Abstract:
A method of making wire rope which when finished comprises a plural number of wires assembled in a twisted state. Each of said wires is first electroplated with zinc and thence diametrically adjusted as to its length by the application of a cold working thereto. Then the wire rope is further electroplated with tin thereby obtaining corrosion-proof and solderable property besides becoming resistant against friction and the like due to its surface lubrication in comparison with conventional wire ropes.
Abstract:
A process for manufacturing an elongated steel element for reinforcing rubber products includes forming, on an elongated steel element, a coating of a ternary or quaternary alloy of copper-M-zinc, where M is one or two metals selected from cobalt, nickel, tin, indium, manganese, iron, bismuth and molybdenum; drawing the elongated steel element in an aqueous lubricant containing a phosphorus compound and nitrate; and twisting two or more of the elongated steel elements into a steel cord. A copper content inside the coating is 58 to 75 wt %. A content of the one or two metals inside the coating is 0.5 to 10 wt %. A final reduction in a diameter of the elongated steel element occurs during the drawing step. The phosphorus compound is present on and/or in the coating in an amount of 0.3 to 1 mg/m2 of the coating, as measured via an Inductively Coupled Plasma technique.
Abstract:
A rope (20) comprising a core element (22) surrounded by a plurality of helically twisted and compacted steel strands (24) comprising steel wires (25, 26, 27) having a nominal tensile strength of at least 1960 N/mm2. The core element (22) comprises natural fibers having a linear density of at least 50 g/m.
Abstract translation:一种绳索(20),包括由包括具有至少为1960N / mm 2的标称拉伸强度的钢丝(25,26,27)的多个螺旋扭曲和压实的钢绞线(24)包围的芯元件(22)。 核心元件(22)包括线密度为至少50g / m 2的天然纤维。
Abstract:
The invention relates to cord (20) comprising a number of filaments twisted together. The peripheral surface of the cord (20) is at least partially coated with an adhesion promoting coating (24). The adhesion promoting coating (24) comprises at least a first layer comprising a silicon based coating, a titanium based coating, a zirconium based coating or a combination thereof. The invention further relates to a composite material comprising such a cord (20) embedded in a polymer material. Furthermore the invention relates to a method to manufacture such a cord (20).
Abstract:
A load bearing member (22) useful in an elevator system (10) includes at least one elongated tension member (36), a conversion coating (46) on the elongated tension member (36), and a polymer jacket (34) at least partially surrounding the coated elongated tension member (36). In one example, the conversion coating (46) includes at least one of an oxide, a phosphate, or a chromate.
Abstract:
The present invention relates to a brass-plated steel cord capable of further improving initial adhesiveness and heat-resistant adhesiveness between a coating rubber and a steel cord and also imparting excellent durability to a resulting rubber article, and more particularly to a brass-plated steel cord, wherein an outermost surface thereof contains 0.3 to 1.7 atomic % of phosphorus, 4.93 to 14 atomic % of zinc, and 0.01 to 2.0 atomic % of a metal having an ionization tendency lower than that of zinc and higher than that of copper as measured by XPS (X-ray photoelectron spectroscopy), and an amount of zinc in the outermost surface is 30 to 90 atomic % based on 100 atomic % of a total amount of zinc and copper.
Abstract:
An elongated steel element adapted for the reinforcement of rubber products is covered with a ternary or quaternary alloy coating of copper-M-zinc. M is one or two metals selected from the group consisting of cobalt, nickel, tin, indium, manganese, iron, bismuth and molybdenum. The copper content inside the coating ranges from 58 weight per cent to 75 weight per cent, the content of said one or two metals inside the coating ranges from 0.5 weight per cent to 10 weight per cent, the remainder is zinc and unavoidable impurities. The one or two metals are present throughout the coating. The phosphorus is present on and/or in the coating in an amount ranging from 0.3 milligram per square meter to 1 milligram per square meter of the coating. The coating further lacks triazole residues. Good results for under cure adhesion have been obtained. Furthermore, a corresponding method for manufacturing such an elongated steel element is disclosed.
Abstract:
A load bearing member includes at least one elongated tension member having at least one wire and a protective coating on the elongated tension member. The protective coating includes a first corrosion inhibitor having an oxide-forming metal, a second corrosion inhibitor having a rare earth metal, and a third corrosion inhibitor having an organic material.