    Abstract: Novel materials having the ability to reversibly store hydrogen are amorphous metal alloys of the formula A8MbM min c wherein A is at least one metal selected from the group consisting of Ag, Au, Hg, Pd and Pt; M is at least one element selected from the group consisting of: Ru, Pb, Cu, Cr, Mo, Si, W, Ni, Al, Sn, Co, Fe, Zn, Cd, Ga and Mn; and M min is at least one element selected from the group consisting of Ca, Mg, Ti, Y, Zr, Hf, Nb, V, Ta and the rare earths; and wherein a ranges from about 0.005 to about 0.80; b ranges from about 0.05 to about 0.70; and c ranges from about 0.08 to about 0.95.

    35.
    发明专利
    未知

    公开(公告)号:NO166541C

    公开(公告)日:1991-08-07

    申请号:NO861193

    申请日:1986-03-25

    Abstract: Novel materials having the ability to reversibly store hydrogen are amorphous metal alloys of the formula A8MbM min c wherein A is at least one metal selected from the group consisting of Ag, Au, Hg, Pd and Pt; M is at least one element selected from the group consisting of: Ru, Pb, Cu, Cr, Mo, Si, W, Ni, Al, Sn, Co, Fe, Zn, Cd, Ga and Mn; and M min is at least one element selected from the group consisting of Ca, Mg, Ti, Y, Zr, Hf, Nb, V, Ta and the rare earths; and wherein a ranges from about 0.005 to about 0.80; b ranges from about 0.05 to about 0.70; and c ranges from about 0.08 to about 0.95.

    37.
    发明专利
    未知

    公开(公告)号:DE3671476D1

    公开(公告)日:1990-06-28

    申请号:DE3671476

    申请日:1986-07-14

    Abstract: Amorphous chromium-metalloid alloys exhibiting corrosion resistance in acid environments are described. The alloys contain a relatively low amount of a metalloid selected from the group of B, C, P, N, S, Sb and As. Additional metalloid elements such as Al, Si and Ge may also be present to enhance other properties of the amorphous alloy.

    AMORPHOUS METAL ALLOY POWDERS AND BULK OBJECTS AND SYNTHESIS OF SAME BY SOLID STATE DECOMPOSITION REACTIONS

    公开(公告)号:CA1233047A

    公开(公告)日:1988-02-23

    申请号:CA475705

    申请日:1985-03-04

    Abstract: Amorphous metal alloy powders are synthesized by solid state decomposition reactions. At least one precursor compound is thermally decomposed at a temperature below the crystallization temperature of the amorphous metal alloy to be formed. The decomposition product comprises an intimate mixture of the elements of the alloy and, after heat-treating if necessary, exhibits amorphous characteristics. Amorphous metal alloy shapes are synthesized by providing an intimate mixture of the components of the amorphous alloy, which mixture includes at least one ductile component. The mixture may be subjected to well-known forming techniques at a temperature below the crystallization temperature of the amorphous metal alloy to be formed. The ductile component of the mixture acts as a binder matrix to provide strength and uniform properties to the formed object.