Abstract:
본 발명은 전기저항을 이용한 복합재료의 미세손상 감지방법에 관한 것으로서, 전도성 강화재가 포함된 복합재료에 사각 패턴화된 다수의 접점들을 설정하는 제1단계, 상기 설정된 접점들이 형성하는 구간의 전기저항 변화율을 측정하는 제2단계 및 상기 측정된 전기저항 변화율로부터 복합재료의 미세손상을 감지하는 제3단계를 포함함으로써, 고가의 장비 없이 간편하게 복합재료의 미세손상 발생 유무뿐만 아니라 전기저항 변화율의 크기에 따라 미세손상의 크기도 판별할 수 있는 장점이 있는 전기저항을 이용한 복합재료의 미세손상 감지방법에 관한 것이다.
Abstract:
PURPOSE: A manufacturing method of reinforced phenol composite using a strengthening plastic chip and a recycling method of carbon fiber reinforced plastic are provided to use discharged chips which are generated during manufacturing a carbon fiber strengthening hole for offering thermal resistance and offer an environment-friendly recycling method of carbon fiber reinforced plastic. CONSTITUTION: A manufacturing method of carbon fiber reinforced plastic comprises the following steps. Carbon fiber reinforced plastic (CFRP) is pulverized. The pulverized plastic is washed by weak acid solution of which pH is from 6.2 to 6.5. The plastic washed by the weak acid is dipped in a solution with C1-4 alcohol or acetone and treated with ultrasonic wave. A mortar is used for pulverizing. The carbon fiber reinforced plastic is a discharged chip which is made during manufacturing a carbon fiber reinforced plastic hole.
Abstract:
PURPOSE: A manufacturing method of a CNT/PP composite material is provided to improve mechanical properties of the composite material, and to obtain the excellent CNT/PP composite material with excellent dispersity. CONSTITUTION: A manufacturing method of a CNT/PP composite material comprises a step of manufacturing a PP powder/xylene mixture; a step of stirring the mixture at 100-150 deg. C for 1-3 hours; a step of manufacturing a CNT/xylene dispersion solution by mixing a carbon nanotubes(CNT) and xylene; a step of injecting swollen the CNT/xylene dispersed solution into the swollen PP powder/xylene mixture; a step of ultra-wave dispersing the result; and a step of removing solvent, deaerating the solvent, and manufacturing final CNT/PP powder.
Abstract:
본 발명은 강화 페놀 복합재료 및 이의 제조방법에 관한 것으로, 더욱 상세하게는 탄소섬유 강화 플라스틱(CFRP)을 분쇄하는 단계, 상기 분쇄된 탄소섬유 강화 플라스틱을 pH 6.2 내지 pH 6.5의 약산 용액으로 세척하는 단계, 및 상기 약산 용액으로 세척된 탄소섬유 강화 플라스틱을 페놀 수지가 침지된 C 1-4 알코올 용액 또는 아세톤에 첨가한 후 초음파 처리하는 단계를 포함하는 강화페놀복합재료의 제조방법에 관한 것이다. 이에 따라, 상기 제조방법으로 제조된 강화 페놀 복합재료를 제공하고, 탄소섬유 강화 플라스틱의 재활용 방법 등에 활용한다.