음극용 리드탭 및 그 제조방법
    1.
    发明公开
    음극용 리드탭 및 그 제조방법 无效
    用于阳极的导板及其制造方法

    公开(公告)号:KR1020090114126A

    公开(公告)日:2009-11-03

    申请号:KR1020080039913

    申请日:2008-04-29

    CPC classification number: H01M10/0404 H01M2/30 H01M2220/30 Y02E60/122

    Abstract: PURPOSE: A method for manufacturing a lead-tab for an anode is provided to prepare a lead-tab for an anode of a secondary battery by a simple process at inexpensive costs, thereby lowering production cost of lithium ions or a lithium polymer secondary battery. CONSTITUTION: A method for manufacturing a lead-tab for an anode comprises a preparation step of preparing a copper plate as a raw material of a current collector; a plating step of plating a copper plate with nickel; a rolling step of rolling nickel-plated copper plate; and a heat treatment step of heating the rolled nickel-plated copper plate. The heat treatment temperature is 300~500 °C.

    Abstract translation: 目的:提供一种用于制造用于阳极的引线片的方法,以便以廉价的成本通过简单的工艺制备二次电池的阳极的引线片,从而降低了锂离子或锂聚合物二次电池的生产成本。 构成:用于制造阳极用引线片的方法包括:制备作为集电体的原料的铜板的制备工序; 镀镍步骤,镀镍铜板; 轧制镀镍铜板的轧制步骤; 以及对轧制的镀镍铜板进行加热的热处理工序。 热处理温度为300〜500℃。

Patent Agency Ranking