公开(公告)号:AU2008341066A1
公开(公告)日:2009-07-02
申请号:AU2008341066
申请日:2008-02-26
Applicant: ATI PROPERTIES INC
Inventor: STINNER CHARLES P , RAKOWSKI JAMES M , GRUBB JOHN F , BERGSTROM DAVID S , DUNN JOHN J
Abstract: An austenitic stainless steel composition having low nickel and molybdenum and exhibiting high corrosion resistance and good formability. The austenitic stainless steel includes, in weight %, up to 0.20 C, 2.0-6.0 Mn, up to 2.0 Si, 16.0-23.0 Cr, 5.0-7.0 Ni, up to 3.0 Mo, up to 3.0 Cu, 0.1-0.35 N, up to 4.0 W, up to 0.01 B, up to 1.0 Co, iron and impurities. The austenitic stainless steel has a ferrite number less than 11 and an MD30 value less than −10° C.
-
公开(公告)号:AU2008341063A1
公开(公告)日:2009-07-02
申请号:AU2008341063
申请日:2008-02-20
Applicant: ATI PROPERTIES INC
Inventor: BERGSTROM DAVID S , GRUBB JOHN F , STINNER CHARLES P , RAKOWSKI JAMES M , DUNN JOHN J
-
公开(公告)号:HK1063823A1
公开(公告)日:2005-01-14
申请号:HK04106552
申请日:2004-08-31
Applicant: ATI PROPERTIES INC
Inventor: GRUBB JOHN F , FRITZ JAMES D
IPC: C22B9/16 , C21D20090101 , C21D1/09 , C21D1/26 , C21D1/34 , C21D6/00 , C21D8/00 , C22B9/18 , C22B9/20 , C22B9/22 , C22C20090101 , C22C38/00 , C22C38/44 , C22C38/58 , F28F21/08
Abstract: A method for producing a stainless steel with improved corrosion resistance includes homogenizing at least a portion of an article of a stainless steel including chromium, nickel, and molybdenum and having a PREN of at least 50, as calculated by the equation:where Cr is weight percent chromium, Mo is weight percent molybdenum, and N is weight percent nitrogen in the steel. In one form of the method, at least a portion of the article is remelted to homogenize the portion. In another form of the method, the article is annealed under conditions sufficient to homogenize at least a surface region of the article. The method of the invention enhances corrosion resistance of the stainless steel as reflected by the steel's critical crevice corrosion temperature.
-
公开(公告)号:BR0213263A
公开(公告)日:2004-10-26
申请号:BR0213263
申请日:2002-03-20
Applicant: ATI PROPERTIES INC
Inventor: BERGSTROM DAVID S , DUNN JOHN J , GRUBB JOHN F , PRATT WILLIAM A
Abstract: A duplex stainless steel including, in weight percent, up to 0.06 percent carbon, 15 up to less than 25 percent chromium, greater than 3 up to 6 percent nickel, up to 3.75 percent manganese, 0.14 up to 0.35 percent nitrogen, up to 2 percent silicon, greater than 1.4 up to less than 2.5 percent molybdenum, up to less than 0.5 percent copper, up to less than 0.2 percent cobalt, up to 0.05 percent phosphorous, up to 0.005 percent sulfur, and 0.001 up to 0.0035 percent boron, with the remainder being iron and incidental impurities is disclosed. The duplex stainless steel may be included in an article of manufacture, such as a strip, bar, plate, sheet, casting, tubing or piping. A method for making such a duplex stainless steel is also disclosed.
-
公开(公告)号:NO20034714L
公开(公告)日:2003-12-22
申请号:NO20034714
申请日:2003-10-21
Applicant: ATI PROPERTIES INC
Inventor: GRUBB JOHN F , FRITZ JAMES D
IPC: C22B9/16 , C21D1/09 , C21D1/26 , C21D1/34 , C21D6/00 , C21D8/00 , C22B9/18 , C22B9/20 , C22B9/22 , C22C38/00 , C22C38/44 , C22C38/58 , F28F21/08
Abstract: A method for producing a stainless steel with improved corrosion resistance includes homogenizing at least a portion of an article of a stainless steel including chromium, nickel, and molybdenum and having a PREN of at least 50, as calculated by the equation:where Cr is weight percent chromium, Mo is weight percent molybdenum, and N is weight percent nitrogen in the steel. In one form of the method, at least a portion of the article is remelted to homogenize the portion. In another form of the method, the article is annealed under conditions sufficient to homogenize at least a surface region of the article. The method of the invention enhances corrosion resistance of the stainless steel as reflected by the steel's critical crevice corrosion temperature.
