CHEMICALLY STRENGTHENED LITHIUM DISILICATE-PETALITE GLASS-CERAMICS

    公开(公告)号:US20200148591A1

    公开(公告)日:2020-05-14

    申请号:US16682143

    申请日:2019-11-13

    Abstract: Ion-exchanged glass ceramic articles described herein have a stress that decreases with increasing distance according to a substantially linear function from a depth of about 0.07 t to a depth of about 0.26 t from the outer surface of the ion-exchanged glass ceramic article from a compressive stress to a tensile stress. The stress transitions from the compressive stress to the tensile stress at a depth of from about 0.18 t to about 0.25 t from the outer surface of the ion-exchanged glass ceramic article. An absolute value of a maximum compressive stress at the outer surface of the ion-exchanged glass article is from 1.8 to 2.2 times an absolute value of a maximum central tension (CT) of the ion-exchanged glass article, and the glass ceramic article has a fracture toughness of 1 MPa√m or more as measured according to the double cantilever beam method.

    Methods of forming shaped glass articles from glass sheets

    公开(公告)号:US10479052B2

    公开(公告)日:2019-11-19

    申请号:US15504133

    申请日:2015-08-17

    Abstract: A method of forming a 3D glass article from a glass sheet includes locating the glass sheet on a mold assembly including a mold surface with a 3D surface profile corresponding to that of the 3D glass article. The glass sheet is heated to a forming temperature. The forming temperature is greater than a temperature of the mold surface. The heated glass sheet is forced onto the mold surface by applying a pressurized gas to a first surface of the glass sheet opposite the mold surface to conform the glass sheet to the mold surface with the glass sheet at the forming temperature that is greater than the temperature of the mold surface.

    Methods of forming shaped glass articles from glass sheets

    公开(公告)号:US10442160B2

    公开(公告)日:2019-10-15

    申请号:US15504133

    申请日:2015-08-17

    Abstract: A method of forming a 3D glass article from a glass sheet includes locating the glass sheet on a mold assembly including a mold surface with a 3D surface profile corresponding to that of the 3D glass article. The glass sheet is heated to a forming temperature. The forming temperature is greater than a temperature of the mold surface. The heated glass sheet is forced onto the mold surface by applying a pressurized gas to a first surface of the glass sheet opposite the mold surface to conform the glass sheet to the mold surface with the glass sheet at the forming temperature that is greater than the temperature of the mold surface.