폴리벤지이미다졸코벤족사졸 및 그 제조 방법
    70.
    发明公开
    폴리벤지이미다졸코벤족사졸 및 그 제조 방법 有权
    聚(苯并咪唑 - 苯并噻唑)及其制备方法

    公开(公告)号:KR1020130095565A

    公开(公告)日:2013-08-28

    申请号:KR1020120017115

    申请日:2012-02-20

    Abstract: PURPOSE: A polyelectrolyte material is provided to have a high proton conductivity and an excellent mechanical strength even though the material is manufactured by being doped with phosphoric acid in-situ. CONSTITUTION: Polyelectrolyte includes poly(benzimidazole-co-benzoxazole). The content of polybenzoxazle in poly(benzimidazole-co-benzoxazole) is 5-30 mole%. Poly(benzimidazole-co-benzoxazole) is poly(benzimidazole-co-benzoxazole) represented by Chemical formula 1 or 2. In Chemical formulas 1 and 2, A is 80-90, and B is 20-10. A manufacturing method of the polyelectrolyte comprises a step of providing poly(benzimidazole-co-benzoxazole) by introducing a benzoxazole unit to polybenzimidazole.

    Abstract translation: 目的:提供聚电解质材料以具有高质子传导性和优异的机械强度,即使该材料是通过原位掺磷酸制造的。 构成:聚电解质包括聚(苯并咪唑 - 共 - 苯并恶唑)。 聚(苯并咪唑 - 共 - 苯并恶唑)中聚苯并恶唑的含量为5-30%(摩尔)。 聚(苯并咪唑 - 共 - 苯并恶唑)是由化学式1或2表示的聚(苯并咪唑 - 共 - 苯并恶唑)。在化学式1和2中,A为80-90,B为20-10。 聚电解质的制造方法包括通过将苯并恶唑单元引入聚苯并咪唑来提供聚(苯并咪唑 - 共 - 苯并恶唑)的步骤。

Patent Agency Ranking