HOT ROLLING METHOD FOR STAINLESS STEEL STRIP

    公开(公告)号:JPS63119909A

    公开(公告)日:1988-05-24

    申请号:JP26536086

    申请日:1986-11-07

    Abstract: PURPOSE:To stably manufacture a stainless steel strip having good surface quality by hot rolling a stock by supplying a dispersion liquid, whose friction coefficient is adjusted by addition of iron oxide, etc., onto the surface of a rolling roll in a position corresponding to the strip edge rolling part. CONSTITUTION:At the time of hot rolling a stainless steel strip, a dispersion liquid whose friction coefficient is adjusted to be 0.2-0.4 by addition of >=1vol% of >=1 kind of iron oxide, silica, and alumina is supplied onto the surface of a rolling roll in a position corresponding to the strip edge at least. In that situation, continuous rolling does not cause insufficient biting or slips and stainless steel stips having the good surface quality are stably manufactured without generation of seizing flaws.

    COLD ROLLING METHOD OF THIN STEEL STRIP

    公开(公告)号:JPS60223601A

    公开(公告)日:1985-11-08

    申请号:JP7926784

    申请日:1984-04-19

    Abstract: PURPOSE:To prevent slip between rolls during accelerated and decelerated rolling and to enable the rolling mill to make stationary rolling at a high speed and high draft by controlling the supply rate of a rolling mill lubricant so as to increase or decrease said rate according to the rolling speed. CONSTITUTION:The rolling speed is detected by a tachometer 3 connected to a roll driving motor 2 of a rolling mill 1 of a backup roll driving system. The supply rate of the rolling mill lubricant discharged from a feed pump 5 for the rolling mill lubricant is controlled by a speed control device 4 of the pump 5 and the rolling mill lubricant is injected to the mill 1 and a strip 9 from nozzles 8. The strip is thus rolled without generation of a slip owing to the excessive lubrication during accelerated and decelerated rolling and a heat scratch owing to the deficient lubrication in the stationary rolling stage at a high speed.

    COLD HEADING OIL FOR STEEL
    65.
    发明专利

    公开(公告)号:JPS5980498A

    公开(公告)日:1984-05-09

    申请号:JP18998082

    申请日:1982-10-30

    Abstract: PURPOSE:A cold heading oil for steel useful as a cold heading oil of high-speed mill grease, etc., having improved lubricating properties and annealing properties, containing a specific mixed monoester. CONSTITUTION:(A) 32-64C (mixed) monoester consisting of 16-20C fatty acid and a monohydric fatty alcohol is blended with (B) 32-64 (mixed) monoester (with the proviso that the difference of carbon number of the ester and the fatty acid is

    PRODUCTION OF CLEANED STEEL SHEET
    66.
    发明专利

    公开(公告)号:JPS56169781A

    公开(公告)日:1981-12-26

    申请号:JP7349480

    申请日:1980-05-31

    Abstract: PURPOSE:To enhance the cleaning effect of hot water, to apply an evaporation promotor, and to lower its consumption amount, by mixing a rolling oil-evaporation promotor into hot water to be injected under a pressure onto a thin steel sheet near the final rolling stand of a continuous cold rolling mill. CONSTITUTION:The thin steel sheet 2 is rolled by a five-stand tandem mill, for instance, using a rolling oil composed of mineral oil and about 20% beef tallow in its first to fourth stands. Between the fourth and fifth stands, washing water 3 kept at a temperature of about 50 deg.C under a pressure of about 100kg/cm and containing an evaporation promotor (a special high molecular compound: polyisobutylene having a molecular weight of 10,000) is injected onto the steel sheet 2, to diminish the rolling oil and iron powder adhered onto the steel sheet 2 and to apply the evaporation promotor onto the steel sheet 2. Thereafter, the steel sheet 2 is carried to an annealing step. In this case, the running speed of the sheet 2 at the fifth stand is about 1,000m/min, the residual adhesion amount of the rolling oil between the fourth and fifth stands after washed is about 25mg/m , and the apply amount of the evaporation promotor at the fifth stand is about 15mg/m .

    PRODUCTION OF COLD ROLLED STEEL PLATE HAVING CLEAN SURFACE

    公开(公告)号:JPS55148720A

    公开(公告)日:1980-11-19

    申请号:JP3906479

    申请日:1979-03-31

    Abstract: PURPOSE:To enable annealing without undergoing cleaning and provide the clean surfaces free from carbon stains by coating the material which exhibits a minimum azeotropic phenomenon with the rolling oil deposited on steel plate surfaces and annealing the steel plate. CONSTITUTION:The material which exhibits a minimum azerotropic phenomenon with the high-lubricity rolling oil deposited on the surfaces of the steel plate after cold rolling is coated by a ameans such as spray coating provided within the rolling line or in an other simple line and the steel plate is annealed in that state. An azeotropic phenomenon occurs with the high-lubricity rolling oil and coated material in the high-temperature atmosphere during annealing, by which the remaining of the rolling oil on the steel plate surfaces is prevented and the cold rolled steel plate having clean surfaces is obtained. The coating material is at least one kind of hydrocabons, alcohols, ketones, amines, and esters of fatty acids or dibasic acids.

    LUBRICANT FOR PLASTIC WORKING OF STEEL

    公开(公告)号:JPS55145796A

    公开(公告)日:1980-11-13

    申请号:JP5312979

    申请日:1979-04-28

    Abstract: PURPOSE:To provide a lubricant for plastic working of steel which excels in seizing resistance and has good heat resistance and friction coefficient, contg. a specified synthetic ester. CONSTITUTION:There is provided a lubricant for plastic working of steel contg. at least one ester selected from esters of formulae I, II and III (wherein R1 is 5-36C alkyl; R2 is 1-36C alkyl, H; l is an integer 1-5; n, m are an integer 1-25). As compared with beef tallow which exhibits the highest performance among conventional lubricants, the above lubricant excels in seizing resistance and the performance in the heat resistance and friction coefficient are superior or comparable to beef tallow.

    METHOD OF EVALUATION OF COLD MILLING OIL

    公开(公告)号:JPS5573788A

    公开(公告)日:1980-06-03

    申请号:JP14753878

    申请日:1978-11-29

    Abstract: PURPOSE:The ingredient of milling oil is examined on specified tests and the results are compared with the calclutation values derived from experimental equations to evaluate correctly the milling oil suitable for cold rolling, thus preventing the heat scartch and increasing the productivity of rolling. CONSTITUTION:The ingredient of milling oil before made into emulsion or obtained by extracting the emulsion is subjected to Bouden test to derive the sliding number until galling occurs n from the relationship between the sliding number and the friction coefficient. Then, the sliding number in is compared with the value derived from the experimental equation satisfying the desired rolling conditions and judged if the oil is suitable as the milling oil.