Abstract:
The present invention to a functional reinforcing agent for repairing stone cultural heritage which is exfoliated due to natural weathering or an artificial reason. An alkoxysilane based functional reinforcing agent including pre-treatment for preserving stone cultural heritage has a feature of comprising: an alkoxysilane based pre-treating agent which has reactor to react with epoxy group; a functional filler which has epoxy group and is applied on the upper side of the alkoxysilane based pre-treating agent; an alkoxysilane based reinforcing agent which comprises by including alkoxysilane based resin which has epoxy group. Additionally, the present invention has an effect of increasing an interaction between the stone and the functional reinforcing agent; preventing a second damage of the stone which is caused by insufficient interaction between the functional reinforcing agent and the stone and friable property of alkoxysilane based reinforcing agent by treating with the alkoxysilane based reinforcing agent after treating with alkoxysilane based pre-treating agent which has reactive group to stone to increase reinforcing effect, after mixing the functional additive which has an epoxy group which is a reactive group in the alkoxysilane which is a main component of the alkoxysilane based reinforcing agent. The present invention has an effect to of preventing a big damage of stone heritage in which a part of weathered stone is destroyed in case the reinforcing part is destroyed by using a nano cluster filler which has a reactivity and granting a high mechanical stability of the alkoxysilane based reinforcing agent thereby having a less interaction between alkoxysilane based reinforcing agent and stone. [Reference numerals] (AA) An embodiment 11 solution; (BB) A comparative example Wacker OH 100
Abstract:
본 발명은 석조문화재 보존용 에폭시 접착제 조성물 및 이를 이용한 접착제에 관한 것으로, 더욱 상세하게는 석조문화재를 보존하기 위해 적용되는 에폭시 수지에 무기물 첨가제를 적용함으로써 열팽창 계수를 최소화시켜 석조문화재를 보존처리 후 에폭시 수지에서 석재에 가해지는 응력을 최소화할 수 있는 석조문화재 보존용 에폭시 접착제 조성물 및 이를 이용한 접착제에 관한 것이다.
Abstract:
The present invention relates to an epoxy resin adhesive used for combining, filling, or restoring stone materials and, more specifically, to an epoxy resin adhesive which contains a mixed hardener in a constant composition ratio, obtained by mixing a rapid hardener rapidly proceeding hardening to a predetermined viscosity and a low speed hardener slowly proceeding hardening to a predetermined viscosity. The epoxy resin adhesive can include a reactive diluent for minutely adjusting the viscosity of the epoxy resin adhesive, and an inorganic additive formed of materials similar to the stone materials of stone cultural heritages. An effect for properly controlling the working time of a worker to preserve and restore various stone cultural heritages is obtained by mixing the rapid hardener and the low speed hardener to obtain a hardener controlling a viscosity by hardening and hardening speed of an epoxy resin, and using the hardener with the epoxy resin which is a main material. An effect for perfectly restoring and preserving stone cultural heritages is obtained by reducing the initial viscosity of the epoxy resin adhesive which contains the main material and the hardener to add the inorganic additive.
Abstract:
The present invention relates to a calculation method of chemical deterioration probability for stone cultural heritage and, more specifically, to a calculation method of the chemical deterioration probability for a stone cultural heritage for obtaining the probability frequency function of normal granite using chemical index of alteration (CIA); for obtaining chemical surface deterioration probability (DP-CIA) using the obtained probability frequency function; for confirming the deterioration condition and current condition of the stone cultural heritage; and for calculating the chemical deterioration probability. In addition, the present invention obtains effects for obtaining reference materials for maintaining the stone cultural heritage and for obtaining a calculation method for calculating the physical deterioration of the stone cultural heritage through the chemical aeration. The calculation method of the chemical deterioration possibility for the stone cultural heritage according to the present invention can calculate the chemical deterioration possibility of stone utilized in the geology and the stone cultrual heritage.
Abstract:
PURPOSE: A consolidant feeding apparatus for conservation of stone cultural properties and stone and a conservation treatment method of stone cultural properties and stone using the same are provided to effectively suppress reaction between moisture in the air and a consolidant for conservation of stone cultural properties and to treat the stone cultural properties through dipping that is more effective than coating. CONSTITUTION: A consolidant feeding apparatus comprises a consolidant storage unit (10) including a consolidant storage tank (11), a consolidant inlet port (12), a dehumidifying air inflow part (13), and a consolidant outlet port; a dehumidifying air supply unit (20) including a dehumidifying agent filling unit (21) to be filled with a dehumidifying agent; an air inflow unit (22) to supply air to the dehumidifying agent filling unit, and a dehumidifying air discharge unit; and a consolidant discharge unit (30) including a flow meter (31) to control flow of a consolidant that is discharged from the reinforcing outlet port of the consolidant storage unit; a valve (32) to control discharge of the consolidant of which flow is controlled by the flow meter, and a consolidant discharge unit to feed the consolidant that is discharged through the valve on a portion of a stone cultural property to be treated.
