公开(公告)号:KR850000280B1
公开(公告)日:1985-03-16
申请号:KR810003107
申请日:1981-08-25
Applicant: STANDARD OIL CO OHIO
Inventor: DOLHYJ SERGE ROMAN , PEPERA MARC ANTHONY
IPC: B01J27/18
-
公开(公告)号:KR840000089B1
公开(公告)日:1984-02-10
申请号:KR800001653
申请日:1980-04-23
Applicant: STANDARD OIL CO OHIO
Inventor: GREENE JANICE LENORE
IPC: C08G69/00
-
公开(公告)号:KR820000961B1
公开(公告)日:1982-05-31
申请号:KR780002328
申请日:1978-07-28
Applicant: STANDARD OIL CO OHIO
Inventor: STRADA F , SURESH D , ORANDOFF D , GRASSELLI R
IPC: B01J23/88 , C07C121/32
Abstract: Acrylonitrile and methacrylonitrile is prepd. by ammoxidation of propylene and isobutyrene resp., using improved catalyst which can be represents as JaQ6ZcFedDeMo12Ox, where J is an alkali metal, Tl and Ag, Q is Co, Ni, Zn, Cd, Be, Mg, Ca, Sr, Ba and Ra, Z represents Ge+Sb, Cu+W, Cu+Sn, Ce+W, Pr+Mn, Sn+Mn, Mn+W, W+Sb, Cr+Sn, W+Sn, Ge+Sn, Sb+Sn, W+P, Sb+P, Cr+Cu, Mn+Cu, Sb+Cu and Mn+P, D is Bi or Te, a = 0.03-0.05, b = 4-10, C = 0.5-7, d = 0.5-5, e - 0.5-5, and x is as necessary for balance. For example, MnWo.5 (Ko.1Ni2.5Co4.5 Fe2BiMo12Ox) supported on 20% SiO2 gave acrylonitrile with 86.4% selectivity and 68.5% conversion per pass at 420≦̸C.
-
公开(公告)号:KR810000452B1
公开(公告)日:1981-05-02
申请号:KR780002433
申请日:1978-08-09
Applicant: STANDARD OIL CO OHIO
Inventor: GRASSELLI R , BRAZDIL J , SURESH D
IPC: B01J23/00
Abstract: Catalyst-prepg. technique is applicable to a wide different types of catalysts, the compns. of which are generally well-known. Such catalysts can be described by following formula(I; M = Bi, Te, Sb, Sn, Cu; N = Mo, W; A - alkali, Ti, Sm; C = Ni, Co, Mn, Mg; D = Fe, Cr, Ce, V; E = P, As, B, Sb; F = rare earth metal, Ti, Zr, Re; a = 0-4; b = 0-20; c = 0.01-20; d = 0-4; e = 0-8; f = 8-16; m = 0.01-10; n = 0.1-30).
-
公开(公告)号:KR810000395B1
公开(公告)日:1981-04-27
申请号:KR770000255
申请日:1977-02-08
Applicant: STANDARD OIL CO OHIO
IPC: C08L33/20
Abstract: An impact-resistant copolymer(I) having low gas permeability and high softening temp. is manufd. by grafting a nitrile rubber latex was grafted with acrylonitrile 70, indene 10, and isobutene 20g to give I having 264 psi heat distortion temp. 79≦̸C and notched Izod impact strength 7.3 ft-1b/in. notch which gave a film having 90% relative humidity water vapor transmission rate 3.5g-mil/100 in. 2/24hr/atm and O transmission rate 2.0 cm3-mil/100 in.2/24 hr/atm.
-
公开(公告)号:KR800001071B1
公开(公告)日:1980-10-04
申请号:KR750002604
申请日:1975-11-28
Applicant: STANDARD OIL CO OHIO
IPC: C08L9/02
Abstract: Polymeric compositions having good impact resistance, low permebility to gases, and high-softening temp. which are composed of a conjugated diene monomer, such as butadiene, an olefinically unsaturated nitrile, such as acrylonitrile, an ester of an olefinically unsaturated acid, such as methyl acrylate, and indene are described.
-
公开(公告)号:KR790001107B1
公开(公告)日:1979-09-03
申请号:KR750000987
申请日:1975-05-07
Applicant: STANDARD OIL CO OHIO
Inventor: HSIN CHIB WU
Abstract: After the amnoxidn. of propylene, the reaction effluent was directly contacted with aq. stream in a quench column. The acrylonitrile and HCN were recovered in the form of aq. soln, and some of the water and impurities were removed by distn. to form a concentrated aq. mixture of acrylonitrile and HCN, which was distilled in an HCN distn. column to remove the HCN in an overhead stream. A side stream in the HCN distn. column was fed to a decanter where an aq. layer and an org. layer were formed.
-
公开(公告)号:KR840000985B1
公开(公告)日:1984-07-13
申请号:KR810002827
申请日:1981-08-04
Applicant: STANDARD OIL CO OHIO
Inventor: SHAW WILFRID GARSIDE , RING JAMES EDWARD , PAPARIZOS CHRISTOS
IPC: C07C57/055 , B01J23/76 , B01J27/198 , B01J27/199 , C01B25/45 , C07B61/00 , C07C51/00 , C07C51/235 , C07C51/25 , C07C67/00
-
公开(公告)号:KR810001985B1
公开(公告)日:1981-12-08
申请号:KR770000283
申请日:1977-02-10
Applicant: STANDARD OIL CO OHIO
IPC: C09D3/74
Abstract: Nitryl polymer for coating metal is prepd. by graft copolymg. acrylonitrile(I) and Me acrylate(II) or styrene with latexes of nitrile rubber of SBR, resp. Thus, a 31.1% solid rubber latex was prepd. by polymn. of 40 parts I with 60 parts 1,3-butadiene in water in the presence of AIBN tert- dodecyl mercaptan and emulsifier, and 31.9 parts of the rubber latex was polymd. with 75 parts I and 25 parts II in water in the presence of K2S2O8, in emulsifier, n-dodecyl mercaptan, and EDTA to give 33% solids copolymer latex.
-
公开(公告)号:KR810000516B1
公开(公告)日:1981-05-25
申请号:KR770002412
申请日:1977-10-08
Applicant: STANDARD OIL CO OHIO
IPC: C07C51/145 , C07C57/04
Abstract: Olefinic aldehydes were oxidized to olefinic acids such as methacrolein, acrolein to methacrylic acid acrylic acid, at 200-500≦̸C over mixed oxide catalysts contg. Mo, P, As and Cu. Thus, a 1:5.7:4.6:8.6 (molar) mixt. of methacrolein, air, N, and steam was passed at a 2-sec-residence time through a tube heated at 354≦̸C and contg. the mixed oxide catalyst on an Alundum support to give methacrylic acid in 93.8% yield.
-
-
-
-
-
-
-
-
-