Abstract:
An aqueous lubricant for use in plastic working of a metallic material which comprises (A) a water soluble inorganic salt and (B) a wax, wherein the components are dissolved or dispersed in water, and wherein a solid concentration ratio (weight ratio) (B)/(A) is 0. 3 SIMILAR 1.5. and a method for producing a lubricative film, characterized in that a lubricative film is produced by applying the aqueous lubricant, preferably in a dried weight of 0.5 SIMILAR 40g/m , on the surface of a metallic material, providing no chemical conversion layer thereon, followed by drying. The aqueous lubricant preferably further comprises (C) a metal salt of a fatty acid in a solid concentration ratio (C) /(A) of 0.01 SIMILAR 0.4. The water soluble inorganic salt (A) is preferably selected from among a sulfate, a silicate, a borate, a molybdate and a tungstate. The wax is preferably a synthetic wax which is dispersed in water and has a melting point of 70 SIMILAR 150 DEG C. The metal salt of a fatty acid (C) is preferably obtained through reacting a saturated fatty acid having 12 SIMILAR 26 carbon atoms with a metal selected from among zinc, calcium, barium, aluminium, magnesium and lithium. The aqueous lubricant can be used for imparting excellent lubricity with ease to the surface of metal having no chemical conversion layer formed thereon.
Abstract:
식 M 2 O ·nSiO 2 (식 중, n 은 2 내지 9 의 수를 나타내고, M 은 Na, K, Li 및 NR 4 (식 중, R 은 각 R 에 대해서 독립적으로 수소원자 또는 알킬기를 나타냄) 의 적어도 1 종을 나타냄) 으로 표시되는 규산알칼리를 물에 배합하여 이루어지는 제 1 보호피막 처리제; 제 1 처리제 및 윤활제를 포함하는 제 2 보호 처리제; 처리제를 사용하여 형성된 보호 피막을 가진 금속 재료; 및 처리제를 이용하는 것을 포함하는 보호 피막 형성 방법. 제 2 처리제는 우수한 자가 윤활 특성을 가진 피막을 형성할 수 있다. 처리제를 금속 재료의 표면에 적용후 건조시키는 단순하고 용이한 방법으로, 처리제는 금속 기재의 화학적 반응을 통해 형성된 피막과 비교할 수 있는 또는 보다 우수한 내베이킹성 및 방청성을 갖는 피막을 형성시킬 수 있다
Abstract:
수용성 무기염 (A), 몰리브덴 디술파이드 및 그래파이트에서 선택되는 윤활성 제제 (B) 및 왁스 (C)를 포함하고, 이 때 이들 성분은 물에 용해되거나 분산되며, (B)/(A)의 농도비(중량비)는 1.0 내지 5.0 범위이고 (C)/(A)는 0.1 내지 1.0 범위인 것이 특징인 금속 재료의 소성 가공용 수성 윤활제. 수성 윤활제를 도포시켜 금속 재료위에 윤활성 피막이 0.5 내지 40g/m 2 의 건조 중량으로 형성되는 것이 특징인 금속 재료상 윤활성 피막의 처리 방법. 수용성 무기염 (A)는 술페이트, 실리케이트, 보레이트, 몰리브데이트 및 텅스테이트로 구성된 군으로부터 선택되는 것이 바람직하다. 바람직하게도 왁스 (C)는 물에 분산되며 70 내지 150℃의 용해점을 갖는 천연 왁스 또는 합성 왁스이다. 화학적 가공층이 형성되지 않은 금속 표면에 우수한 윤활성을 용이하게 부여하기 위해 본 수성 윤활제를 사용할 수 있다.
