폴리아미드 수지의 제조 방법
    1.
    发明公开
    폴리아미드 수지의 제조 방법 有权
    制备聚酰胺树脂的方法

    公开(公告)号:KR1020120113559A

    公开(公告)日:2012-10-15

    申请号:KR1020110031326

    申请日:2011-04-05

    Abstract: PURPOSE: A manufacturing method of polyamide resin is provided to enhance heat resistance and spinning processability by inducing thermal decomposition temperature and degrading dissolution point. CONSTITUTION: A manufacturing method of polyamide resin comprises the following steps: manufacturing a mixture by mixing monomers including 2-pyrrolidone with alkaline catalyst ; and polymerizing the monomers by mixing the mixture with acyl based initiator. The polyamide resin is a homopolymer including 2-pyrrolidone in a polymerized form, or a copolymer including 2-pyrrolidone and C5-7 lactam in a polymerized form. In the first step, the alkaline catalyst is mixed in 2.5-9 parts by mole based on 100.0 parts by mole of the monomer including 2-pyrrolidone. [Reference numerals] (AA) Linear form(inherent); (BB) Linear form(reduced)

    Abstract translation: 目的:提供聚酰胺树脂的制造方法,通过诱导热分解温度和降解溶解点来提高耐热性和纺丝加工性。 构成:聚酰胺树脂的制造方法包括以下步骤:通过将包含2-吡咯烷酮的单体与碱性催化剂混合来制备混合物; 并通过将该混合物与基于酰基的引发剂混合来使单体聚合。 聚酰胺树脂是包含聚合形式的2-吡咯烷酮的均聚物,或聚合形式的包含2-吡咯烷酮和C 5-7内酰胺的共聚物。 在第一步中,基于100.0份(摩尔)包含2-吡咯烷酮的单体,碱性催化剂以2.5-9份(摩尔)相混合。 (AA)线形(固有); (BB)线形(减)

    폴리아미드 수지의 제조 방법
    2.
    发明授权
    폴리아미드 수지의 제조 방법 有权
    制备聚酰胺树脂的方法

    公开(公告)号:KR101355335B1

    公开(公告)日:2014-01-24

    申请号:KR1020110031326

    申请日:2011-04-05

    Abstract: 본 발명은 폴리아미드 수지의 제조 방법에 관한 것으로, 2-피롤리돈을 포함하는 모노머 및 알칼리성 촉매를 혼합하여 혼합물을 제조하는 단계; 및 상기 혼합물 및 아실계 개시제를 혼합하여 2-피롤리돈을 포함하는 모노머를 중합시키는 단계를 포함하는 폴리아미드 수지의 제조 방법을 제공한다. 본 발명의 폴리아미드 수지의 제조 방법은 고흡수성을 유지하면서도 융융점 저하 및 열분해 온도의 상승을 유도하여 방사 가공성 및 내열성이 향상된 폴리아미드 수지를 제조할 수 있고, 기존의 나일론 6 수지 등의 제조 설비를 사용하는 것이 가능하므로 경제적이다.