公开(公告)号:KR1020040037316A
公开(公告)日:2004-05-07
申请号:KR1020020065766
申请日:2002-10-28
Applicant: 한국전기연구원
IPC: C04B35/475 , H01L41/187 , H01P7/10
CPC classification number: H01L41/187 , C04B35/475 , H01L41/43 , H01P7/10
Abstract: PURPOSE: Provided is a Pb-free piezoelectric ceramic composition of the (Bi4-xLax)(Ti3-5y/4Vy)O12 + zmol% TiO2 for ceramic oscillators requiring good piezoelectric characteristics and sinterability by substituting V for Ti and adding excess Ti in the conventional (Bi,La)4Ti3O12 system. CONSTITUTION: The Pb-free piezoelectric ceramic composition is expressed by the formula of (Bi4-xLax)(Ti3-5y/4Vy)O12 + zmol% TiO2, wherein x, y and z are in the ranges of 0.7
Abstract translation: 目的:提供一种用于陶瓷振荡器的(Bi4-xLax)(Ti3-5y / 4Vy)O12 + zmol%TiO2的无铅压电陶瓷组合物,其需要良好的压电特性和烧结性,通过用V代替Ti并在其中添加过量的Ti 常规(Bi,La)4Ti3O12体系。 构成:无铅压电陶瓷组合物由(Bi4-xLax)(Ti3-5y / 4Vy)O12 + zmol%TiO2的式表示,其中x,y和z在0.7 <= x < 0.8摩尔,0.01 <= y <= 0.3摩尔,0 <= z <= 10摩尔%。 该组合物通过以下步骤制备:将原料如Bi 2 O 3,La 2 O 3,TiO 2和V 2 O 5混合; 在800℃煅烧2-4小时; 添加添加剂如TiO2和研磨; 压力100MPa压力; 在900-1200℃烧结2小时; 将压实件的端面抛光至1mm厚度; 形成Ag电极; 极化电极为9kV / mm和120deg.C 20-30min。 对于陶瓷振荡器,芯片型陶瓷振荡器,使用具有改善的机电系数(kp)和机械品质因数(Qm)以及宽带宽频率的无铅压电陶瓷组合物。
-
公开(公告)号:KR1020030025712A
公开(公告)日:2003-03-29
申请号:KR1020010058884
申请日:2001-09-22
Applicant: 한국전기연구원
IPC: H01L21/8242
Abstract: PURPOSE: A method of fabricating a thin film capacitor for integrated electromagnetic device is provided to prevent diffusion and volatilization of lead within a PZT thin film in a post thermal process. CONSTITUTION: An insulating planarization layer is formed on a semiconductor substrate. The first and the second buffer layers are formed on the insulating planarization layer. A capacitor of an integrated device is formed by using a pattern of a bottom electrode, a pattern of a PZT thin film dielectric(6), and a pattern of an upper electrode(5). The upper electrode(5) is formed with copper. The bottom electrode is formed with a conductive oxide layer such as Pt or RuO. An upper electrode deposition process is performed after a PZT film dielectric formation process and an annealing process are performed. The third and the fourth buffer layers(14,13) are formed between the PZT thin film dielectric(6) and the upper electrode(5). A passivation layer(4) is deposited on a surface of the upper electrode(5).
Abstract translation: 目的:提供一种制造用于集成电磁装置的薄膜电容器的方法,以防止在后热处理中PZT薄膜内的铅的扩散和挥发。 构成:在半导体衬底上形成绝缘平坦化层。 第一和第二缓冲层形成在绝缘平坦化层上。 通过使用底电极的图案,PZT薄膜电介质(6)的图案和上电极(5)的图案来形成集成器件的电容器。 上电极(5)由铜形成。 底部电极由Pt或RuO等导电氧化物层形成。 在进行PZT膜电介质形成工艺和退火处理之后进行上电极淀积工艺。 第三和第四缓冲层(14,3)形成在PZT薄膜电介质(6)和上电极(5)之间。 钝化层(4)沉积在上电极(5)的表面上。
-
公开(公告)号:KR1020170059803A
公开(公告)日:2017-05-31
申请号:KR1020150164235
申请日:2015-11-23
Applicant: 한국전기연구원
IPC: C01G33/00
Abstract: 본발명은, 판상의니오븀산칼륨입자및 그제조방법에있어서, KCO, NbO및염을혼합하여열처리하는단계를통해제조되는것을기술적요지로한다. 이에의해플럭스(flux) 공법을통해압전세라믹스의고상단결정성장법이나결정배향법에사용가능한판상의니오븀산칼륨입자를제조가능한효과가있다.