-
公开(公告)号:AU765419B2
公开(公告)日:2003-09-18
申请号:AU2179100
申请日:1999-12-13
Applicant: ATI PROPERTIES INC
Inventor: SORACE DOMINIC A , GRUBB JOHN F
Abstract: An alloy having a composition, by weight, of about 0.025% or less carbon, about 0.5 to about 4.1% manganese, about 5.5 to about 6.2% silicon, about 11 to about 15% chromium, about 9.0 to about 15.5% nickel, about 0.8 to about 1.2% molybdenum and about 0.8 to about 2% copper and the remainder being essentially iron with incidental impurities. This composition results in lean alloy content in a high silicon austenitic stainless steel for concentrated sulfuric acid service while maintaining a corrosion rate similar to and competitive with existing alloys for such service. Acceptable characteristics were found when hot working was carried out in the range of about 2100 DEG F. to about 2200 DEG F. Annealing in the range of about 1925 DEG F. to about 2025 DEG F. is preferred, as is rapid water quenching after annealing.
-
公开(公告)号:ZA200209034B
公开(公告)日:2003-08-28
申请号:ZA200209034
申请日:2002-11-06
Applicant: ATI PROPERTIES INC
Inventor: GRUBB JOHN F , POLINSKI RONALD E , FRITZ JAMES D
Abstract: A method of enhancing the corrosion resistance of an austenitic steel includes removing material from at least a portion of a surface of the steel such that corrosion initiation sites are eliminated or are reduced in number relative to the number resulting from processing in a conventional manner. Material may be removed from the portion by any suitable method, including, for example, grit blasting, grinding and/or acid pickling under conditions more aggressive than those used in conventional processing of the same steel.
-
公开(公告)号:CA2443545A1
公开(公告)日:2002-10-31
申请号:CA2443545
申请日:2002-04-18
Applicant: ATI PROPERTIES INC
Inventor: FRITZ JAMES D , GRUBB JOHN F
IPC: C22B9/16 , C21D1/09 , C21D1/26 , C21D1/34 , C21D6/00 , C21D8/00 , C22B9/18 , C22B9/20 , C22B9/22 , C22C38/00 , C22C38/44 , C22C38/58 , F28F21/08 , C22C28/00 , C21D9/00 , C22C19/05
Abstract: A method for producing a stainless steel with improved corrosion resistance includes homogenizing at least a portion of an article of a stainless steel including chromium, nickel, and molybdenum and having a PREN of at least 50, as calculated by the equation: PREN = Cr + (3.3 x Mo) + (30 x N), where Cr i s weight percent chromium, Mo is weight percent molybdenum, and N is weight percent nitrogen in the steel. In one form of the method, at least a portion of the article is remelted to homogenize the portion. In another form of the method, the article is annealed under conditions sufficient to homogenize at least a surface region of the article. The method of the invention enhances corrosion resistance of the stainless steel as reflected by the steel's critical crevice corrosion temperature.
-
公开(公告)号:DK2280089T3
公开(公告)日:2016-11-07
申请号:DK10075573
申请日:2002-03-01
Applicant: ATI PROPERTIES INC
Inventor: BERGSTROM DAVID S , DUNN JOHN J , GRUBB JOHN F , PRATT WILLIAM A
-
公开(公告)号:CA2706478C
公开(公告)日:2016-08-16
申请号:CA2706478
申请日:2008-02-26
Applicant: ATI PROPERTIES INC
Inventor: BERGSTROM DAVID S , RAKOWSKI JAMES M , STINNER CHARLES P , DUNN JOHN J , GRUBB JOHN F
Abstract: An austenitic stainless steel composition having low nickel and molybdenum and exhibiting high corrosion resis-tance and good formability. The austenitic stainless steel includes, in weight %, up to 0.20 C, 2.0-6.0 Mn, up to 2.0 Si, 16.0-23.0 Cr, 5.0-7.0 Ni, up to 3.0 Mo, up to 3.0 Cu, 0.1-0.35 N, up to 4.0 W, up to 0.01 B, up to 1.0 Co, iron and impurities. The austenitic stainless steel has a ferrite number less than 11 and an MD30 value less than -10°C.
-
-
-
-
-
-
-
-
-