Light-amplifying optical fiber and method of making the same
    361.
    发明授权
    Light-amplifying optical fiber and method of making the same 有权
    光放大光纤及其制造方法

    公开(公告)号:US06687439B1

    公开(公告)日:2004-02-03

    申请号:US09674071

    申请日:2000-10-26

    Abstract: The present invention relates to a light-amplifying optical fiber comprising a structure for realizing a flat gain characteristic or oscillation characteristic in a wider wavelength band, and a method of making the same. The light-amplifying optical fiber according to the present invention comprises a second doped area containing a first doped area including an optical axis center and having a larger outer diameter than the first doped area. The second doped area is doped with at least one of Al2O3, P2O5, Y2O3, and B2O3 as an oxide of an element having a valence different from that of a cation constituting a main material of the light-amplifying optical fiber; whereas the first doped area is doped with at least one of Er, Nd, Tm, Yb, and Pr as a rare-earth element together with the oxide.

    Abstract translation: 本发明涉及一种包括用于实现更宽波长带中的平坦增益特性或振荡特性的结构的光放大光纤及其制造方法。根据本发明的光放大光纤包括: 第二掺杂区域包含包含光轴中心并且具有比第一掺杂区域更大的外径的第一掺杂区域。 掺杂有Al 2 O 3,P 2 O 5,Y 2 O 3和B 2 O 3中的至少一种作为与构成光放大光纤的主要材料的阳离子的价态不同的元素的氧化物的第2掺杂区域; 而第一掺杂区域与氧化物一起掺杂有Er,Nd,Tm,Yb和Pr中的至少一种作为稀土元素。

    Sol-gel-derived optical fiber preform and method of manufacture
    365.
    发明申请
    Sol-gel-derived optical fiber preform and method of manufacture 失效
    溶胶凝胶衍生的光纤预制棒及其制造方法

    公开(公告)号:US20030147605A1

    公开(公告)日:2003-08-07

    申请号:US10062748

    申请日:2002-02-01

    Abstract: A method forms an optical fiber preform. The method includes forming a sol-gel-derived rod having a first diameter. Forming the sol-gel-derived rod includes preparing a sol-gel solution including at least 3 mole % of a catalyst. The sol-gel solution is allowed to undergo gelation to form a wet gel monolith. The wet gel monolith is dried and shrunk by exposing the wet gel monolith to a temporal temperature profile, thereby forming a xerogel monolith. The xerogel monolith is consolidated, thereby forming the sol-gel-derived rod. The method further includes drawing the sol-gel-derived rod to substantially reduce its diameter, thereby forming a drawn rod having a second diameter less than the first diameter.

    Abstract translation: 一种方法形成光纤预制件。 该方法包括形成具有第一直径的溶胶 - 凝胶衍生的棒。 形成溶胶 - 凝胶衍生的棒包括制备包含至少3摩尔%的催化剂的溶胶 - 凝胶溶液。 使溶胶 - 凝胶溶液进行凝胶化以形成湿凝胶整料。 通过将湿凝胶整料暴露于时间温度曲线,将湿凝胶整料干燥并收缩,从而形成干凝胶整料。 将干凝胶整料固结,从而形成溶胶 - 凝胶衍生的棒。 该方法还包括拉伸溶胶 - 凝胶衍生的棒以大大减小其直径,由此形成具有小于第一直径的第二直径的拉伸杆。

    Multi-layer burner module, adapter, and assembly therefor
    367.
    发明申请
    Multi-layer burner module, adapter, and assembly therefor 有权
    多层燃烧器模块,适配器及其组装

    公开(公告)号:US20030113679A1

    公开(公告)日:2003-06-19

    申请号:US10027846

    申请日:2001-12-19

    Abstract: A burner module for delivering a flow of chemical reactants to a combustion site of a chemical vapor deposition process includes a plurality of substantially planar layers. The substantially planar layers are arranged in a generally parallel and fixed relationship and define an inlet, an outlet and a passage fluidly connecting the inlet and outlet. At least one of the layers is a distribution layer having a plurality of apertures therethrough and fluidly communicating with the passage. The plurality of apertures collectively define a non-uniform pattern arranged and configured to improve the uniformity of a flow out through the outlet. Burner adapter and assembly embodiments are also included.

    Abstract translation: 用于将化学反应物流输送到化学气相沉积工艺的燃烧部位的燃烧器模块包括多个基本平坦的层。 基本上平面的层被布置成大致平行和固定的关系,并且限定入口,出口和流体连接入口和出口的通道。 层中的至少一个是具有穿过其并与通道流体连通的多个孔的分布层。 多个孔共同限定了布置和配置为改善通过出口流出的均匀性的不均匀图案。 还包括燃烧器适配器和组装实施例。

    Dispersion control fiber and method of manufacturing large size preform thereof
    370.
    发明申请
    Dispersion control fiber and method of manufacturing large size preform thereof 有权
    分散控制纤维及其制造大尺寸预型体的方法

    公开(公告)号:US20020186955A1

    公开(公告)日:2002-12-12

    申请号:US10166095

    申请日:2002-06-11

    Abstract: A dispersion control fiber and a method of manufacturing a large size preform. The dispersion control fiber comprises a core composed of SiO2, GeO2, and P2O5, and a cladding composed of SiO2, GeO2, P2O5, and Freon. The P2O5 content is selected not to exceed 10% of the total weight of a compound composing the core. The method of manufacturing a large size preform for a dispersion control fiber by an MCVD process comprising depositing SiO2, GeO2, P2O5, and Freon in an inner periphery of a deposition tube to form a cladding layer, and depositing SiO2, GeO2, and P2O5 on an inner periphery of the cladding layer to form a core layer.

    Abstract translation: 一种分散控制纤维及其制造方法。 色散控制纤维包括由SiO 2,GeO 2和P 2 O 5组成的芯,以及由SiO 2,GeO 2,P 2 O 5和氟利昂组成的包层。 选择P2O5含量不超过构成核心的化合物总重量的10%。 通过MCVD方法制造用于分散控制纤维的大尺寸预成型体的方法包括在沉积管的内周中沉积SiO 2,GeO 2,P 2 O 5和氟利昂以形成包覆层,并将SiO 2,GeO 2和P 2 O 5沉积在 包层的内周,形成芯层。