公开(公告)号:AT484535T
公开(公告)日:2010-10-15
申请号:AT08759662
申请日:2008-05-16
Applicant: BASF SE
Inventor: SCHAEDLER VOLKER , FRICKE MARC , WIEGMANN WERNER , EMGE ANDREAS , RAMAN VIJAY IMMANUEL , SANCHEZ-FERRER ANTONIO
IPC: C08G18/32 , C08G18/76 , C08G101/00
Abstract: The invention relates to a xerogel comprising from 30 to 90% by weight of a monomer component (a1) composed of at least one polyfunctional isocyanate and from 10 to 70% by weight of a monomer component (a2) composed of at least one polyfunctional aromatic amine, at least one of which is selected from 4,4′-diaminodiphenylmethane, 2,4′-diaminodiphenylmethane, 2,2′-dIamino-diphenylmethane and oligomeric diaminodiphenylmethane, where the sum of the % by weight of monomer components (a1) and (a2) adds up to 100% by weight and where the monomer components are present in polymeric form in the xerogel and the volume-weighted mean pore diameter of the xerogel is at most 5 μm. The invention further relates to a process for preparing xerogels, to the xerogels thus obtainable and to the use of the xerogels as an insulating material and in vacuum insulation panels.
-
公开(公告)号:MX2010004701A
公开(公告)日:2010-05-20
申请号:MX2010004701
申请日:2008-11-13
Applicant: BASF SE
Inventor: EMGE ANDREAS , LOEFFLER ACHIM , ORTALDA MARCO , FREIDANK DANIEL , MOHMEYER NILS , SCHOEPS SIBYLLE
IPC: C08G18/12
Abstract: Poliuretano espumado obtenible por la mezcla de a) poliisocianatos, b) compuestos con un peso molecular relativamente elevado que tienen grupos reactivos para con los grupos isocianato, c) partículas sólidas, d) agentes de soplado, e) siendo apropiado, un extensor de cadena, un agente reticulante o mezclas de los mismos, f) siendo apropiado, un catalizador y g) siendo apropiado, otros aditivos para dar una mezcla de reacción y dejar a la misma reaccionar en forma completa, donde la proporción del extensor de cadena es menor al 6% en peso, con base en el peso total de los componentes a) a f), donde el contenido de las partículas sólidas es mayor al 15% en peso, con base en el peso total de los componentes a) a f), y donde la funcionalidad promedio de los compuestos con un peso molecular relativamente elevado que tienen grupos reactivos para con los grupos isocianato es menor que 2,5. Además, un moldeado que comprende un poliuretano espumado de acuerdo con la invención, un proceso para la preparación del poliuretano espumado de acuerdo con la invención y el uso de una moldura de acuerdo con la invención como una suela para calzado.
-
公开(公告)号:ES2335322T3
公开(公告)日:2010-03-24
申请号:ES07803299
申请日:2007-09-06
Applicant: BASF SE
Inventor: EMGE ANDREAS , FREIDANK DANIEL , SEIFERT HOLGER
Abstract: Procedimiento para la obtención de espumas rígidas de poliuretano por conversión de a) poliisocianatos con b) compuestos con, al menos, dos átomos de hidrógeno reactivos ante grupos isocianato en presencia de c) agentes de expansión caracterizado porque como compuestos se utilizan, junto con, al menos, dos átomos de hidrógeno reactivos ante grupos isocianato b), al menos, un poliol Graft b1) que puede obtenerse a través de la polimerización in-situ de monómeros olefínicamente insaturados en un alcohol de poliéter b1i), asimismo, el alcohol de poliéter b1i) presenta una funcionalidad de 2 a 4 y un índice hidroxilo en el rango de entre 100 y 250 mg KOH/g, su cadena poliéter está formada por óxido de propileno y hasta un 20% en peso, en relación al alcohol de poliéter b1i), de óxido de etileno, y, como monómeros olefínicamente insaturados se utilizan acrilnitrilo y estireno en una relación en peso de acrilnitrilo: estireno de > 1 : 1 a 4 : 1, y la conversión se lleva a cabo en presencia de, al menos, un compuesto mezclable en presencia de, al menos, un alcohol de poliéter b1i) con, al menos, un doble enlace olefínico b1ii).
