Abstract:
A dielectric ceramic composition for low temperature sintering and a multi-layered ceramic condenser using the same are provided to sinter the composition under a reduction atmosphere. A dielectric ceramic composition includes (Ba(1-x)Cax)mTiO3 as a main component. The dielectric ceramic composition includes MgCO3, Re2O3, MO, MnO, V2O5, Cr2O3, and SiO2 as residue. The composition is a(Ba1-xCax)mTiO3-BMgCO3-cRe2O3-dMnO-fSiO2-gV2O5-hCr2O3.
Abstract:
본 발명은 내환원성 유전체 조성물 및 그 제조방법에 관한 것이다. 본 발명은 주성분인 (Ca 1-x Sr x ) m (Ti y Zr 1-y )O 3 (0≤x≤1, 0≤y≤0.09, 0.7≤m≤1.05) 100중량부에 대하여, aMnO-bSiO 2 -dR 1 O-eR 2 O 2 (a+b+d+e=100이며, 20≤a≤60, 10≤b≤65, 0≤d+e≤65, R 1 은 Mg, Ca, Sr, Ba중 선택된 하나 이상의 성분, R 2 는 Zr, Ti중 선택된 하나 이상의 성분): 0.5~10중량부, MnO 2 : 0.1~3중량부를 포함하여 이루어진다. 또한, 본 발명은 상기 내환원성 유전체 조성물의 제조방법을 제공한다. 본 발명은 1250℃ 이하의 낮은 소성온도에서 소성하더라도 글래스 뭉침 현상이 발생되지 않아 이를 적층 세라믹 콘덴서에 적용할 경우 박층 고용량화 및 신뢰성을 확보할 수 있는 효과가 있다.
Abstract:
본 발명은 적층 세라믹 콘덴서에 관한 것으로서, X5R 특성을 만족하고 저온소성이 가능하고 유전율의 변화가 작은 유전체 조성물 및 이를 이용한 적층 세라믹 콘덴서 및 그 제조방법을 제공하고자 하는데, 그 목적이 있는 것이다. 본 발명은 BaTiO 3 , MgCO 3 , Y 2 O 3 , Cr 2 O 3 , Mn 2 V 2 O 7 , 및 소결조제인 xBaO-yZrO 2 -zSiO 2 (0.1≤x≤0.3, 0.1≤y≤0.3, 0.4≤z≤0.8, x + y + z = 1)를 함유하고; 그리고 상기 성분들의 조성비는 그 성분들을, aBaTiO 3 -bMgCO 3 -cY 2 O 3 -dCr 2 O 3 -e(Mn 2 V 2 O 7 )-f(xBaO-yZrO 2 -zSiO 2 )의 조성식으로 표현할 때, 몰비로, a=100, 0.1≤b≤3.0, 0.3≤c≤2.0, 0.05≤d≤0.2, 0.01≤e≤1.5, 0.5≤f≤3.0의 조건을 만족하도록 이루어진 적층 세라믹 콘덴서용 유전체 조성물 및 이를 이용한 적층 세라믹 콘덴서 및 그 제조방법을 그 요지로 한다. 본 발명에 의하면, 4㎛이하의 초박층 고용량 적층 세라믹 콘덴서를 제조함에 있어서 내부 전극의 뭉침으로 인한 용량 저하 문제와 전극간 단락 불량을 현저히 줄일 수 있다.
Abstract:
첨가제가 고도로 분산되도록 세라믹 분말에 첨가제를 분산, 코팅하는 방법에 관한 것이다. Mg, Y, Dy, Mn, Ba 및 Ca의 질산염, 초산염, 산화물 및 탄산염으로 구성되는 그룹으로부터 선택된 최소 하나의 금속염 수용액 또는 금속염의 졸에 에테닐벤젠을 첨가하고 그 후, (Ba(1-x)Cax)TiO3, 0≤x≤0.05) 세라믹 분말을 첨가, 예비혼합하는 단계; 예비혼합물을 비즈 밀에서 해쇄 및 혼합하는 단계; 분무건조하는 단계; 및 400~700℃로 열처리하는 단계를 포함하는 세라믹 분말에 첨가제를 균일하게 분산, 코팅하는 방법이 제공된다. 액상법으로 유전체 분말에 첨가제를 고분산시킴으로써 첨가제가 편석되지 않고, 미립분말의 소결제어 및 분산성이 향상된다. 첨가제가 고분산된 유전체 분말은 1005 size 1㎌이상의 고용량 적층세라믹 콘덴서 제조에 적합하고 개선된 신뢰성을 나타낸다.
Abstract:
입자 크기 분포가 고르고, 분산성이 우수하며, 적층세라믹 콘덴서의 내부전극 재료에 사용가능한 구형 니켈 분말 제조방법이 제공된다. 니켈 분말은 니켈 전구체 화합물에 니켈 1몰당 히드라진을 2 -20몰로 첨가하여 니켈 히드라진 착화물을 생성하는 단계; 및 상기 니켈 히드라진 착화물에 농도가 40중량% 이상인 알칼리 금속의 수산화물을 첨가하는 단계를 포함하는 방법으로 제조된다. 알칼리 금속 수산화물의 수화발열로 반응이 가열됨으로 반응물이 고른 온도분포로 가열되어, 입자크기 분포가 균일하며 분산성이 좋은 구형의 미세한 니켈 금속 분말로 제조되며, 이는 적층세라믹 콘덴서의 내부전극 재료로 사용하기 적합한 것이다.