Abstract:
수용성 무기염 (A)와 왁스 (B)를 포함하고, 이 때 이들 성분은 물에 용해되거나 분산되며 그 고체 농도비(중량비) (B)/(A)는 0.3 내지 1.5인 것이 특징인 금속 재료의 소성 가공용 수성 윤활제 및, 그 위에 화학적 가공층이 제공되지 않은 금속 재료의 표면위에 수성 윤활제를, 바람직하게는 0.5 내지 40g/m 2 의 건조 중량으로 도포시키고, 이어서 건조시킴으로써 윤활성 피막을 제조하는 것을 특징으로 하는 윤활성 피막의 형성 방법. 바람직하게도 수성 윤활제는 추가로 지방산의 금속염 (C)를, 0.01 내지 0.4의 고체 농도비 (C)/(A)로 포함한다. 수용성 무기염 (A)는 술페이트, 실리케이트, 보레이트, 몰리브데이트 및 텅스테이트 중에서 선택되는 것이 바람직하다. 바람직하게도 왁스는 물에 분산되며 70 내지 150℃의 용해점을 갖는다. 지방산의 금속염 (C)는 12 내지 26개의 탄소 원자를 갖는 포화 지방산과 아연, 칼슘, 바륨, 알루미늄, 마그네슘 및 리튬 중에서 선택된 금속을 반응시켜 얻는 것이 바람직하다. 화학적 가공층이 형성되지 않은 금속 표면에 우수한 윤활성을 용이하게 부여하기 위해 본 수성 윤활제를 사용할 수 있다.
Abstract:
An article comprises a substrate; a coating comprising a carbon composite; and a binding layer disposed between the substrate and the coating. The carbon composite comprises carbon and a binder containing one or more of the following: SiO2; Si; B; B2O3; a metal; or an alloy of the metal; and the metal comprises one or more of the following: aluminum; copper; titanium; nickel; tungsten; chromium; iron; manganese; zirconium; hafnium; vanadium; niobium; molybdenum; tin; bismuth; antimony; lead; cadmium; or selenium.
Abstract:
A protective agent for an image bearing member of an image forming apparatus. The protective agent is applied onto a surface of the image bearing member and includes a hydrophobic organic compound (A), an inorganic fine particle (B), and an inorganic lubricant (C).
Abstract:
[OBJECTIVE] To provide a lubricant for hot plastic working which is excellent in lubricating properties, feedability and operability and will produce no adverse affects on the corrosion resistance of the products. [MEANS FOR SOLUTION] A lubricant for hot plastic working which is characterized in that the composition is comprised of, in an anhydrous condition, 50 to 80% by mass of iron oxide, 20 to 50% by mass of sodium silicate and 1 to 20% by mass of calcium oxide and that the total content of the impurities of zinc oxide, lead oxide and copper oxide is not higher than 5% by mass, where the content of the stabilizer is not counted.. This lubricant is suited for use in lubricating guide shoes in piercing-rolling of high-Cr steel species.
Abstract:
An aqueous lubricant for use in plastic working of a metallic material which comprises (A) a water soluble inorganic salt and (B) a wax, wherein the components are dissolved or dispersed in water, and wherein a solid concentration ratio (weight ratio) (B)/(A) is 0. 3 SIMILAR 1.5. and a method for producing a lubricative film, characterized in that a lubricative film is produced by applying the aqueous lubricant, preferably in a dried weight of 0.5 SIMILAR 40g/m , on the surface of a metallic material, providing no chemical conversion layer thereon, followed by drying. The aqueous lubricant preferably further comprises (C) a metal salt of a fatty acid in a solid concentration ratio (C) /(A) of 0.01 SIMILAR 0.4. The water soluble inorganic salt (A) is preferably selected from among a sulfate, a silicate, a borate, a molybdate and a tungstate. The wax is preferably a synthetic wax which is dispersed in water and has a melting point of 70 SIMILAR 150 DEG C. The metal salt of a fatty acid (C) is preferably obtained through reacting a saturated fatty acid having 12 SIMILAR 26 carbon atoms with a metal selected from among zinc, calcium, barium, aluminium, magnesium and lithium. The aqueous lubricant can be used for imparting excellent lubricity with ease to the surface of metal having no chemical conversion layer formed thereon.