Abstract translation: 根据铌酸钾粒子的本发明,以及制造板形的方法,和通过热处理一KCO的混合物的工序制造的,NbO的一个mityeom技术基础。 由此,可以制造可用于压电陶瓷的固相单晶生长法或通过助熔剂法的晶体取向法的板状铌酸钾颗粒。
-
公开(公告)号:KR101541316B1
公开(公告)日:2015-08-03
申请号:KR1020130131268
申请日:2013-10-31
Applicant: 한국전기연구원
IPC: C04B35/468 , H01B3/12
Abstract: 본발명은졸-겔방법을이용한 Cu-BaTiO복합유전체조성물및 그제조방법에관한것으로, 용액석출공정에있어바륨전구체(Barium precursor)와티타늄전구체(Titanium precursor)를출발원료로사용하는제1단계와; 용액석출공정중 졸-겔법을이용하여 80℃내지 95℃의온도에서 6 시간내지 24 시간의시간동안반응조에서반응시키는제2단계와; 상기제2단계이후에금속구리입자를도입하여졸-겔법을이용하여분산반응시키켜혼합액을제조하는제3단계와; 상기제3단계후에상기혼합액을건조하여복합유전체를형성시키는제4단계;를포함하여구성되는졸-겔방법을이용한 Cu-BaTiO복합유전체조성물제조방법을기술적요지로한다. 이에따라, 졸-겔세라믹스공정을이용하여티탄산바륨나노세라믹스분말을만들고, 나노분말과금속을혼합하여복합유전체조성물을형성시킴에의해순수바륨타이터네이트(Barium Titanate) 보다유전율이높고, 금속의코어아일랜드가첨가됐음에도불구하고전압에의한손실이나타나지않아, 커패시터유전체로써활용이가능한이점이있다.
-
45.
公开(公告)号:KR1020150057650A
公开(公告)日:2015-05-28
申请号:KR1020130141274
申请日:2013-11-20
Applicant: 한국전기연구원
IPC: C04B35/468 , C04B35/624 , C04B35/74 , H01B3/10
CPC classification number: C04B35/4682 , C04B35/624 , C04B35/63416 , C04B35/64 , C04B2235/408 , C04B2235/658 , C04B2235/667 , C04B2235/96 , H01G4/1227 , H01G4/30
Abstract: 본발명은졸-겔방법을이용한 Ag-BaTiO복합유전체조성물및 그제조방법에관한것으로, 용액석출공정에있어바륨전구체(Barium precursor)와티타늄전구체(Titanium precursor)를출발원료로사용하는제1단계와; 용액석출공정중 졸-겔법을이용하여 80℃내지 95℃의온도에서 6 시간내지 24 시간동안반응조에서반응시키는제2단계와; 상기제2단계이후에금속은 입자를도입하여졸-겔법을이용하여분산반응시켜혼합액을제조하는제3단계와; 상기제3단계후에상기혼합액을건조하여복합유전체를형성시키는제4단계;를포함하여구성되는졸-겔방법을이용한 Ag-BaTiO복합유전체조성물제조방법을기술적요지로한다. 이에따라, 졸-겔세라믹스공정을이용하여티탄산바륨나노세라믹스분말을만들고, 나노분말과금속은 입자를혼합하여복합유전체조성물을형성시킴에의해순수바륨타이터네이트(Barium Titanate) 보다유전율이높고, 금속의코어아일랜드가첨가됐음에도불구하고전압에의한손실이나타나지않아, 커패시터유전체로써활용이가능한이점이있다.
Abstract translation: 本发明涉及一种Ag-BaTiO_3复合电介质组合物及其制造方法,该方法包括:在溶液沉淀法中使用钡前体和钛前体作为起始原料的第一步骤; 在溶液沉淀法中使用溶胶 - 凝胶法,使起动原料在反应槽中在80-95℃下反应6-24小时的第二步; 通过引入金属银颗粒并在第二步骤之后使用溶胶 - 凝胶法和分散反应制备混合溶液的第三步骤; 以及在第三步骤之后通过干燥所述混合溶液形成所述复合电介质的第四步骤。 Ag-BaTiO_3复合电介质组合物的电导率高于纯钛酸钡,由于通过溶胶 - 凝胶陶瓷工艺制备钛酸钡陶瓷粉末,然后通过将纳米粉末与金属银颗粒混合而形成复合电介质组合物。 此外,Ag-BaTiO 3复合电介质组合物可以用作电容器电介质,因为即使组成包括金属芯岛也不会发生电压的损失。
-
公开(公告)号:KR101383356B1
公开(公告)日:2014-04-14
申请号:KR1020120086324
申请日:2012-08-07
Applicant: 한국전기연구원
IPC: C04B35/468 , C04B35/64 , H01B3/12
Abstract: 본 발명은 고유전율을 갖는 복합 세라믹유전체 조성물 및 그 제조방법에 관한 것으로, 티탄산 바륨(Barium Titanate, BaTiO
3 )에 수 ㎛의 입자 크기를 가지는 니켈(Nickel, Ni), 구리(Cu), 은(Ag) 중 하나 이상의 금속 원소를 첨가하여 출발원료로 사용하는 제1단계와; 상기 금속원소는 조성비 x(0<x≤20)wt% 범위 내에서 각 조성에 따른 시료를 증류수 또는 에탄올을 분산매로 하여 지르코니아볼을 사용하여 24시간 동안 볼밀하여 혼합, 분쇄하는 제2단계와; 상기 볼밀한 시료를 건조시키는 제3단계와; 상기 건조된 시료에 PVA(Polyvinyl Alcohol: 5wt% 수용액)을 첨가하고 압력을 가하는 방법으로 성형하여 시편을 형성시키는 제4단계와; 상기 시편을 도가니에 질소 가스(N
2 atmosphere) 분위기 전기로에서 1300 ~ 1350℃ 온도 범위 내에서 소결하는 제5단계;를 포함하여 구성되는 고유전율을 갖는 복합 세라믹유전체 조성물 제조방법을 기술적 요지로 한다. 또한, 본원발명은 티탄산 바륨(Barium Titanate, BaTiO
3 )에 금속 원소를 첨가하여 형성시킨 티탄산 바륨(Barium Titanate, BaTiO