Abstract:
Disclosed is a dielectric composition, which is advantageous in light of increased homogeneity and insulation resistance, a method of preparing the same and a multi-layer ceramic capacitor using the same. The dielectric composition consists of a dielectric component represented by (Ba1-x-yCaxAy)m(Ti1-a-b-cZraB'bB''c)O3+m, (wherein, 0.01
Abstract:
The method is carried out in the following manner: An aqueous mixture solution containing barium chloride and titanium chloride is added into an aqueous oxalic acid solution, so that barium titanyl oxalate would be precipitated. Then the precipitates are aged, washed and filtered. The filtered barium titanyl oxalate precipitates are crushed, and dried. Then a thermal decomposition is carried out to obtain a agglomerated barium titanate powder, and this is crushed again to obtain the final barium titanate powder. In order to obtain barium titanate based powder such as Ba(Ti1-zZrz)O3, (Ba1-xCax)(Ti1-zZrz)O3, and (Ba1-x-yCaxSry)(Ti1-zZrz)O3, the desired elements (Ca, Sr, Zr and so on) are added to barium titanyl oxalate when crushed before thermal decomposition step. After thermal decomposition and crushing, the barium titanate based powder can be obtained.
Abstract:
PURPOSE: Provided is a high frequency dielectric composition, aZrO2 - bZnO - cTa2O5 - dTiO2(0.0 =42, Q value>=30000 and temperature coefficient of resonance frequency(TCF) of -10 to +10ppm/deg.C, and good sinterability.
Abstract translation:目的:提供一种高频介电组合物,ZrO 2 -bZnO-cTa 2 O 5 -dTiO 2(0.0≤a≤45.0,1.0≤b≤20.0,1.0≤c≤20.050.0≤d≤1.0) = 60.0),具有高Qf值,高介电常数和低共振频率温度系数(TCF)。 构成:高频介电组合物包含ZrO 2 -bZnO-cTa 2 O 5 -dTiO 2(0.0≤a≤45.0,1.0≤b≤20.0,1.0≤c≤20.050.0≤d≤60.0 )作为主要体系,添加至少一种选自MgO,MnO 2,CaO,SiO 2,Sb 2 O 5,Sb 2 O 3,Al 2 O 3和WO 3中的至少一种化合物作为添加剂。 所得的应用于双工器的介电组合物的介电常数≥42,Q值≥30000,并且谐振频率温度系数(TCF)为-10〜+ 10ppm /℃,并具有良好的可烧结性。
Abstract:
PURPOSE: A preparation method of barium titanate powder with good dielectric characteristics and high yield is provided by preparing powder by an oxalate method and wet milling powder mixed with N-contained additive, and thermal treating. CONSTITUTION: The preparation method of BaTiO3 powder comprises the steps of: (i) spraying a mixed solution of BaCl2 and TiCl4 over oxalic acid(H2C2O4) to form barium titanyl oxalate(BaTiO(C2O4)-4H2O, BTO) particles; (ii) aging for 0.5-2hrs and washing; (iii) wet milling BTO particles with 0.5-20mol%(based on barium titanyl oxalate) of N-contained additives to prevent acidification of the mixture, viscosity increase after milling, and decrease of dielectric characteristics, where M2+(Mg, Ca, Sr) or M4+(Zr, Hf, Sn) is optionally added to form Perovskite barium titanium compounds; (iv) thermal treating at 700-1200deg.C for BaTiO3 powder. The N-contained additive is selected from ammonia, amine such as mono(di, tri)-methyl amine or di(tri)-ethyl amine, and ammonium compound such as ammonium hydroxide, ammonium carbonate, ammonium acetate, etc.
Abstract translation:目的:通过草酸盐法制备粉末,与含氮添加剂混合的湿磨粉末和热处理,提供介电特性好,产率高的钛酸钡粉末的制备方法。 组成:BaTiO3粉末的制备方法包括以下步骤:(i)将草酸(H 2 C 2 O 4)上的BaCl 2和TiCl 4的混合溶液喷雾以形成草酸氧钛钡(BaTiO(C 2 O 4)-4H 2 O,BTO)颗粒; (ii)老化0.5-2小时并洗涤; (iii)用0.5-20mol%(基于草酸钡氧钛)的含N添加剂的湿磨BTO颗粒以防止混合物酸化,研磨后粘度增加,介电特性降低,其中M2 +(Mg,Ca,Sr )或M4 +(Zr,Hf,Sn),以形成钙钛矿钡钛化合物; (iv)对于BaTiO 3粉末,在700-1200℃热处理。 含N的添加剂选自氨,单(二,三) - 甲胺或二(三) - 乙胺等胺类,氢氧化铵,碳酸铵,乙酸铵等铵化合物。