Abstract:
PURPOSE: A method for manufacturing BixTe3-ySey nanocompound thermoelectric materials and the nanocompound thermoelectric materials manufactured by the same are provided to control a temperature to show the maximum thermoelectric performance index by controlling the charge carrier density of a nanocompound. CONSTITUTION: Bi(III)-stabilizer complex solutions are made by injecting a Bi precursor, a reducing agent, and a stabilizer into solvents(A1). BixTe3-ySey is made by reacting a Te precursor with the Bi(III)-stabilizer complex solutions(A2). BixTe3-ySey nanoparticles are obtained by filtering and drying the BixTe3-ySey(A3). The BixTe3-ySey nanoparticles are thermally processed(A4). [Reference numerals] (A1) Making Bi(III)-stabilizer complex solutions; (A2) Forming BixTe3-ySey by reacting a Te precursor with the Bi(III)-stabilizer complex solutions; (A3) Obtaining BixTe3-ySey nanoparticles by filtering and drying the BixTe3-ySey; (A4) Thermally processing the BixTe3-ySey nanoparticles; (AA) Start; (BB) End;
Abstract:
일 실시예에 따른 분말 열처리 장치는, 분말이 장입되며 열처리가 진행되는 반응관, 상기 반응관을 둘러싸도록 상기 반응관의 외부에 배치되는 외부관, 상기 반응관 및 상기 외부관을 회전시키는 회전 장치를 포함한다. 상기 반응관은 길이 방향에 수직인 방향으로의 단면이 다각형 형상을 가지는 반응실을 포함하고, 상기 반응관 및 상기 외부관 사이의 공간에는 소정의 분위기 가스를 공급함으로써 상기 반응관을 외부 환경으로부터 격리시킨다.
Abstract:
Bi 및 Sb 전구체를 용매 중에 투입하여 Bi-Sb 용액을 형성하는 단계, Te 분말을 산과 용매의 혼합용액에 투입하여 Te 용액을 형성하는 단계, 상기 Bi-Sb 용액과 상기 Te 용액을 혼합하여 반응시켜 Bi x Sb 2 -xTe 3 반응물을 형성하는 단계, 상기 Bi x Sb 2 -xTe 3 반응물을 여과 및 건조하여 Bi x Sb 2 -xTe 3 나노입자를 얻는 단계, 및 상기 Bi x Sb 2 -xTe 3 나노입자를 열처리하는 단계를 포함하는 나노화합물 열전재료 제조방법이 제공된다.