Abstract:
A polyolefin composition comprising: A) from 19 wt% to 50 wt% of a propylene ethylene copolymer having an ethylene derived units content ranging from 1.5 wt% to 6.0 wt% B) from 50 wt% to 81 wt% of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from 1.5 wt% and 6.0 wt% and 1-butene derived units content of between 4.8 wt% and 12.4 wt%; the sum of the amount of component A) and B) being 100; the composition being characterized by the following features: molecular weight distribution (MWD), expressed in terms of Mw/Mn, greater than 4.0; the creep and recovery curve measured on the polymer fuse at 200°C measured according to the procedure reported in the characterizing section shows a maximum value between 600 and 1200 seconds lower than 53x10 -5 1/Pa.
Abstract:
A polyolefin composition comprising: a) from 40.0 wt% to 58.5 wt%, of a propylene homopolymer having the fraction insoluble in xylene at 25°C higher than 96 wt% and an melt flow rate ranging from 95.0 to 200.0 g/10 min; b) from 21.0 wt% to 30.0 wt%, of a copolymer of ethylene and propylene, the copolymer having an amount of recurring units deriving from ethylene ranging from 35.0 wt% to 60.0 wt%, and the polymer fraction soluble in xylene at 25°C of component a) + component b) having an intrinsic viscosity value ranging from 3.1 to 4.2 dl/g; and, c) from 20.5 wt% to 30.0 wt%, of ethylene homopolymer; said composition having a value of melt flow rate ranging from 9.0 to 30.0 g/10 min, and the ratio between the MFR of component a) MFR a and the MFR of the total composition MFR T MFR a /MFR T is comprised between 5.0 and 15.0.
Abstract:
1. A polyolefin composition comprising: A) from 65 wt% to 85 wt%, of a propylene/ethylene/ 1-butene terpolymer wherein: i) the content of ethylene derived units ranges from 0.6 wt% to 2.5 wt; ii) the content of 1-butene derived units ranges from 6 wt% to 12 wt%; iii) the fraction soluble in xylene at 25 °C ranges from 3.5 wt% to 20 wt%; B) from 15 wt% to 35 wt% of a propylene/ethylene copolymer having a content of ethylene derived units ranging from 10 wt% to 40 wt%; the copolymer optionally can contains 1-butene derived units in an amount less than 1 wt%; the sum A) + B) being 100.
Abstract:
Propylene polymer compositions comprising: A) from 70 wt% to 95 wt%, of a random copolymer of propylene with ethylene, containing from 3.5 wt% to 8.5 wt%, of ethylene derived units, having a content of fraction soluble in xylene at 25°C comprised between 7.1 wt% and 15.2 wt% and having a melting point higher than 142.0°C; B) from 5 wt% to 35 wt%, of a copolymer of propylene with ethylene, containing from 8.5 wt% to 17.0 wt % of ethylene derived units; the sum A+B being 100; wherein the melt flow rate, MFR (ISO 1133 (230°C, 2.16 kg).) from 0.6g/10 min to 20.2 g/10 min.
Abstract:
A polyolefin composition comprising (percent by weight): A) from 65% to 75% of a propylene homopolymer or a propylene copolymer containing from 0.1% to 5.0% of ethylene derived units having a fraction soluble in Xylene at 25°C lower than 3wt%; B) from 25 % to 35% of an ethylene copolymer containing from 3% to 12 % of propylene derived units; said composition having a melt flow rate (MFR) determined according to ISO method 133(230° C and 2.16 kg)comprised between 11 g/10 min and 50 g/10 min; the xylene soluble fraction ranging from 3% to 15% and the intrinsic viscosity (IV) of the xylene soluble fraction ranging from 0.8 dl/g to 2 dl/g.
Abstract:
A container comprising a polyolefin composition comprising: A) from 59 wt% to 84 wt%, of a propylene homopolymer having isotactic pentads (mmmm) measured with by 13 C-NMR higher than 96%, B) from 16 wt% to 41 wt%, of a copolymer of propylene and ethylene with from 30wt% to 44wt%, of ethylene derived units; the sum A) + B) being 100; the composition having an MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) comprised from 72 to 100 g/10 min.
Abstract:
A polyolefin composition comprising: a) from 66 wt% to 76 wt% of a propylene polymer having the fraction insoluble in xylene at 25°C, higher than 97 wt%, a polydispersity index lower than 4.5, and a melt flow rate (MFR) determined according to ISO method 1133 (230° C and 2.16 kg)comprised between 6.0 g/10 min and 10.0 g/10 min, b) from 12 wt% to 20 wt% of acopolymer of ethylene and propylene, the copolymer having an amount of recurring units deriving from ethylene ranging from 40 wt% to 53 wt%,the polymer fraction soluble in xylene at 25°C having an intrinsic viscosity value ranging from 2 to 4 dl/g; c) from 12% to 20%% of ethylene homopolymer; the sum of the amount of a) +b) +c) being100; said composition having a value of melt flowrate (MFR) determined according to ISO method 1133 (230° C and 2.16 kg)ranging from 3.6 to 8.0 g/10 min.
Abstract:
A propylene composition comprising (percent by weight): A) 70%-95%, of a propylene homopolymer having a Polydispersity Index (P.I.) value of from 4.6 to 10, a fraction insoluble in xylene at 25 °C, higher than 90 %, and MFR L (Melt Flow Rate according to ISO 1133, condition L, i.e. 230°C and 2.16 kg load) from 47 to 90 g/10 min; B) 5%-30%, of a copolymer of propylene containing from 40% to 34.5% extremes included of ethylene derived units; the composition having an intrinsic viscosity of the fraction soluble in xylene at 25 °C comprised between 3 and 5 dl/g.
Abstract:
A polymer composition comprising (per cent by weight): a) 57%-74%, of a crystalline propylene polymer having an amount of isotactic pentads (mmmm), measured by 13 C-MNR on the fraction insoluble in xylene at 25° C, higher than 97.5 molar % and a polydispersity index ranging from 5 to 10; b) 8 to 15%, of an elastomeric copolymer of ethylene and propylene, the copolymer having an amount of recurring units deriving from ethylene ranging from 30 to 50%, and being partially soluble in xylene at ambient temperature; the polymer fraction soluble in xylene at ambient temperature having an intrinsic viscosity value ranging from 2.5 to 3.5 dl/g; and c) 18-28%, of ethylene homopolymer having an intrinsic viscosity value ranging from 1.5 to 4 dl/g; said composition having a value of melt flow rate ranging from 35 to 60 g/10 min, and the amount of hexane extractables lower than 4.0 wt%.
Abstract:
A propylene composition comprising (percent by weight): A) 60%-90%, of a crystalline propylene copolymer containing from 3.5% to 10% of ethylene derived units; B) 10%-40%, of a copolymer of propylene containing from 18.5% to 23.5%, of ethylene derived units.