폐카본 슬러지로부터 고품위 카본을 회수하는 방법
    1.
    发明公开
    폐카본 슬러지로부터 고품위 카본을 회수하는 방법 无效
    废碳废水中高品质碳的回收方法

    公开(公告)号:KR1020020037532A

    公开(公告)日:2002-05-22

    申请号:KR1020000067490

    申请日:2000-11-14

    CPC classification number: C09C1/56 B09B3/00 Y02W30/522

    Abstract: PURPOSE: A method for recovering high quality carbon from waste carbon sludge is provided, to remove the ash content by 99% or more and the iron content by 100% from waste carbon sludge generated due to the incomplete combustion in a flame reaction of water for producing hydrogen gas. CONSTITUTION: The method comprises the steps of making waste carbon slurry by using waste carbon sludge and water; pulverizing the waste carbon slurry; floatation-treating the pulverized one; ultrasonicating the floated one; and magnetic separating the ultrasonicated product. The concentration of the slurry is 1-5 wt%. Preferably the floatation is carried out by using kerosene as a collector, and Aero Froth 73, MIBC or pine oil as a foaming agent. The magnetic separation is carried out at a slurry concentration of 1-5.5 % with magnetic flux of 1,000-18,000 G.

    Abstract translation: 目的:提供从废碳污泥中回收高质量碳的方法,以除去灰分含量99%以上,铁含量100%,由于在水的火焰反应中不完全燃烧产生的废碳污泥 产生氢气。 构成:该方法包括使用废碳污泥和水制造废碳浆料的步骤; 粉碎废碳浆料; 漂浮处理粉碎的; 超声波漂浮的; 并将超声波产品磁分离。 浆料的浓度为1-5重量%。 优选地,通过使用煤油作为收集器,以及Aero Froth 73,MIBC或松油作为发泡剂来进行浮选。 磁性分离以1-5.5%的浆液浓度进行,磁通量为1,000-18,000G。

Patent Agency Ranking