Abstract:
Resin compositions, e.g., epoxy resin compositions, comprising flame retardant materials obtained by heating phosphonic acid salts at temperatures above 200° C., have excellent properties and exhibit manageable curing behavior. Laminates, composites, molded articles and the like, which have excellent flame retardant properties and physical characteristics, are readily prepared from the resin compositions of the invention.
Abstract:
A modified poly(arylene ether) resin composition includes a mixed resin that includes a poly(arylene ether) resin, a styrene-based resin and a polyolefin resin; a flame retardant; and mineral oil. A weight-average molecular weight of the mineral oil is 460 to 1,000 g/mol. A wire is manufactured using the modified poly(arylene ether) resin composition.
Abstract:
Significant disadvantages of the use of polylactic acid (PLA), lack of good heat stability and flame retardance, have been overcome by the use of an aryl phosphate in combination with talc. The compound achieves a threshold of 65° C. in heat deflection temperature and V-0 flame retardance at 1.6 mm thickness.
Abstract:
A black-colored plastic composition includes specific amounts of a brominated polycarbonate, a poly(butylene terephthalate), a block polyestercarbonate containing resorcinol ester units, diantimony trioxide, and a black colorant. The composition exhibits a deeper black color than a corresponding composition without the block polyestercarbonate. The composition can be used to mold black parts of consumer electronic devices, such as flat screen television bezels, cell phone backs, and exterior parts of household appliances such as toasters and microwave ovens.
Abstract:
Disclosed is a halogen-free resin composition. The halogen-free resin composition comprises: (A) 10-60 parts by weight of dicyclopentadiene benzoxazine resin, (B) an epoxy resin, (C) an active ester curing agent, and (D) a phosphorus-containing flame retardant, based on 100 parts by weight of the total amount of total organic solid matters of (A), (B), (C), and (D). A prepreg and a laminate which are prepared using the halogen-free resin composition have low dielectric constant, low dielectric loss factor, low water absorption, high dimensional stability, high thermal resistance and good flame retardancy, processability and chemical resistance.
Abstract:
Resin compositions, e.g., epoxy resin compositions, comprising flame retardant materials obtained by heating phosphonic acid salts at temperatures above 200° C., have excellent properties and exhibit manageable curing behavior. Laminates, composites, molded articles and the like, which have excellent flame retardant properties and physical characteristics, are readily prepared from the resin compositions of the invention.
Abstract:
Disclosed herein is a method of reducing the amount of antimony flame retardant compound in a flame retardant composition which comprises using calcium oxide or a combination of talc and calcium oxide as a filler in the composition, wherein the composition comprises specific amounts of a polyester, a brominated flame retardant compound, an antimony flame retardant compound, and a filler comprising calcium oxide or a combination of talc and calcium oxide. Also disclosed are compositions prepared by such a method and articles derived therefrom.
Abstract:
The present invention provides a resin composition comprising: (A) 100 parts by weight of epoxy resin; (B) from 10 to 80 parts by weight of benzoxazine resin; (C) from 10 to 50 parts by weight of dicyclopentadiene phenol resin; and (D) from 0.5 to 5 parts by weight of amine hardener; wherein the resin composition is free of diallyl bisphenol A (DABPA).
Abstract:
A resin composition has high flame retardancy and excellent heat resistance, peel strength with copper foil, thermal expansion coefficient, heat resistance property upon moisture absorption, and electrical properties, a prepreg and single-layer or laminated sheet, a metal foil-clad laminate using the prepreg, and the like. The resin composition has polyphenylene ether (A) having a number average molecular weight of 500 to 5000, a phosphorus-containing cyanate ester compound (B) represented by formula (13), a cyclophosphazene compound (C), a halogen-free epoxy resin (D), a cyanate ester compound (E) other than the phosphorus-containing cyanate ester compound (B), an oligomer (F) of styrene and/or substituted styrene, and a filler (G), wherein a content of the phosphorus-containing cyanate ester compound (B) is 1 to 10 parts by mass based on 100 parts by mass of a total of the (A) to (F) components. wherein m represents an integer of 1 to 3.
Abstract:
A halogen-free fire-retardant thermoplastic composition composed of: 50% to 70% by weight of fire-retardant fillers, 0.1% to 45% by weight of a copolymer of ethylene and of an ethylenic monomer bearing a polar function, 10% to 25% by weight of a non-functionalized very low density polyethylene (VLDPE), optionally, up to 10% of additives, and 0.1% to 10% by weight of a linear low density polyethylene (LLDPE), characterized in that the density of the very low density polyethylene (VLDPE) is between 0.85 and 0.91, in that the density of the linear low density polyethylene is greater than 0.91 and in that the linear low density polyethylene (LLDPE) is grafted with maleic anhydride grafts present on the main chain. Also, a cable, tube, pipe or the like, a layer of which is formed with said composition.