다성분계 비스무스 몰리브데이트 촉매, 그 제조방법 및 상기 촉매를 이용한 1,3-부타디엔 제조방법
    52.
    发明公开
    다성분계 비스무스 몰리브데이트 촉매, 그 제조방법 및 상기 촉매를 이용한 1,3-부타디엔 제조방법 有权
    多元双酚B-MOLYBASE催化剂及其制备方法及使用合成催化剂制备1,3丁二烯的方法

    公开(公告)号:KR1020100028702A

    公开(公告)日:2010-03-15

    申请号:KR1020080087550

    申请日:2008-09-05

    CPC classification number: B01J23/31 B01J37/036 B01J37/04 B01J37/08 C07C11/167

    Abstract: PURPOSE: A multicomponent bismuth-molybdate catalyst, a method of producing thereof, and a method of producing 1,3-butadiene using thereof are provided to obtain the 1,3-butadiene with high yield using a C4 distillate with a lot of impurities as a reactant directly. CONSTITUTION: A multicomponent bismuth-molybdate catalyst is used to produce 1,3-butadiene from a C4 distillate including normal-butane and normal-butene by an oxidative dehydration, which essentially contains bismuth and molybdenum component and a metallic component with divalent or trivalent cation. The metallic component with divalent or trivalent cation is selected from the group consisting of cobalt, nickel, zinc, magnesium, manganese, copper, iron, potassium, sodium, aluminum, vanadium, zirconium, tungsten and silicon.

    Abstract translation: 目的:提供一种多组分钼酸铋催化剂及其制备方法,以及使用该方法制备1,3-丁二烯的方法,使用具有大量杂质的C 4馏出物以高产率获得1,3-丁二烯 直接反应。 构成:使用多组分钼酸铋催化剂通过氧化脱水从包含正丁烷和正丁烯的C4馏出物生产1,3-丁二烯,其基本上含有铋和钼组分以及具有二价或三价阳离子的金属组分 。 具有二价或三价阳离子的金属组分选自钴,镍,锌,镁,锰,铜,铁,钾,钠,铝,钒,锆,钨和硅。

    폴리스티렌 입자의 존재 하에서 티타늄 실리카라이트-1촉매를 제조하는 방법 및 상기 촉매를 이용한산화프로필렌의 제조 방법
    53.
    发明授权
    폴리스티렌 입자의 존재 하에서 티타늄 실리카라이트-1촉매를 제조하는 방법 및 상기 촉매를 이용한산화프로필렌의 제조 방법 失效
    在聚苯乙烯颗粒存在下生产钛硅沸石-1催化剂的方法和使用该催化剂生产环氧丙烷的方法

    公开(公告)号:KR100927524B1

    公开(公告)日:2009-11-17

    申请号:KR1020070109638

    申请日:2007-10-30

    CPC classification number: Y02P20/52

    Abstract: 본 발명은 MFI 구조의 티타늄 함유 제올라이트인 티타늄 실리카라이트-1(Titanium Silicalite-1: TS-1) 촉매의 제조 방법 및 상기 촉매를 이용하여 산화프로필렌(Propylene Oxide: PO)을 제조하는 방법에 관한 것으로, 좀 더 구체적으로는, 폴리스티렌(Polystyrene: PS) 입자의 존재 하에서 수열합성에 의해 티타늄 실리카라이트-1 촉매를 제조하는 방법, 및 상기 촉매의 존재 하에 과산화수소를 산화제로 사용하여 프로필렌을 에폭시화(Epoxidation)함으로써 산화프로필렌을 제조하는 방법에 관한 것이다.
    본 발명에 따라 제조된 티타늄 실리카라이트-1에는 프로필렌 에폭시화 반응에 대해 불활성인 아나타제(Anatase) 상이 적게 형성되므로, 본 발명에 따른 티타늄 실리카라이트-1을 프로필렌의 에폭시화 반응의 촉매로 사용할 경우, 보다 향상된 산화프로필렌의 선택도 및 수율을 얻을 수 있는 효과를 갖는다.
    티타늄 실리카라이트-1, 폴리스티렌, 프로필렌, 과산화수소, 산화프로필렌, 프로필렌 에폭시화

    Abstract translation: 涉及一种方法,用于生产:(PO环氧丙烷):含有沸石本发明-1钛是氧化丙烯的MFI结构(钛硅质岩1 TS-1)的钛硅沸石使用该方法制造的催化剂和催化剂的 更具体地,聚苯乙烯:由(聚苯乙烯PS)中的粒子的方法的存在下,通过水热合成使用用于生产在用氧化剂环氧丙烯化学催化剂的存在下,钛硅沸石-1催化剂和过氧化氢(环氧化 )生产环氧丙烷。

    연속 흐름식 2중 촉매 반응 장치를 이용하여노르말-부텐으로부터 1,3-부타디엔을 제조하는 방법
    54.
    发明公开
    연속 흐름식 2중 촉매 반응 장치를 이용하여노르말-부텐으로부터 1,3-부타디엔을 제조하는 방법 有权
    使用连续流动双壁反应器从N-丁烯生产1,3-丁二烯的方法

