公开(公告)号:DE19845289A1
公开(公告)日:2000-04-06
申请号:DE19845289
申请日:1998-10-01
Applicant: BASF AG
Inventor: FISCHER MICHAEL , KNOLL MANFRED , GINSS CHRISTOPHE , BERZ STEPHAN
IPC: C08F265/04 , C08F279/02 , C08K3/04 , C08K5/00 , C08L25/08 , C08L25/12 , C08L25/14 , C08L51/00 , C08L51/06 , C08L55/02 , C08L67/02 , C08L101/00 , C08L67/03 , C08L25/06 , C08L33/18
Abstract: The invention relates to a thermoplastic moulding material containing the following ingredients in relation to the sum of ingredients A C and optionally D-A, whereby said sum corresponds to 100 wt. %: a) 10-98 wt. % of at least one aromatic polyester as ingredient A; b) 1-50 wt. % of at least one particle-shaped grafted copolymer with a soft phase glass transition temperature of less than 0 DEG C and an average particle size of 50-1000 nm as ingredient B; c) 1-50 wt. % of at least one copolymer consisting of monomers c1) 50-90 wt. % of at least one vinyl aromatic monomer as ingredient C1 and c2) 10-25 wt. % acrylonitrile and/or methylnitrile as ingredient C2, as ingredient C; d) 0-25 wt. % other compatible polymers that can be homogenously mixed with ingredients A and/or C or dispersed therein as ingredient D; e) 0-10 wt. % usual additives such as carbon black, pigments, UV stabilizers, oxidation retarders, lubricating agents and mould-release agents as ingredient E. The invention also relates to moulded parts made of said moulding materials, used in the interiors of motor vehicles, in addition to the use of said moulding materials in the production of moulded parts.
-
公开(公告)号:CA2611626C
公开(公告)日:2012-11-27
申请号:CA2611626
申请日:2006-06-13
Applicant: BASF AG
Inventor: EIPPER ANDREAS , BRUCHMANN BERND , WEISS CARSTEN , VOELKEL MARK , ROSENAU BERNHARD , GINSS CHRISTOPHE , HOEFLI KURT
Abstract: The invention relates to a method for producing multiple component moulded bodies. Said method is characterised in that at least one layer of the moulded body is formed from a thermoplastic moulding compound consisting of A) between 10 and 99.99 wt. % of at least one thermoplastic polyester, B) between 0.01 and 50 wt. % of B1) at least one highly branched or hyperbranched polycarbonate having an OH index of between 1 and 600 mg KOH/g of polycarbonate (according to DIN 5324O1 part 2), or B2) at least one highly branched or hyperbranched polyester of type A*By where x is at least 1.1 and y is at least 2.1 or the mixtures thereof, and C) between 0 and 60 wt. % of other additives. The sum of the weight percentage of the constituents A) to C) is equal to 100 %.
-
公开(公告)号:BRPI0705307A2
公开(公告)日:2009-01-20
申请号:BRPI0705307
申请日:2007-05-24
Applicant: BASF AG P GROUP S R L
Inventor: VOELKEL MARK , WEISS CARSTEN , GINSS CHRISTOPHE , PIZZATI GIANLUCA , BORTOLON VITTORIO , EIPPER ANDREAS
-
公开(公告)号:CA2611626A1
公开(公告)日:2006-12-21
申请号:CA2611626
申请日:2006-06-13
Applicant: BASF AG
Inventor: HOEFLI KURT , BRUCHMANN BERND , GINSS CHRISTOPHE , EIPPER ANDREAS , WEISS CARSTEN , ROSENAU BERNHARD , VOELKEL MARK
Abstract: The invention relates to a method for producing multiple component moulded bodies. Said method is characterised in that at least one layer of the mould ed body is formed from a thermoplastic moulding compound consisting of A) betwe en 10 and 99.99 wt. % of at least one thermoplastic polyester, B) between 0.01 and 50 wt. % of B1) at least one highly branched or hyperbranched polycarbonate having an OH index of between 1 and 600 mg KOH/g of polycarbonate (according to DIN 5324O1 part 2), or B2) at least one highly branched or hyperbranched polyester of type A*By where x is at least 1.1 and y is at least 2.1 or the mixtures thereof, and C) between 0 and 60 wt. % of other additives. The sum of the weight percentage of the constituents A) to C) is equal to 100 %.
-
35.
