콘드로이틴황산 또는 아카란황산을 이용한 안정성, 안전성 및 상처치료 효과가 개선된 생체적합성 은나노입자 및 이의 제조방법
    1.
    发明公开
    콘드로이틴황산 또는 아카란황산을 이용한 안정성, 안전성 및 상처치료 효과가 개선된 생체적합성 은나노입자 및 이의 제조방법 无效
    具有改善的稳定性,使用硫酸锡或硫酸锌的安全和治疗效果的生物成分银纳米颗粒及其制备方法

    公开(公告)号:KR1020120137642A

    公开(公告)日:2012-12-24

    申请号:KR1020110056137

    申请日:2011-06-10

    CPC classification number: A61K9/5161 A61K9/06 A61K9/5192 A61K33/38 Y10S514/97

    Abstract: PURPOSE: A silver nanoparticle using chondroitin sulfate or acharan sulfate is provided to suppress bacteria without toxicity and to enable quick wound healing. CONSTITUTION: A biocompatible silver nanoparticle improves safety, stability, and wound healing effect using chondroitin sulfate or acharan sulfate. The size of the silver nanoparticle is 5-50 nm. A method for preparing the silver nanoparticles comprises: a step of dissolving chondroitin sulfate or acharan sulfate in 0.01-2.0 mM of distilled water to prepare a reducing agent solution; a step of dissolving 0.01-10.0 mM nitric acid in distilled water to prepare a nitric acid solution; a step of mixing the reducing agent solution and nitric acid solution to prepare a mixture solution; and a step of reacting the mixture solution in an autoclave or microwave.

    Abstract translation: 目的:提供使用硫酸软骨素或硫酸沙卡糖的银纳米颗粒,以抑制细菌无毒性,并能快速伤口愈合。 构成:生物相容性银纳米颗粒使用硫酸软骨素或硫酸阿卡拉酸提高安全性,稳定性和伤口愈合效果。 银纳米颗粒的尺寸为5-50nm。 制备银纳米颗粒的方法包括:将硫酸软骨素或硫酸阿卡沙溶解在0.01-2.0mM蒸馏水中以制备还原剂溶液的步骤; 将0.01-10.0mM硝酸溶解在蒸馏水中以制备硝酸溶液的步骤; 将还原剂溶液和硝酸溶液混合以制备混合溶液的步骤; 以及在高压釜或微波炉中使混合溶液反应的步骤。

Patent Agency Ranking