    公开(公告)号:KR1020090103424A

    公开(公告)日:2009-10-01

    申请号:KR1020080029032

    申请日:2008-03-28

    CPC classification number: C07C5/42 C07C2523/80 C07C2523/887 C07C11/167

    Abstract: PURPOSE: A method for producing 1,3-butadiene from n-butene using continuous-flow dual-bed reactor with excellent catalyst reproducibility is provided to obtain 1,3-butadiene at high yield by maximizing activity of oxidation-dehydrogenation of n-butene. CONSTITUTION: A method for producing 1,3-butadiene from n-butene using continuous-flow dual-bed reactor comprises the steps of: laminating and filling a bismuth molybdate-based first catalyst and a ferrite-based second catalyst, which are a catalyst-fixed layer on a reactor by a quartz layer so that a separated laminated layer is formed; performing oxidation-dehydrogenation while consecutively passing a C4 mixture including normal butane and a reactant containing air and steam through a catalyst layer of the reactor; and obtaining 1,3-butadiene.

    Abstract translation: 目的:提供使用具有优异催化剂再现性的连续流动双床反应器从正丁烯生产1,3-丁二烯的方法,通过使正丁烯氧化脱氢的活性最大化,以高产率获得1,3-丁二烯 。 构成:使用连续流动双床反应器从正丁烯生产1,3-丁二烯的方法包括以下步骤:层压和填充钼酸铋基第一催化剂和作为催化剂的铁酸盐基第二催化剂 - 混合层,通过石英层在反应器上形成分离的层压层; 进行氧化脱氢,同时使含有正丁烷的C4混合物和含有空气和蒸汽的反应物通过反应器的催化剂层; 并得到1,3-丁二烯。

    알루미나 담체에 화학적으로 고정화된 니켈 촉매, 그 제조 방법 및 상기 촉매를 이용한 액화천연가스의 수증기 개질 반응에 의한 수소 가스 제조 방법
    59.
    发明公开
    알루미나 담체에 화학적으로 고정화된 니켈 촉매, 그 제조 방법 및 상기 촉매를 이용한 액화천연가스의 수증기 개질 반응에 의한 수소 가스 제조 방법 有权
    镍合金催化剂化学稳定在多孔氧化铝支持下,通过使用合适的催化剂对液化天然气进行蒸汽转化,制备方法及氢气生产方法

    公开(公告)号:KR1020160073061A

    公开(公告)日:2016-06-24

    申请号:KR1020140181396

    申请日:2014-12-16

    CPC classification number: Y02P20/52 B01J37/02 B01J23/755 B01J37/08 C01B3/40

    Abstract: 본발명은알루미나담체에화학적으로고정화된니켈촉매, 그제조방법및 상기촉매를이용한액화천연가스(Liquefied Natural gas; LNG)의수증기개질반응에의한수소가스제조방법에관한것으로, 보다상세하게는액화천연가스(LNG)의수증기개질반응에의한수소가스제조에사용되며, 알루미나담체상에양전하를부여하고니켈전구체의킬레이트화(Chelation)에의해얻어진음이온성의니켈계복합이온을산 처리된알루미나담체표면의양전하와결합하게하여고정화시킨뒤 건조및 소성과정을거쳐제조되며, 니켈의담지량이 5 내지 50 중량%인것을특징으로하는알루미나담체에화학적으로고정화된니켈촉매, 그제조방법및 상기촉매를이용한액화천연가스(LNG)의수증기개질반응에의한수소가스제조방법에관한것이다. 본발명에의하면상용함침법에의해알루미나담체에담지된니켈촉매에비해물리적특성및 활성니켈표면적이개선된촉매를제조할수 있을뿐만아니라, 이를액화천연가스(LNG)의수증기개질반응에적용하여고순도의수소가스를장시간동안효율적으로제조할수 있다.

    Abstract translation: 本发明涉及化学固定在氧化铝载体上的镍催化剂及其制备方法,以及通过使用催化剂通过液化天然气(LNG)的蒸汽重整制备氢气的方法。 更具体地说,本发明涉及化学固定在氧化铝载体上的镍催化剂及其制备方法,以及通过使用催化剂通过LNG的蒸汽重整制备氢气的方法,所述镍催化剂的特征在于:使用 用于通过LNG的蒸汽重整制备氢气; 通过在氧化铝载体上赋予正电荷,然后将通过螯合镍前体获得的阴离子镍基络合物离子与酸处理的氧化铝载体的表面的正电荷结合,然后干燥和塑化 结果; 并具有加载5〜50重量%的镍的能力。 根据本发明,可以制备具有通过典型浸渍由氧化铝载体承载的镍催化剂具有改进的物理性能和活性镍表面的催化剂,使得本发明可以应用于LNG的蒸汽重整,从而有效地制备氢 天然气高纯度长时间。

Patent Agency Ranking