公开(公告)号:BRPI0513239A
公开(公告)日:2008-04-29
申请号:BRPI0513239
申请日:2005-07-08
Applicant: BASF AG
Inventor: HAHN KLAUS , EHRMANN GERD , RUCH JOACHIM , ALLMENDINGER MARKUS , SCHMIED BERNHARD , HOLOCH JAN
IPC: C08J9/00
Abstract: A process for producing expandable styrene polymers (EPS) having improved expandability, wherein from 0.1 to 1% by weight, based on the styrene polymer, of a free-radical former is metered into a styrene polymer melt containing blowing agent at a melt temperature in the range from 150 to 220° C. and the melt is extruded through a die plate with subsequent underwater pelletization.
-
公开(公告)号:MX2007012266A
公开(公告)日:2007-10-12
申请号:MX2007012266
申请日:2006-04-05
Applicant: BASF AG
Inventor: HAHN KLAUS , RUCH JOACHIM , ALLMENDINGER MARKUS
Abstract: La invencion se refiere a un metodo para producir particulas de espuma de poliestireno con una densidad de volumen que varia entre 40 y 400 g/l por la extrusion de una fusion de poliestireno conteniendo dioxido de carbono y/o agua como el agente de expansion, a traves de una boquilla y por granulacion bajo el agua. De acuerdo con la invencion, la granulacion bajo el agua se lleva a cabo a una presion que varia entre 1y 30 bar.
-
公开(公告)号:CA2621731A1
公开(公告)日:2007-03-01
申请号:CA2621731
申请日:2006-08-09
Applicant: BASF AG
Inventor: ALLMENDINGER MARKUS , SCHMIED BERNHARD , HAHN KLAUS , RIETHUES MICHAEL
IPC: C08J9/00
Abstract: Production of foamed bodies involves sintering polymer-coated, prefoamed particles in a mold under pressure in the absence of water vapor.
-
公开(公告)号:DE102005015892A1
公开(公告)日:2006-10-12
申请号:DE102005015892
申请日:2005-04-06
Applicant: BASF AG
Inventor: ALLMENDINGER MARKUS , HAHN KLAUS , RUCH JOACHIM , SCHMIED BERNHARD , HOLOCH JAN
Abstract: The invention relates to a process for producing antistatically treated, expandable styrene polymers, in which a styrene polymer melt is admixed with from 0.05 to 6% by weight of an antistatic and a blowing agent, extruded through a die and pelletized.
-
公开(公告)号:DE102005005494A1
公开(公告)日:2006-08-10
申请号:DE102005005494
申请日:2005-02-04
Applicant: BASF AG
Inventor: HAHN KLAUS , EHRMANN GERD , RUCH JOACHIM , ALLMENDINGER MARKUS , SCHMIED BERNHARD , HOLOCH JAN , MUEHLBACH KLAUS
-
公开(公告)号:DE50302746D1
公开(公告)日:2006-05-11
申请号:DE50302746
申请日:2003-06-06
Applicant: BASF AG
Inventor: DIETZEN FRANZ-JOSEF , EHRMANN GERD , SCHMIED BERNHARD , LAUN MARTIN , HAHN KLAUS , RUCH JOACHIM , HOLOCH JAN , ALLMENDINGER MARKUS , DATKO ACHIM
IPC: C08J9/00 , C08J9/16 , B29B9/10 , B29B11/10 , B29C44/34 , B29C48/345 , B29K25/00 , B29K105/04
Abstract: A process for the preparation of expandable styrene polymers having a molecular weight Mw of greater than 170,000 g/mol, which comprises conveying a blowing agent-containing styrene polymer melt having a temperature of at least 120° C. through a die plate with holes whose diameter at the die exit is at most 1.5 mm, and subsequently granulating the extrudate, and expandable styrene polymers (EPS) having a molecular weight Mw of more than 170,000 g/mol with 0.05 to 1.5% by weight of internal water.
-
公开(公告)号:DE102004034516A1
公开(公告)日:2006-02-16
申请号:DE102004034516
申请日:2004-07-15
Applicant: BASF AG
Inventor: HAHN KLAUS , EHRMANN GERD , RUCH JOACHIM , ALLMENDINGER MARKUS , SCHMIED BERNHARD , HOLOCH JAN
Abstract: The invention relates to a method for the production of flameproof, expandable styrol polymers (EPS) by extruding a styrol polymer melt containing a propellant and flameproof agents through a nozzle plate with subsequent under water granulation. The residence time of the flameproof agent is less than 30 minutes at a melting temperature in the region of between 140 to 220 °C.
-
公开(公告)号:DE102004034514A1
公开(公告)日:2006-02-16
申请号:DE102004034514
申请日:2004-07-15
Applicant: BASF AG
Inventor: HAHN KLAUS , EHRMANN GERD , RUCH JOACHIM , ALLMENDINGER MARKUS , SCHMIED BERNHARD , HOLOCH JAN , SCHMAUS PAULUS
Abstract: A process for producing flame-resistant, expandable styrene polymers (EPS) or flame-resistant extruded styrene polymer foams (XPS), wherein an organic bromine compound having a bromine content of at least 70% by weight is used as flame retardant and a liquid peroxide, hydroperoxide or a peroxide solution is used as flame retardant synergist.
-
公开(公告)号:DE102004034515A1
公开(公告)日:2006-02-02
申请号:DE102004034515
申请日:2004-07-15
Applicant: BASF AG
Inventor: HAHN KLAUS , EHRMANN GERD , RUCH JOACHIM , ALLMENDINGER MARKUS , SCHMIED BERNHARD , HOLOCH JAN
-
公开(公告)号:PL374432A1
公开(公告)日:2005-10-17
申请号:PL37443203
申请日:2003-06-06
Applicant: BASF AG
Inventor: DIETZEN FRANZ-JOSEF , EHRMANN GERD , SCHMIED BERNHARD , LAUN MARTIN , HAHN KLAUS , RUCH JOACHIM , ALLMENDINGER MARKUS , DATKO ACHIM , HOLOCH JAN
IPC: C08J9/00 , B29B9/10 , B29B11/10 , B29C44/34 , B29C48/345 , B29K25/00 , B29K105/04 , C08J9/16
Abstract: A process for the preparation of expandable styrene polymers having a molecular weight Mw of greater than 170,000 g/mol, which comprises conveying a blowing agent-containing styrene polymer melt having a temperature of at least 120° C. through a die plate with holes whose diameter at the die exit is at most 1.5 mm, and subsequently granulating the extrudate, and expandable styrene polymers (EPS) having a molecular weight Mw of more than 170,000 g/mol with 0.05 to 1.5% by weight of internal water.
-
-
-
-
-
-
-
-
-