Abstract:
The invention relates to the use of a mineral having perovskite structure in vinyl aromatic polymer foam, i) for decreasing the thermal conductivity, ii) for increasing the mechanical properties (namely compressive strength and bending strength), or iii) for improving the self-extinguishing properties of the foam. The polymer foam further comprises one or more athermanous additives selected from a) powder inorganic additive selected from powders of silica and calcium phosphate, b) powder carbonaceous additive selected from powders of graphite, carbon black, petroleum coke, graphitized carbon black, graphite oxides, and graphene, and c) powder geopolymer and powder geopolymer composite.
Abstract:
Die Erfindung betrifft ein Verfahren zur Herstellung eines mehrschichtigen Formkörpers zur Wärmedämmung von Gebäuden, bei dem schäumbare oder vorgeschäumte Polymer-Partikel zur Ausbildung einer Schicht verwendet werden. Erfindungsgemäß werden die schäumbaren oder vorgeschäumten Polymer-Partikel zumindest teilweise mit einem organischen Bindemittel beschichtet und in einer Form zur Durchführung eines Endschäumprozesses mit wenigstens einer Platte aus expandiertem oder extrudiertem Polystyrol-Hartschaum verbunden. Des Weiteren betrifft die Erfindung einen mehrschichtigen Formkörper zur Wärmedämmung von Gebäuden.
Abstract:
Die Erfindung betrifft ein Verfahren zur Herstellung von expandierten Schaumstoffpartikeln aus einem Granulat, enthaltend eine Polyestermischung zusammengesetzt aus: • a) 50 bis 99 Gew.-%, bezogen auf die Komponenten a und b, eines biologisch abbaubaren Polyesters auf Basis von aliphatischen oder aliphatischen und aromatischen Dicarbonsäuren und aliphatischen Diolen, und • b) 1 bis 50 Gew.-%, bezogen auf die Komponenten a und b, Polymilchsäure, umfassend die folgenden Schritte: • (i) Herstellen einer Suspension enthaltend ein Granulat der Polyestermischung in einem Suspendiermedium, • (ii) Imprägnieren des in der Suspension aus Schritt (i) enthaltenen Granulates mit mindestens einem physikalischen oder chemischen Treibmittel, um ein mit Treibmittel beladenes Granulat in Suspension zu erhalten, indem die Mischung unter Rühren bis zur Entspannungstemperatur IMT aufgeheizt wird und • (ii) Entspannen der in Schritt (ii) erhaltenen Suspension nach Ablauf einer Haltezeit, um expandierte Schaumstoffpartikel zu erhalten, dadurch gekennzeichnet, dass in einem wässrigen Suspendiermedium gefahren wird, das Treibmittel in Schritt (i) oder in Schritt (ii) während der Aufheizphase oder unmittelbar nach der Aufheizphase zugegeben wird und in Schritt (ii) die Suspension nach dem Aufheizen während 3 bis 100 Minuten bei einer Temperatur im Bereich von IMT minus 5°C bis IMT plus 2°C gehalten wird. Weiterhin betrifft die Erfindung expandierte Schaumstoffpartikel erhältlich nach diesem Verfahren sowie die Herstellung von Formteilen aus diesen Schaumstoffpartikeln.
Abstract:
The present invention relates to a molding made of expanded bead foam, wherein at least one fiber (F) is partly within the molding, i.e. is surrounded by the expanded bead foam. The two ends of the respective fibers (F) that are not surrounded by the expanded bead foam thus each project from one side of the corresponding molding. The present invention further provides a panel comprising at least one such molding and at least one further layer (S1). The present invention further provides processes for producing the moldings of the invention from expanded bead foam or the panels of the invention and for the use thereof, for example as rotor blade in wind turbines.
Abstract:
Composite resin particles including: a polyethylene-based resin and a polystyrene-based resin, wherein the polyethylene-based resin and the polystyrene-based resin are included in the ranges of 50 to 20% by mass and 50 to 80% by mass respectively, with respect to the total of these resins, the polyethylene-based resin is composed of: a first polyethylene-based resin having a medium density to a high density in the range of 925 to 965 kg/m3; and a second polyethylene-based resin which is linear and which has a lower density than the first polyethylene-based resin, and the first polyethylene-based resin and the second polyethylene-based resin are included in the ranges of 90 to 30% by mass and 10 to 70% by mass respectively, with respect to the total of these resins.
Abstract translation:复合树脂颗粒包括:聚乙烯类树脂和聚苯乙烯类树脂,其中聚乙烯类树脂和聚苯乙烯类树脂的含量分别为50〜20质量%,50〜80质量% 相对于这些树脂的总和,聚乙烯类树脂由以下组成:中密度为925〜965kg / m 3的高密度的中等密度的第一聚乙烯类树脂; 和第二聚乙烯系树脂,其直链状且密度比第一聚乙烯系树脂低,第一聚乙烯系树脂和第二聚乙烯系树脂的含量为90〜30质量% 和相对于这些树脂的总量分别为10〜70质量%。
Abstract:
Polyethylene resin foamed particles having a storage elastic modulus of 900 Pa or more and 5000 Pa or less at an angular frequency of 1 rad/second, and the storage elastic modulus is 100000 Pa or less at an angular frequency of 100 rad/second. The storage elastic modulus is obtained in a dynamic viscoelasticity measurement of the a polyethylene resin particles at 190° C. The polyethylene resin foamed particles also have a DSC curve obtained from a differential scanning calorimetry (DSC) at a temperature rising speed of 10° C./minute within a range of 20° C. to 220° C. The DSC curve has two melting peaks of a melting peak on a low temperature side and a melting peak on a high temperature side.
Abstract:
A process for producing expanded foam beads from pellets comprising at least one biodegradable polyester. The process comprises (i) producing a suspension comprising pellets in an aqueous suspension medium, (ii) impregnating the pellets present in the suspension from step (i) with at least one physical blowing agent by heating the pellet suspension to a depressurization temperature IMT, with stirring, to provide pellets laden with blowing agent in the suspension medium, and (iii) depressurizing the suspension obtained in step (ii) and cooling the depressurized suspension with a liquid aqueous coolant, in order to obtain the expanded foam beads. The blowing agent can be added in step I, or in step ii during the heating phase or following the heating phase. Following the heating phase, the suspension is maintained at a temperature in the range from IMT minus 5° C. to IMT plus 2° C. for 3 to 100 minutes, and the ratio of aqueous coolant to suspension medium is at least 0.3. The invention further relates to expanded foam beads obtained by the process and to moldings that are produced from the expanded foam beads.
Abstract:
From electroconductive polypropylene resin foamed particles produced by foaming electroconductive polypropylene resin particles including an electroconductive polypropylene resin composition that contains 11 parts by weight or more and 25 parts by weight or less of an electroconductive carbon black relative to 100 parts by weight of a polypropylene resin and has a melt index of 1.0 g/10 min or more and 4.0 g/10 min or less where the melt index is determined at a load of 5,000 g at 230±0.2° C., a polypropylene resin in-mold foam molded article having excellent electric conductivity and also having higher flame retardancy without any flame retardant can be obtained.