Abstract:
본 발명은 석조문화재의 생물학적 풍화정도를 정량적으로 산출하여 석조문화재의 훼손상태를 평가하고, 훼손상태에 따른 보존처리 방안을 확립할 수 있도록 하는 석조문화재의 생물오염지수 산정방법에 관한 것으로서, 보다 상세하게는, 석조문화재가 위치한 장소의 환경요인을 측정ㆍ분석하여 환경요인에 따른 풍화등급을 산출하고, 석조문화재의 표면에 자생하는 생물을 채취하여 채집된 생물에 의한 석조문화재의 생물오염피복율에 따른 풍화등급을 산출하며, 석조문화재의 표면에 자생하는 생물의 생물량 농도에 따른 풍화등급을 산출하여 석조문화재의 생물오염지수를 산정하는 방법에 관한 것이다. 또한 본 발명은 석조문화재의 정량적인 생물오염지수(생물풍화등급)을 산정이 가능하도록 하는 효과를 얻을 수 있고; 계절조사를 통해 계절의 영향을 최소화하여, 계절에 관계없이 안정적인 평가 결과를 도출할 수 있는 효과를 얻을 수 있으며; 종래의 분석에 어려움이 있던 조류오염지수가 생물오염지수 산정에 실제 포함되지 않아, 지수의 적용성을 높여 비전문가도 쉽게 사용할 수 있는 효과를 얻을 수 있다.
Abstract:
본 발명은 암석의 표면을 파괴하지 아니하고, 암석의 풍화도지수를 산출하기 위한 표면 반발 경도계를 이용한 암석의 풍화도지수 산출방법에 관한 것으로서, 표면 반발 경도계와 초음파 측정장비를 이용하여 공시암석의 표면경도값과 초음파속도값을 각각 측정하고, 측정된 표면경도값과 초음파속도값 간의 상관관계를 산출하여, 일반적으로 인정된 풍화도지수와 초음파 측정장비를 통하여 측정된 초음파속도값 간의 상관관계를 풍화도지수와 표면경도값으로 적용가능하여, 암석의 파괴 없이 해당 암석(측정암석)의 풍화도지수를 정량적으로 산출할 수 있도록 하는 표면 반발 경도계를 이용한 암석의 풍화도지수 산출방법에 관한 것이다. 또한 본 발명은 초음파를 이용한 암석의 풍화도 산출 이외에, 표면 반발 경도계를 활용한 석조문화재용 비파괴 진단방법 및 데이터의 신뢰도를 확보가능하고, 암석의 암종과 무관하고 암석의 풍화상태에 맞는 풍화도지수를 암석의 표면 파괴없이 제공가능한 효과를 얻을 수 있으며, 암석의 표면 파괴없이 산출된 풍화도지수를 이용하여 석조문화재와 같은 문화유산을 풍화도에 따라 다양하게 적용하여 보존관리할 수 있는 효과를 얻을 수 있다.
Abstract:
본 발명은 석재의 접합, 충진 또는 복원에 이용되는 에폭시 수지 접착제에 관한 것으로서, 보다 상세하면, 주제인 에폭시 수지에 대하여, 일정의 점도까지 경화속도를 빠르게 진행시키는 속경화제와 일정의 점도까지 경화속도를 천천히 진행시키는 저속경화제를 일정의 비율로 혼합한 혼합 경화제가 일정 조성비로 혼합되는 구성을 하는 에폭시 수지 접착제에 관한 것이고; 상기 구성의 에폭시 수지 접착제에 에폭시 수지 접착제의 미세한 점도 조절을 실현할 수 있도록 하는 반응성 희석제가 더 포함될 수 있고, 석조문화재의 석재와 유사한 소재로 구성되는 무기첨가제를 더 포함할 수 있는 에폭시 수지 접착제에 관한 것이다. 또한 본 발명은 에폭시 수지의 경화속도 및 경화에 따른 점도를 조절하는 경화제를 속경화제와 저속경화제를 혼합하여 주제인 에폭시 수지와 혼합하여 이용함으로써, 다양한 상태를 갖는 다양한 석조문화재의 보존ㆍ복원을 위한 작업자의 작업시간을 적절하게 조절가능하도록 하는 효과를 얻을 수 있고; 주제와 경화제가 혼합된 에폭시 수지 접착제의 초기 점도를 무기첨가제를 혼합할 수 있을 정도로 낮춤으로써, 석조문화재의 보다 완벽한 보존ㆍ복원을 실현할 수 있도록 한 효과를 얻은 수 있다.