off. By using the fluororesin film 1 with those features as a protective film for a ski board, the serviceability and the application performance are made excellent by far. As the fluororesin film 1, undrawn ETFE film of a copolymer of tetrafluoroethylene and ethylene is especially effective by mechanical strength and flexibility. The thickness of the fluororesin film 1 is not limited, but 0.5-500 μm is preferable.
-
公开(公告)号:JPH09295391A
公开(公告)日:1997-11-18
申请号:JP11260796
申请日:1996-05-07
Applicant: TORAY INDUSTRIES
Inventor: NAKAHARA KATSUJI , IKEDA MIKITO , WACHI TAKAAKI
Abstract: PROBLEM TO BE SOLVED: To provide a recording sheet excellent in silicone oil and ink absorbabiity, toner fixing properties, printability and water resistance by coating the single surface of a plastic film with a recording layer based on a crosslinked polyalkylene oxide resin, colloidal silica, a hydrophilic polymeric resin and a fluorine type surfactant. SOLUTION: This recording sheet is constituted by coating at least the single surface of a plastic film with a recording layer based on a crosslinked polyalkylene oxide resin, colloidal silica, a hydrophilic polymeric resin and a fluorine type surfactant. As a recording layer coating method, there is no limit but a known method such as a gravure coating method, a reverse coating method, a die coating method or a bar coating method can be adapted. If necessary, by executing known surface treatment such as corona discharge treatment or primer treatment within air or other atmosphere before coating, coating properties are improved and the recording layer can be strongly formed on the film.
-
公开(公告)号:JPH09183159A
公开(公告)日:1997-07-15
申请号:JP28701496
申请日:1996-10-29
Applicant: TORAY INDUSTRIES
Inventor: SHIMIZU KUNIMITSU , NAKAHARA KATSUJI , IKEDA MIKITO
IPC: A01G9/14 , B29C65/00 , B29C65/02 , B29K27/12 , B29L9/00 , B29L31/10 , B32B7/10 , B32B27/18 , B32B27/30
Abstract: PROBLEM TO BE SOLVED: To prevent a peeling from the bonded part or a breaking from generating, and provide a bonded sheet material which is excellent in transparency by specifying the tensile shear bonding strength of the bonded part wherein the end parts in the width direction of a plastic film are bonded under a state being superposed to each other. SOLUTION: This bonded sheet has a bonded part wherein the end parts in the width direction of a plastic film are bonded under a state being superposed to each other, and the tensile shear bonding strength of the bonded part is 1kgf/cm or higher. There is no special specification for the bonding method of the bonded part, and heat-sealing such as hot plate method, roller method, or slide-sealing method, impulse sealing, ultrasonic sealing, high frequency sealing or laminating with an adhesive or hot adhesive, etc., can be mentioned. Also, the light transmittance of the bonded part is 50% or higher, the haze is less than 70%, and the bonded part is bonded extending to the total width of the superposed part. Also, the plastic film contains an ultraviolet absorbent.
-
公开(公告)号:JPH0957893A
公开(公告)日:1997-03-04
申请号:JP22065195
申请日:1995-08-29
Applicant: TORAY INDUSTRIES
Inventor: TANAKA IWAO , IKEDA MIKITO , NAGURA SATOSHI
IPC: B05D7/04 , A01N59/16 , A01N61/00 , B05D7/24 , B32B9/00 , C08J7/06 , C08K3/00 , C08L67/00 , C08L67/02 , C08L101/00
Abstract: PROBLEM TO BE SOLVED: To obtain an antibacterial oriented plastic film which has a strong antibacterial effect and can maintain the antibacterial function over a long period of time. SOLUTION: An inorganic compound 2 containing silver 1μm or less in particle size is fixed on the surface of a plastic film 1 which has surface roughness (Ra) of 0.2μm or more, maximum roughness (Rt) of 1μm or more, and 5 pieces/mm or more of roughness (Pc) of 0.5μm or more.
-
公开(公告)号:JPH0947704A
公开(公告)日:1997-02-18
申请号:JP21967695
申请日:1995-08-04
Applicant: TORAY INDUSTRIES
Inventor: YOKOI TADAO , IKEDA MIKITO
Abstract: PROBLEM TO BE SOLVED: To form a coating film excellent in uniformity and appearance by preventing coating defects particularly caused by the foaming of a coating material in pan supply type coating. SOLUTION: In a pan supply type coating device for applying the coating material 2 on the surface of a traveling base material 4 by housing the coating material 2 in a pan 1 and using a rotating roll 3, a pant of the surface of which is dipped in the coating material 2, liquid-in doctor blades 11, 14 respectively opposed to the surface of the roll 3 are provided in the inlet side or inlet side and outlet side of the surface of the roll to the coating material 2 in the rotary direction of the rotating roll 3 and under the liquid of the coating material 2.