3 ) 조성물에 아일랜드(island) 금속 코어(core)를 형성시키는 고유전율을 갖는 복합 세라믹유전체 조성물을 또한 기술적 요지로 한다. 이에 따라, 본 발명에 따른 복합 세라믹유전체 조성물은 순수 티탄산 바륨(Barium Titanate, BaTiO
3 ) 보다 유전율이 높고, 손실계수는 작으며, 고전계로 충전 가능한 커패시터 유전체로써 활용이 가능하다. 특히 충전 커패시턴스(capacitance) 가 증가하면 충전 전압은 감소하는 것이 보통인데 본 발명에서는 비유전율은 증가하지만 충전전계도 일정하게 유지가 된다. 그러므로 높은 전압을 갖는 특성이 있어 정전용량을 키우면서 전압도 상승하는 전력 저장용 커패시터의 유전체로 활용할 수 있는 이점이 있다.-
公开(公告)号:KR1020140020011A
公开(公告)日:2014-02-18
申请号:KR1020120086324
申请日:2012-08-07
Applicant: 한국전기연구원
IPC: C04B35/468 , C04B35/64 , H01B3/12
CPC classification number: C04B35/468 , C04B35/64 , C04B35/74 , C04B2235/3236 , H01B3/12
Abstract: The present invention relates to a composite ceramic dielectric composition with a high dielectric constant and a manufacturing method thereof. The present invention provides a composite ceramic dielectric composition with a high dielectric constant, wherein the composition forms an island metal core in barium titanate composition formed by adding metal elements to barium titanate.
Abstract translation: 本发明涉及具有高介电常数的复合陶瓷电介质组合物及其制造方法。 本发明提供具有高介电常数的复合陶瓷电介质组合物,其中组合物通过向钛酸钡中添加金属元素而形成钛酸钡组合物中的岛状金属芯。
-
公开(公告)号:KR1020130143204A
公开(公告)日:2013-12-31
申请号:KR1020120066508
申请日:2012-06-21
Applicant: 한국전기연구원
IPC: F02P3/12
Abstract: The present invention relates to an ignition device for an engine using a piezoelectric element, and, more specifically, to an ignition device for an engine using a piezoelectric element, in which ignition is performed through a piezoelectric element generating a high voltage from a mechanical movement due to driving of an engine so as to reduce the power consumption, therefore, to improve the fuel efficiency of the vehicle, to simplify an electrical circuit related to an ignition plug, and to enable stable ignition due to the precise ignition time. The present invention has the gist of technology that an ignition device for an engine using a piezoelectric element comprises an ignition plug installed in the upper end within a cylinder of an engine; a piezoelectric element fixed to one external side of the engine at an interval corresponding to the cylinder, and electrically connected to the ignition plug; a pressurizing unit installed between one external side of the engine and a connecting rod of a piston so that the upper part is able to contact with the piezoelectric element, and generating a high voltage by pressurizing the piezoelectric element with a mechanical movement upon the vertical reciprocating motion of the piston in driving of the engine; and a voltage applying module electrically connected between the ignition plug and the piezoelectric element and applying the high voltage generated in the piezoelectric element by the pressurizing unit to the ignition plug so as to be able to be used as an ignition voltage.