-
公开(公告)号:PL1842976T3
公开(公告)日:2010-01-29
申请号:PL07103984
申请日:2007-03-13
Applicant: BASF SE
Inventor: ALTEHELD ARMIN , EMGE ANDREAS , GUERIN MOREIRA ANDRE , SCHIPS CARSTEN , FRANCIS TIMOTHY , HAHN KLAUS , SEIFERT HOLGER , TURZNIK GERHARD
-
公开(公告)号:AT449120T
公开(公告)日:2009-12-15
申请号:AT07803299
申请日:2007-09-06
Applicant: BASF SE
Inventor: EMGE ANDREAS , FREIDANK DANIEL , SEIFERT HOLGER
Abstract: The invention relates to a process for producing rigid polyurethane foams by reacting a) polyisocyanates with b) compounds having at least two hydrogen atoms which are reactive toward isocyanate groups in the presence of c) blowing agents, wherein at least one graft polyol b1) which can be prepared by in-situ polymerization of olefinically unsaturated monomers in a polyether alcohol b1i), where the polyether alcohol b1i) has a functionality of from 2 to 4 and a hydroxyl number in the range from 100 to 250 mg KOH/g, its polyether chain comprises propylene oxide and up to 20% by weight, based on the polyether alcohol b1i), of ethylene oxide, and acrylonitrile and styrene in a weight ratio of acrylonitrile:styrene of from >1:1 to 4:1 are used as olefinically unsaturated monomers, is used as compounds having at least two hydrogen atoms which are reactive toward isocyanate groups b), and the reaction is carried out in the presence of at least one compound b1ii) which has at least one olefinic double bond and is miscible with the polyether alcohol b1i).
-
公开(公告)号:DE502007001214D1
公开(公告)日:2009-09-17
申请号:DE502007001214
申请日:2007-03-13
Applicant: BASF SE
Inventor: ALTEHELD ARMIN , EMGE ANDREAS , GUERIN MOREIRA ANDRE , SCHIPS CARSTEN , FRANCIS TIMOTHY , HAHN KLAUS , SEIFERT HOLGER , TURZNIK GERHARD
-
公开(公告)号:ES2920952T3
公开(公告)日:2022-08-12
申请号:ES17754361
申请日:2017-08-21
Applicant: BASF SE
Inventor: MEYER ANDRE , EMGE ANDREAS
IPC: C08G18/48 , C08F283/00 , C08F283/06 , C08G18/08 , C08G18/32 , C08G18/36 , C08G18/50 , C08G18/66 , C08G18/76 , C09J151/08 , C09J175/04 , C09J175/08
Abstract: La invención se relaciona con un método para producir un material compuesto de fibra de poliuretano, en el que (a) di- y/o poliisocianato, (b) compuestos con átomos de hidrógeno que son reactivos hacia los grupos de isocianato, (c) que contienen al menos un carbono-carbonato-carbonato-carbonato doble enlace, (d) opcionalmente un catalizador que acelera la reacción de uretano, (e) opcionalmente iniciadores radicales, y (f) opcionalmente se mezclan agentes y aditivos auxiliares adicionales para formar una mezcla de reacción con la que un material de fibra se hambre y cura. Los compuestos con átomos de hidrógeno que son reactivos hacia el isocianato en promedio tienen al menos 1.5 grupos de hidrógeno que son reactivos hacia el isocianato por molécula; La densidad de doble enlace del compuesto (C) es al menos 21%; La funcionalidad de doble enlace del compuesto (c) es mayor que 1; El compuesto (c) no tiene grupos que son reactivos hacia el isocianato; y la relación equivalente de los grupos de isocianato de los di- y/o poliisocianatos (a) y los átomos de hidrógeno que son reactivos hacia el isocianato del compuesto (b) de 0.8 a 2. La invención se relaciona adicionalmente con un material compuesto de fibra de poliuretano que puede obtenerse utilizando el método de acuerdo con la invención y el uso del material compuesto de fibra de poliuretano como componentes estructurales. (Traducción automática con Google Translate, sin valor legal)
-
公开(公告)号:ES2540280T5
公开(公告)日:2022-04-19
申请号:ES05798205
申请日:2005-09-28
Applicant: BASF SE
Inventor: EMGE ANDREAS , SEIFERT HOLGER , DINSCH STEFAN , KLASSEN JOHANN , STELLING CHRISTIAN
-
49.
