Abstract:
Polyolefin compositions particularly suitable for cast film, exhibiting heat sealability, retortability, low haze and stiffness, comprising: 1) 75-85% of a propylene homopolymer or copolymer of propylene with ethylene and/or one or more C 4 -C 10 α-olefin(s), the homopolymer or copolymer having melting temperature equal to or higher than 150°C, 2) 15-25% of a copolymer of ethylene with one or more C 4 -C 10 α-olefin(s) containing from 20 to 30% of said C 4 -C 10 α-olefin(s); said composition having MFR (at 230°C, 2.16 kg) of from 5-10 g/10 min, the total content of ethylene of from 10 to 20 %, the total content of C 4 -C 10 α-olefin(s) of from 2 to 8 %, the ratio XStot/XSm of the total fraction soluble in Xylene at room temperature to the fraction soluble in Xylene at room temperature of the matrix component (1) of from 5 to 15, and the value of the intrinsic viscosity of the total fraction soluble in Xylene at room temperature (XSIVtot) of 1.5 dl/g or less.
Abstract:
A polyolefm compositions comprising: A) From 77 wt% to 90 wt%, of a propylene homopolymer having the fraction soluble in xylene at 25 °C lower than 2 wt%; B) from 10 wt% to 23 wt% of a copolymer of ethylene with one C4-C10 alpha-olefin containing from 20 wt% to 30 wt%, of said C4-C10 alpha-olefin derived units; said composition having - the value of melt flow rate (MFR) at 230 °C, 2.16 kg of from 0.5 to 4.5 g/10 min; - the total content of ethylene of from 10 wt% to 18 wt%; - the value of the intrinsic viscosity of the total fraction soluble in Xylene at 25°C (AMXSIVtot) is less than 1.5 dl/g.
Abstract:
A polyolefin composition comprising: A) from 19 wt% to 50 wt% of a propylene ethylene copolymer having an ethylene derived units content ranging from 1.5 wt% to 6.0 wt%; B) from 50 wt% to 81 wt% of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from 1.5 wt% and 6.0 wt% and 1-butene derived units content of between 4.8 wt% and 12.4 wt%; the sum of the amount of component A) and B) being 100; the composition being characterized by the following features: - the ratio C2wt%/C4wt% is comprised between 0.22 and 3.0, where C2wt% is the weight per cent of ethylene derived units and C4wt% is the weight per cent of 1-butene derived units; - the content of xylene soluble fraction at 25°C is comprised between 2 and 15 wt%; - molecular weight distribution (MWD), expressed in terms of Mw/Mn, greater than 4.0; recoverable compliance at 200°C having a maximum value between 800 and 1200 seconds lower than 65x10 -5 Pa -1 .
Abstract:
A polyolefin composition comprising: A) from 19 wt% to 50 wt% of a propylene ethylene copolymer having an ethylene derived units content ranging from 1.5 wt% to 6.0 wt% B) from 50 wt% to 81 wt% of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from 1.5 wt% and 6.0 wt% and 1-butene derived units content of between 4.8 wt% and 12.4 wt%; the sum of the amount of component A) and B) being 100.
Abstract:
A polyolefin composition comprising: A) from 19 wt% to 50 wt% of a propylene ethylene copolymer having an ethylene derived units content ranging from 1.5 wt% to 6.0 wt% B) from 50 wt% to 81 wt% of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from 1.5 wt% and 6.0 wt% and 1-butene derived units content of between 4.8 wt% and 12.4 wt%; the sum of the amount of component A) and B) being 100; the composition being characterized by the following features: molecular weight distribution (MWD), expressed in terms of Mw/Mn, greater than 4.0; the creep and recovery curve measured on the polymer fuse at 200°C measured according to the procedure reported in the characterizing section shows a maximum value between 600 and 1200 seconds lower than 53x10 -5 1/Pa.
Abstract:
A polyolefin compositions comprising: A) From 77 wt% to 90 wt%, of a propylene homopolymer having the fraction soluble in xylene at 25°C lower than 2 wt%; B) from 10 wt% to 23 wt% of a copolymer of ethylene with one C 4 -C 10 alpha-olefin containing from 20 wt% to 30 wt%, of said C 4 -C 10 alpha-olefin derived units; said composition having - the value of melt flow rate (MFR) at 230 °C, 2.16 kg of from 0.5 to 4.5 g/10 min; - the total content of ethylene of from 10 wt% to 18 wt%; - the value of the intrinsic viscosity of the total fraction soluble in Xylene at 25°C (AMXSIVtot) is less than 1.5 dl/g.
Abstract:
A polyolefin composition comprising: A) from 19 wt% to 50 wt% of a propylene ethylene copolymer having an ethylene derived units content ranging from 1.5 wt% to 6.0 wt%; B) from 50 wt% to 81 wt% of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from 1.5 wt% and 6.0 wt% and 1-butene derived units content of between 4.8 wt% and 12.4 wt%; the sum of the amount of component A) and B) being 100; the composition being characterized by the following features: - the ratio C2wt%/C4wt% is comprised between 0.22 and 3.0, where C2wt% is the weight per cent of ethylene derived units and C4wt% is the weight per cent of 1-butene derived units; - the content of xylene soluble fraction at 25°C is comprised between 2 and 15 wt%; - molecular weight distribution (MWD), expressed in terms of Mw/Mn, greater than 4.0; recoverable compliance at 200°C having a maximum value between 800 and 1200 seconds lower than 65x10-5 Pa-1.
Abstract:
A film made from or containing a polyolefin composition made from or containing: A) from about 19 wt % to about 50 wt %, based upon the total weight of the polyolefin composition, of a propylene ethylene copolymer having an ethylene derived units content ranging from about 1.5 wt % to about 6.0 wt %, based upon the total weight of the propylene ethylene copolymer; and B) from about 50 wt % to about 81 wt %, based upon the total weight of the polyolefin composition, of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from about 1.5 wt % to about 6.0 wt %, based upon the total weight of the propylene ethylene 1-butene terpolymer, and 1-butene derived units content of between about 4.8 wt % and about 12.4 wt %, based upon the total weight of the propylene ethylene 1-butene terpolymer; the sum of the amount of component A) and B) being 100.