Abstract:
The present invention relates to a method for producing thermosetting resin moldings, to the thermosetting resin moldings as such, to the use of the thermosetting resin moldings as structural components and to the use of a thermoplastic polymer having a porosity in the range of from 10 to 90% to increase the toughness of a thermosetting resin.
Abstract:
The invention relates to a method for producing a polyester polyol comprising the following method steps: (a) producing a reaction mixture comprising the following components: A: at least one carboxylic acid obtained from natural raw materials, having at least two acid groups, B: at least one multivalent alcohol, C: at least one organic phosphite compound, D: at least one Lewis acid; (b) heating the reaction mixture to a temperature of at least 160°C and separating the water that is generated during the reaction; (c) heating the reaction mixture to a temperature of at least 210°C at a pressure below 1013 mbar for a period of 0.1 to 25 hours.
Abstract:
Thermoplastic molding compositions, comprising A) from 10 to 99.999% by weight of a polyimide B) from 0.001 to 20% by weight of iron powder with a particle size of at most 10 mum (d50 value), which is obtainable via thermal decomposition of pentacarbonyliron, C) from 0 to 70% by weight of further additives, where the total of the percentages by weight of components A) to C) is 100%.
Abstract:
The invention relates to the production of porous structures, selected from porous fibers, sheets, films, coatings or molded objects of synthetic polymers by dissolving the polymer in an ionic liquid and precipitating or coagulating the dissolved synthetic polymer by contacting the solution with a liquid precipitation medium.
Abstract:
The present invention relates to a method for producing an aliphatic or partially aromatic polyamide, in which a polyamide prepolymer undergoes a solid-phase polymerization process.
Abstract:
The invention relates to a method for producing an aliphatic or semi-aromatic polyamide oligomer. According to the invention, an aqueous composition of the monomers is oligomerized at elevated temperature and elevated pressure and the product obtained by oligomerization is preferably expanded.
Abstract:
The present invention relates to semi-aromatic copolyamides having a high glass transition temperature and a high degree of crystallinity, to a polyamide molding compound containing said semi-aromatic copolyamide and to the use of the semi-aromatic copolyamides and of the polyamide molding compounds.