公开(公告)号:ES2120638T3
公开(公告)日:1998-11-01
申请号:ES95100237
申请日:1995-01-10
Applicant: BASF AG
Inventor: TATZEL HERMANN , HAARDT UDO , DOMAS FRIEDRICH
-
公开(公告)号:AT164345T
公开(公告)日:1998-04-15
申请号:AT91122249
申请日:1991-12-27
Applicant: BASF AG
Inventor: HAARDT UDO , SEILER ERHARD , TATZEL HERMANN , SCHWAGER HARALD , DOMAS FRIEDRICH
Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …
-
53.
公开(公告)号:DE19702995A1
公开(公告)日:1997-09-04
申请号:DE19702995
申请日:1997-01-28
Applicant: BASF AG
Inventor: KRUECKAU FRITZ ERNST , HAARDT UDO , LENZ WERNER
IPC: B32B5/32 , B60K37/00 , B60N2/42 , B60N2/427 , B60N2/48 , B60R19/22 , B60R21/04 , B62D21/15 , F16F1/37 , C08J9/16 , C08L23/12 , C08L25/06
Abstract: In an energy-absorbing moulding, which consists of 2 foam layers, A and B, arranged behind one another in the direction of application of stress, layer A is a polypropylene foam with a density of 20-120 g/dm and layer B is a polystyrene foam with a density of 20-60 g/dm .
-
公开(公告)号:DE59305792D1
公开(公告)日:1997-04-17
申请号:DE59305792
申请日:1993-06-24
Applicant: BASF AG
Inventor: TATZEL HERMANN , HAARDT UDO
-
公开(公告)号:AT141310T
公开(公告)日:1996-08-15
申请号:AT91120866
申请日:1991-12-05
Applicant: BASF AG
Inventor: HAARDT UDO , TATZEL HERMANN
IPC: B29C44/00 , B29C44/04 , B29C44/44 , B29C67/02 , B29C67/20 , B29K23/00 , B29K105/04 , B32B5/32 , C08J9/232 , C08J9/24 , C08J9/33 , C08J9/34 , F16H25/06 , C08L23/10
Abstract: Mouldings made from polyolefin particle foams having a mean density of from 0.015 to 0.100 g/cm and containing at least two different regions whose densities differ by from 0.005 to 0.030 g/cm , where the transition zone between the different density regions has a thickness of not more than 25 mm.
-
公开(公告)号:MX9303892A
公开(公告)日:1994-04-29
申请号:MX9303892
申请日:1993-06-28
Applicant: BASF AG
Inventor: TATZEL HERMANN , HAARDT UDO
-
公开(公告)号:AU645388B2
公开(公告)日:1994-01-13
申请号:AU1038792
申请日:1992-01-22
Applicant: BASF AG
Inventor: HAARDT UDO , SEILER ERHARD , TATZEL HERMANN , SCHWAGER HARALD , DOMAS FRIEDRICH
Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …
-
公开(公告)号:DE4101806A1
公开(公告)日:1992-07-30
申请号:DE4101806
申请日:1991-01-23
Applicant: BASF AG
Inventor: HAARDT UDO , SEILER ERHARD , TATZEL HERMANN , SCHWAGER HARALD , DOMAS FRIEDRICH
Abstract: Shock-absorbing propylene polymer composite moulded articles containing …… a. a layer of thickness 0.5 to 10 mm, containing a propylene polymer of melting point 130 to 165 DEG C, … b. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … c. a foam layer of thickness 3 to 200 mm having a density of 0.015 to 0.1 g/cm based on a propylene copolymer of melting point 125 to 155 DEG C, … d. an intermediate layer of thickness 0.05 to 0.5 mm of a melt adhesive based on an olefin copolymer of melting point 90 to 140 DEG C, … e. a layer of thickness 0.5 to 10 mm containing a propylene polymer of melting point 130 to 165 DEG C. …
-
公开(公告)号:NO920295A
公开(公告)日:1992-07-24
申请号:NO920295
申请日:1992-01-22
Applicant: BASF AG
Inventor: HAARDT UDO , SEILER ERHARD , TATZEL HERMANN , SCHWAGER HARALD , DOMAS FRIEDRICH
CPC classification number: B32B5/18 , B32B5/20 , B32B7/12 , B32B27/065 , B32B27/32 , B32B2266/025 , B32B2307/56 , B32B2323/10 , Y10T428/24967 , Y10T428/249981 , Y10T428/249986 , Y10T428/249988 , Y10T428/249992 , Y10T428/249993
-
公开(公告)号:DE4040908A1
公开(公告)日:1992-06-25
申请号:DE4040908
申请日:1990-12-20
Applicant: BASF AG
Inventor: HAARDT UDO , TATZEL HERMANN
IPC: B29C44/00 , B29C44/04 , B29C44/44 , B29C67/02 , B29C67/20 , B29K23/00 , B29K105/04 , B32B5/32 , C08J9/232 , C08J9/24 , C08J9/33 , C08J9/34 , F16H25/06
Abstract: Mouldings made from polyolefin particle foams having a mean density of from 0.015 to 0.100 g/cm and containing at least two different regions whose densities differ by from 0.005 to 0.030 g/cm , where the transition zone between the different density regions has a thickness of not more than 25 mm.
-
-
-
-
-
-
-
-
-