Abstract translation: 本发明涉及一种使用压电元件的发动机点火装置,更具体地说,涉及一种使用压电元件的发动机点火装置,其中通过机械运动产生高电压的压电元件进行点火 由于发动机的驱动以降低功率消耗,因此提高车辆的燃料效率,简化与火花塞相关的电路,并且由于精确的点火时间而能够稳定点火。 本发明具有以下要点:使用压电元件的发动机点火装置包括:安装在发动机气缸内的上端的火花塞; 压电元件,其以对应于所述气缸的间隔固定到所述发动机的一个外侧,并且电连接到所述火花塞; 安装在发动机的一个外侧和活塞的连接杆之间的加压单元,使得上部能够与压电元件接触,并且通过在垂直往复运动时以机械运动对压电元件进行加压来产生高电压 活塞在发动机驱动中的运动; 电压施加模块电连接在火花塞和压电元件之间,并通过加压单元将压电元件产生的高电压施加到火花塞,以便能够用作点火电压。
-
公开(公告)号:KR1020130064611A
公开(公告)日:2013-06-18
申请号:KR1020110131310
申请日:2011-12-08
Applicant: 한국전기연구원
IPC: C04B35/468 , C04B35/01 , H01L41/187
CPC classification number: H01L41/1871
Abstract: PURPOSE: A lead-free piezoelectric ceramics for a sensor and an actuator is provided to improve dielectric ratio and piezoelectric constant by arranging paraelectric materials of small sizes around ferroelectric materials of large sizes and forming the trap structure. CONSTITUTION: A lead-free piezoelectric ceramics for a sensor and an actuator is composed of paraelectric materials and ferroelectric materials. The paraelectric materials and the ferroelectric materials are mixed at the volume ratio of 1 : 5-20. The sizes of the paraelectric materials are smaller than the sizes of the ferroelectric materials. The paraelectric materials are piezoelectric materials which are arranged around the ferroelectric materials. When electric field is generated in the piezoelectric materials, the paraelectric phase is changed into ferroelectric phase and the domain of the ferroelectric phase is changed. The ferroelectric material is composed of (Bi0.5Na0.5)TiO3 or (Bi0.5Na0.5)TiO3-(Bi0.5K0.5)TiO3-based materials. The paraelectric material is obtained by mixing an additive for lowering phase-change temperatures into the ferroelectric materials.
Abstract translation: 目的:提供一种用于传感器和致动器的无铅压电陶瓷,通过在大尺寸的铁电材料周围布置小尺寸的对电材料并形成陷阱结构来提高介电常数和压电常数。 构成:用于传感器和致动器的无铅压电陶瓷由顺电材料和铁电材料组成。 顺电材料和铁电材料以1:5-20的体积比混合。 顺电材料的尺寸小于铁电材料的尺寸。 顺电材料是布置在铁电材料周围的压电材料。 当在压电材料中产生电场时,顺电相变为铁电相,铁电相的畴变化。 铁电材料由(Bi0.5Na0.5)TiO3或(Bi0.5Na0.5)TiO3-(Bi0.5K0.5)TiO3基材料组成。 顺电材料通过将用于将相变温度降低的添加剂混合到铁电材料中而获得。
-
公开(公告)号:KR101198298B1
公开(公告)日:2012-11-07
申请号:KR1020100093777
申请日:2010-09-28
Applicant: 한국전기연구원
IPC: H01L41/187 , C04B35/495 , C04B35/48
CPC classification number: H01L41/1873 , C04B35/495 , C04B35/62685 , C04B35/62821 , C04B35/62823 , C04B2235/3201 , C04B2235/3203 , C04B2235/3208 , C04B2235/3213 , C04B2235/3236 , C04B2235/3248 , C04B2235/3255 , C04B2235/3267 , C04B2235/768
Abstract: 본 발명은 비납계 압전 세라믹 조성물과 그의 제조방법에 관한 것으로서, 센서나 액추에이터로 사용되는 비납계 압전 세라믹 조성물에 있어서, 원료용 비납계 압전 세라믹을 각각 제조한 후 혼합, 분쇄, 건조, 소결시켜, 상유전체상 및 강유전체상이 혼합되고 이러한 상들이 코어-셀 구조로 존재하는 압전 성형물을 제조함으로써, 상기 압전 성형물에 전계 인가시 셀 부위에서 상유전체상에서 강유전체상으로의 상변이와 코어 부위에서 강유전체상의 도메인 재배열이 발생되어 고변형율을 나타내는 것을 특징으로 하는 센서나 액추에이터로 사용되는 비납계 압전 세라믹 조성물을 기술적 요지로 한다. 이에 의해 최종 압전 성형물이 최소 두 가지 이상을 상을 가지면서, 전계 인가시 상변이와 도메인 재배열이 발생되어 고변형율에 의한 유전율의 증가와 압전상수(d
33 )가 우수하여, 충격 센서, 가속도센서, 초음파 센서, 적층형 압전액추에이터, 압전변압기 및 초음파 진동자, 착화소자와 같은 고신뢰성 압전부품을 제조할 수 있으며, 납에 의한 환경 오염을 감소시킬 수 있는 이점이 있다.
-
-
-
-
-
-
-
-
-