Lean austenitic stainless steel
    52.
    发明专利

    公开(公告)号:AU2013200660B2

    公开(公告)日:2015-09-17

    申请号:AU2013200660

    申请日:2013-02-07

    Abstract: - 17 [0054] An austenitic stainless steel having low nickel and molybdenum and 5 exhibiting comparable corrosion resistance and formability properties to higher nickel and molybdenum alloys consisting of in % weight up to 0.20 C, 2.0-9.0 Mn, up to 2.0 Si, 16.0-23.0 Cr, 1.0-3.0 Ni, up to 3.0 Mo, 0.1-0.35 N, up to 4.0 W, up to 0.01 B, up to 1.0 Co, iron and impurities, the steel having a ferrite number less than 10, and a MD30 value of less than 20'C. 4059328_1 (GHMatters) P84069.AU.1 7/02/13

    Lean austenitic stainless steel
    55.
    发明专利

    公开(公告)号:AU2013200660A1

    公开(公告)日:2013-02-28

    申请号:AU2013200660

    申请日:2013-02-07

    Abstract: - 17 [0054] An austenitic stainless steel having low nickel and molybdenum and 5 exhibiting comparable corrosion resistance and formability properties to higher nickel and molybdenum alloys consisting of in % weight up to 0.20 C, 2.0-9.0 Mn, up to 2.0 Si, 16.0-23.0 Cr, 1.0-3.0 Ni, up to 3.0 Mo, 0.1-0.35 N, up to 4.0 W, up to 0.01 B, up to 1.0 Co, iron and impurities, the steel having a ferrite number less than 10, and a MD30 value of less than 20'C. 4059328_1 (GHMatters) P84069.AU.1 7/02/13

    ACERO INOXIDABLE AUSTENITICO CON BAJO CONTENIDO DE NIQUEL QUE CONTIENE ELEMENTOS DE ESTABILIZACION.

    公开(公告)号:MX2010006038A

    公开(公告)日:2010-08-11

    申请号:MX2010006038

    申请日:2008-02-20

    Abstract: Una composición de acero inoxidable austenítico que incluye niveles relativamente bajos de níquel y molibdeno, y que presenta resistencia a la corrosión, resistencia a la deformación a temperaturas elevadas y propiedades de formabilidad comparables a ciertas aleaciones que incluyen niveles elevados de níquel y molibdeno. Modalidades del acero inoxidable austenítico incluyen, en porcentaje en peso, hasta 0.20% de C, 2.0-9.0% de Mn, hasta 2.0% de Si, 16.0-23.0% de Cr, 1.0-7.0% de Ni, hasta 3.0% de Mo, hasta 3.0% de Cu, 0.05- 0.35% de N, hasta 4.0% de W, (75(%C)) = (Nb+Ti+V+Ta+Zr) = 1.5, hasta 0.01% de B, hasta 1.0% de Co, hierro e impurezas. Además, modalidades del acero pueden incluir 0.5 = (Mo+W/2) 5.0 y/o 1.0 = (Ni+Co) s 8.0.

    CORROSION RESISTANT AUSTENITIC STAINLESS STEEL

    公开(公告)号:CA2355109C

    公开(公告)日:2009-09-22

    申请号:CA2355109

    申请日:1999-12-13

    Abstract: An alloy having a composition, by weight, of about 0.025 % or less carbon, about 0.5 to about 4.1 % manganese, about 5.5 to about 6.2 % silicon, about 11 to about 15 % chromium, about 9.0 to about 15.5 % nickel, about 0.8 to about 1.2 % molybdenum and about 0.8 to about 2 % copper and the remainder being essentially iron with incidental impurities. This composition results in lean alloy content in a high silicon austenitic stainless steel for concentrated sulfuric acid service while maintaining a corrosion rate similar to and competitive with existing alloys for such service. Acceptable characteristics were found when hot working was carried out in the range of about 2100 .degree.F to about 2200 .degree.F. Annealing in the range of about 1925 .degree.F to about 2025 .degree.F is preferred, as is rapid water quenching after annealing.