公开(公告)号:MY123030A
公开(公告)日:2006-05-31
申请号:MYPI9904178
申请日:1999-09-27
Applicant: BASF AG
Inventor: FISCHER MICHAEL DR , WEBER MARTIN DR , GINSS CHRISTOPHE , BERZ STEPHAN , XDF NORBERT KRE
IPC: C08J5/04 , C08F265/04 , C08F279/02 , C08K3/40 , C08K5/00 , C08K7/14 , C08L25/08 , C08L25/12 , C08L25/14 , C08L51/00 , C08L51/06 , C08L55/02 , C08L67/02 , C08L67/03 , C08L101/10
Abstract: A GLASS-FIBER-REINFORCED THERMOPLASTIC MOLDING COMPOSITION COMPRISES, BASED ON THE TOTAL OF COMPONENTS A TO D AND, IF DESIRED, E AND F, WHICH IN TOTAL GIVE 100% BY WEIGHT, A) AS COMPONENT A, FROM 10 TO 97% BY WEIGHT OF AT LEAST ONE AROMATIC POLYESTER, B) AS COMPONENT B, FROM 1 TO 50% BY WEIGHT OF AT LEAST ONE PARTICULATE GRAFT COPOLYMER WHOSE SOFT PHASE HAS A GLASS TRANSITION TEMPERATURE BELOW 0ºC AND WHOSE MEDIAN PARTICLE SIZE IS FROM 50 TO 1000 NM, C) AS COMPONENT C, FROM 1 TO 50% BY WEIGHT OF AT LEAST ONE COPOLYMER MADE FROM THE FOLLOWING MONOMERS C1) AS COMPONENT C1, FROM 50 TO 90% BY WEIGHT OF AT LEAST ONE VINYLAROMATIC MONOMER, AND C2) AS COMPONENT C2, FROM 10 TO 25% BY WEIGHT OF ACRYLONITRILE AND/OR METHACRYLONITRILE, D) AS COMPONENT D, FROM 1 TO 50% BY WEIGHT OF GLASS FIBERS, E) AS COMPONENT E, FROM 0 TO 25% BY WEIGHT OF OTHER COMPATIBLE POLYMERS HOMOGENEOUSLY MISCIBLE WITH COMPONENTS A AND/OR C OR DISPERSIBLE IN THESE, AND F) AS COMPONENT F, FROM 0 TO 10% BY WEIGHT OF CONVENTIONAL ADDITIVES, SUCH AS UV STABILIZERS, OXIDATION RETARDERS, LUBRICANTS AND MOLD-RELEASE AGENTS. MOLDINGS MADE FROM THESE MOLDING COMPOSITIONS AND USED IN MOTOR VEHICLE INTERIORS ARE ALSO DESCRIBED, AS IS THE USE OF THE MOLDING COMPOSITIONS TO PRODUCE THE MOLDINGS.
-
公开(公告)号:DE50104216D1
公开(公告)日:2004-11-25
申请号:DE50104216
申请日:2001-04-17
Applicant: BASF AG
Inventor: ROESCH JOACHIM , HUEFFER STEPHAN , IGL GEORG , BARTL JUERGEN , TAEGER LUEDECKE , KLENZ RAINER , GINSS CHRISTOPHE , GUENTHER ERHARD , LIESE MICHAELA
IPC: B32B37/10 , B29C45/14 , B29C45/16 , B29C70/68 , B32B5/18 , B32B7/04 , B32B9/02 , B32B37/15 , D06N7/04 , B32B31/10 , B32B31/30
Abstract: The invention relates to a process for the production of a multilayered composite element which comprises a layer of leather, a layer of a hard component formed from a polymer, which is bonded to the leather layer in certain areas, and a layer of a soft component, which is arranged between the leather component and the hard component, which comprises laying the leather against one mold surface of a mold, positioning the soft component on the leather, and molding the polymer acting as hard component onto the leather layer and the soft component layer at a pressure of at least 50 bar, preferably greater than 100 bar, in particular greater than 180 bar, and at a temperature of greater than 100° C., preferably from 180 to 280° C., in particular from 200 to 250° C., by bonding the leather and the hard component to one another in certain areas at least, with temperature of the mold surface of the mold being controlled, at least during the bonding. The invention furthermore relates to a composite element obtainable by the process. The composite element is extremely robust, has a soft touch surface and is inexpensive to produce.