-
公开(公告)号:JPH078699A
公开(公告)日:1995-01-13
申请号:JP18451093
申请日:1993-06-28
Applicant: TORAY INDUSTRIES
Inventor: SUGIURA SEIYA , IKEDA MIKITO
IPC: D06F93/00
Abstract: PURPOSE:To easily read characters or marks even after a processing without being affected by the processing by a method wherein a printing is done on one surface of a base material made of a heat-resistant, water-resistant and chemical-resistant synthetic resin, and on the opposite surface to the printed surface, an heat-resistant, water-resistant and chemical-resistant adhesive is applied. CONSTITUTION:A polyester film is used as a base film, and on one surface of the film, a printing is applied. Then, in a diluted solvent of toluene/ethyl acetate, a composition, for which 60 pts.wt. of a solid component of a thermally crosslinkable acrylic resin is blended with 40 pts.wt. per solid component of titanium oxide, which is a whitening pigment, is evenly diffused, and a coating agent with a concentration of 10wt.% is prepared. Then, the coating agent is applied onto the base film by the gravure coating method, and the coated layer is dried to complete a film for a printing-receiving layer. By this method, a label with excellent heat-resistance, water-resistance and chemical-resistance can be obtained, and the label is not dyed or discolored in the process of dying of a cloth.
-
公开(公告)号:JPH1110813A
公开(公告)日:1999-01-19
申请号:JP16754397
申请日:1997-06-24
Applicant: TORAY INDUSTRIES
Inventor: YOKOI TADAO , IKEDA MIKITO
IPC: B32B27/36
Abstract: PROBLEM TO BE SOLVED: To make an easy adhesion film excellent in adhesion between layers, suitability for thermal lamination of PVC, etc., by constituting a macromolecular binding agent out of modified polyester resin containing a vinyl group or of the modified polyester resin containing the vinyl group and chlorinated olefin resin. SOLUTION: An easy adhesion film is formed by providing a receptive layer containing a macromolecular binding agent, a crosslinking agent and a lubricant on one surface of a base at least. Although polyester, acrylic, polyurethane resins and the like can be used for the macromolecular binding agent, copolymer polyester resin obtained by grafting a compound having an unsaturated bond, or the copolymer polyester resin obtained by grafting the compound having the unsaturated bond, and chlorinated olefin resin obtained by chlorinating polyolefin, are used among them. The copolymer polyester resin obtained by grafting the compound having the unsaturated bond is obtained by grafting the compound having the unsaturated bond onto polyester resin containing a polar group.
-
公开(公告)号:JPH115894A
公开(公告)日:1999-01-12
申请号:JP16153397
申请日:1997-06-18
Applicant: TORAY INDUSTRIES
Inventor: YOKOI TADAO , IKEDA MIKITO
Abstract: PROBLEM TO BE SOLVED: To obtain a recording film excellent in carriability, whiteness, coverability, UV light printing suitability, carbon receiving suitability, heat transfer printing suitability, electrophotographic printing suitability, etc., by disposing a specific receiving layer on at least one surface of a substrate. SOLUTION: This recording film is produced by disposing a receiving layer preferably having a thickness of 1-8 μm and a lubricity of >=20 sec on at least one surface of a substrate preferably comprising a white polyester film having an apparent specific gravity of 0.6-1.5 and a whiteness of >=50%. The receiving layer comprises a polymer hinder comprising a modified polyester resin such as a polar group-containing polyester or a copolyester resin grafted with an unsaturated bond-containing compound, a quaternary ammonium salt polymer, and inorganic particles and/or organic particles preferably comprising amorphous silica consisting mainly of silicon dioxide and having an average particle diameter of 0.5-5 μm and an oil absorption of 200-500 ml/100 g.
-
公开(公告)号:JPH10329407A
公开(公告)日:1998-12-15
申请号:JP14010497
申请日:1997-05-29
Applicant: TORAY INDUSTRIES
Inventor: NAKAHARA KATSUJI , IKEDA MIKITO
Abstract: PROBLEM TO BE SOLVED: To obtain a superior ink absorption property, water resistiveness, and moisture proof by containing a cross-linked polyalkyleneoxide resin in the ink receptacle layer, and making a solubility rate in one minute of water immersion into a specific percent age or lower in a recording sheet having an ink receptacle layer provided, at least, on one surface of a base material. SOLUTION: The solubility rate of an ink receptacle layer in one minute of water immersion is required to be 50% or lower and, more preferably, to be 40% or lower and, further preferably, to be 20%. When the solubility rate exceeds 50%, print images tend to flow. Also, the receptacle layer is preferable to have a lower layer consisting mainly of a cationic copolymer and polyalkylene oxide resin and an upper layer consisting mainly of hydrophilic polymeric resin for the enhancement of a coloring property (glossiness), and the relation is preferably to be d1>=d2 between the thickness d1 of the lower layer consisting mainly of a cationic copolymer and polyalkylene oxide resin and the thickness d2 of the upper layer consisting mainly of hydrophilic resin. When d2 comes beyond d1, the water resistiveness or moisture proof lowers.
-
-
-
-
-
-
-
-
-