公开(公告)号:RU2765295C2
公开(公告)日:2022-01-28
申请号:RU2020108690
申请日:2018-07-31
Applicant: BASF SE
Inventor: MEYER ANDRE , EMGE ANDREAS , HASENPATT MICHAEL
IPC: B29B15/12
Abstract: Изобретениеотноситсяк устройствудляпропиткиволоконматричнымматериалом. Техническимрезультатомявляетсяобеспечениепостояннойзаданнойобъемнойдоливолокон, неизменяющейсявследствиеколебанийтехнологическихпараметровпроцессапропитки. Техническийрезультатдостигаетсяустройствомдляпропиткиволоконматричнымматериалом, котороевключаетузелпропиткиволоконматричнымматериалом. Приэтомоновключаетузелдлярегулировкиобъемногосодержанияволокон, имеющийпоменьшеймереодноотверстие, черезкотороепропускаютпропитанныеволокна. Причемминимальныйразмерпоперечногосечениякаждогоотверстиярассчитываюттакимобразом, чтобыможнобылоудалятьстолькоматричногоматериала, сколькотребуетсядлядостижениязаданногообъемногосодержанияволокон. Приэтомузелдляустановкиобъемногосодержанияволоконвключаетверхнюючастьи нижнюючасть. Причемотверстиевыполненосоответственночастичнов нижнейчастии частичнов верхнейчасти. 2 н. и 22 з.п. ф-лы, 30 ил.
-
50.
公开(公告)号:PH12020551287A1
公开(公告)日:2021-07-12
申请号:PH12020551287
申请日:2020-08-20
Applicant: BASF SE
Inventor: EMGE ANDREAS , MEYER ANDRE , ELING BEREND , AUFFARTH STEFAN
IPC: C08J9/00 , C08F283/00 , C08G18/08 , C08G18/22 , C08G18/32 , C08G18/36 , C08G18/48 , C08G18/66 , C08G18/72 , C08G18/76 , C08G18/79 , C08K5/10
Abstract: The invention relates to a method for producing a polyurethane material, wherein (a) di- and/or polyisocyanates, (b) compounds that have hydrogen atoms reactive with isocyanate groups and that do not contain any compounds having carbon-carbon double bonds, (c) compounds containing at least one carbon-carbon double bond, (d) optionally a catalyst that accelerates the urethane reaction and (e) optionally further auxiliary agents and additives are mixed to form a reaction mixture and are cured at temperatures of greater than 120 øC. The compounds having hydrogen atoms reactive with isocyanate (b) have on average at least 1.5 hydrogen groups reactive with isocyanate per molecule, and the compounds having a carbon-carbon double bond (c) contain compounds (c1) that have at least one carbon-carbon double bond and at least one group selected from groups reactive with isocyanate or from isocyanate groups and/or (c2) that have at least two carbon-carbon double bonds. The reaction mixture is stabilized to such an extent that the polyurethane material that is obtained after mixing of components (a) to (c) and, if present, (d) and (e) at room temperature, injection into a metal mold temperature-controlled to 80 øC and having the dimensions 20 cm x 30 cm x 0.4 cm, demolding after 60 minutes and cooling to room temperature, has a heat distortion temperature (three-point bending at 0.45 MPa extreme fiber stress according to DIN EN ISO 75) that is at least 15 øC lower than the heat distortion temperature of the identically produced polyurethane material which, after production, is additionally thermally treated for 120 minutes at 150 øC in a furnace and subsequently cooled to room temperature. The invention further relates to a polyurethane material that can be obtained by a method of this type, and to the use of the polyurethane material, in particular a polyurethane fiber composite material, as structural components.
-
-
-
-
-
-
-
-
-