-
公开(公告)号:DE59910301D1
公开(公告)日:2004-09-23
申请号:DE59910301
申请日:1999-09-29
Applicant: BASF AG
Inventor: FISCHER MICHAEL , WEBER MARTIN , GINSS CHRISTOPHE , BERZ STEPHAN , KRESS NORBERT
IPC: C08J5/04 , C08F265/04 , C08F279/02 , C08K3/40 , C08K5/00 , C08K7/14 , C08L25/08 , C08L25/12 , C08L25/14 , C08L51/00 , C08L51/06 , C08L55/02 , C08L67/02 , C08L67/03 , C08L101/10
Abstract: The invention relates to a fiber-reinforced thermoplastic moulding material containing the following ingredients in relation to the sum of ingredients A-D and optionally E and F, representing a total of 100 wt. %: d) 10-97 wt. % of at least one aromatic polyester as ingredient A; e) 1-50 wt. % of at least one particle-shaped grafted copolymer with a soft phase glass transition temperature that is lower than 0 DEG C and an average particle size of 50-1000 nm as ingredient B; f) 1-50 wt. % of at least one copolymer made of monomers c1) 50-90 wt. % of at least one vinyl aromatic monomer as ingredient C1 and c2) 10-25 wt. % acrylonitrile and/or methacrylonitrile as ingredient C2, as ingredient C; 1-50 wt. % glass fibers as ingredient D; f) 0-25 wt. % other ingredients that are compatible, can be mixed in a homogenous manner with ingredients A and/or C and can be dispersed therein, as ingredient E; f) 0-10 wt. % usual additives such as UV stabilizers, oxidation retarders, lubricating agents and release agents as ingredient F. The invention also relates to moulded parts made from said moulding materials and used in the interiors of motor vehicles. The invention further relates to the use of moulding materials in the production of moulded parts.
-
-
公开(公告)号:BR9914201A
公开(公告)日:2001-07-03
申请号:BR9914201
申请日:1999-10-01
Applicant: BASF AG
Inventor: FISCHER MICHAEL , KNOLL MANFRED , GINSS CHRISTOPHE , BERZ STEPHAN
IPC: C08F265/04 , C08F279/02 , C08K3/04 , C08K5/00 , C08L25/08 , C08L25/12 , C08L25/14 , C08L51/00 , C08L51/06 , C08L55/02 , C08L67/02 , C08L101/00
Abstract: A thermoplastic molding composition comprises, based on the total of components A to C and, if desired, D and E, which in total give 100% by weight,a) as component A, from 10 to 98% by weight of at least one aromatic polyester,b) as component B, from 1 to 50% by weight of at least one particulate graft copolymer whose soft phase has a glass transition temperature below 0° C. and whose median particle size is from 50 to 1000 nm,c) as component C, from 1 to 50% by weight of at least one copolymer made from the following monomersc1) as component C1, from 50 to 90% by weight of at least one vinylaromatic monomer, andc2) as component C2, from 10 to 25% by weight of acrylonitrile and/or methacrylonitrile,d) as component D, from 0 to 25% by weight of other compatible polymers hormogeneously miscible with components A and/or C or dispersible in these, ande) as component E, from 0 to 10% by weight of conventional additives, such as UV stabilizers, carbon black, pigments, oxidation retarders, lubricants and mold-release agents.Moldings made from these molding compositions and used in motor vehicle interiors are also described, as is the use of the molding compositions to produce the moldings.
-
公开(公告)号:DE19845317A1
公开(公告)日:2000-04-06
申请号:DE19845317
申请日:1998-10-01
Applicant: BASF AG
Inventor: FISCHER MICHAEL , WEBER MARTIN , GINSS CHRISTOPHE , BERZ STEPHAN , KRES NORBERT
IPC: C08J5/04 , C08F265/04 , C08F279/02 , C08K3/40 , C08K5/00 , C08K7/14 , C08L25/08 , C08L25/12 , C08L25/14 , C08L51/00 , C08L51/06 , C08L55/02 , C08L67/02 , C08L67/03 , C08L101/10 , C08L25/06 , C08L33/20
Abstract: The invention relates to a fiber-reinforced thermoplastic moulding material containing the following ingredients in relation to the sum of ingredients A-D and optionally E and F, representing a total of 100 wt. %: d) 10-97 wt. % of at least one aromatic polyester as ingredient A; e) 1-50 wt. % of at least one particle-shaped grafted copolymer with a soft phase glass transition temperature that is lower than 0 DEG C and an average particle size of 50-1000 nm as ingredient B; f) 1-50 wt. % of at least one copolymer made of monomers c1) 50-90 wt. % of at least one vinyl aromatic monomer as ingredient C1 and c2) 10-25 wt. % acrylonitrile and/or methacrylonitrile as ingredient C2, as ingredient C; 1-50 wt. % glass fibers as ingredient D; f) 0-25 wt. % other ingredients that are compatible, can be mixed in a homogenous manner with ingredients A and/or C and can be dispersed therein, as ingredient E; f) 0-10 wt. % usual additives such as UV stabilizers, oxidation retarders, lubricating agents and release agents as ingredient F. The invention also relates to moulded parts made from said moulding materials and used in the interiors of motor vehicles. The invention further relates to the use of moulding materials in the production of moulded parts.
-
-
-
-
-
-
-
-
-