公开(公告)号:KR1020090099693A
公开(公告)日:2009-09-23
申请号:KR1020080024834
申请日:2008-03-18
Applicant: 성균관대학교산학협력단
CPC classification number: Y02B20/181
Abstract: PURPOSE: A method for manufacturing oxynitride phosphor using a firing apparatus of oxynitride phosphor is provided to prepare oxynitride powder suitable for white LED using a blue LED or ultraviolet-ray LED as a light source. CONSTITUTION: A method for manufacturing oxynitride phosphor using a firing apparatus of oxynitride phosphor comprises the steps of: mixing at least one or a mixture of two kinds or more selected from the group consisting of silicon nitride(Si3N4), aluminum nitride(AlN), gallium nitride(GaN) and boron nitride(BN) to prepare a nitride pellet sintered body; preparing for a burning apparatus and positioning the prepared nitride pellet sintered body at the lower part of a second crucible; mixing silicon nitride, aluminum nitride, M1-containing compound, M2-containing compound, and optionally silicon oxide and aluminum oxide; charging the mixed powder in the nitride pellet sintered body; reducing and heating the burning apparatus filled with the mixed powder; and pulverizing the powder obtained after heat treatment.
Abstract translation: 目的:提供一种使用氮氧化物荧光体的烧制装置制造氧氮化物荧光体的方法,以使用蓝色LED或紫外线LED作为光源制备适用于白色LED的氮氧化物粉末。 构成:使用氮氧化物荧光体的烧制装置制造氮氧化物荧光体的方法包括以下步骤:将选自氮化硅(Si 3 N 4),氮化铝(AlN),氮化铝 氮化镓(GaN)和氮化硼(BN),以制备氮化物颗粒烧结体; 准备燃烧装置并将制备的氮化物颗粒烧结体定位在第二坩埚的下部; 混合氮化硅,氮化铝,含M1化合物,含M2化合物,以及任选的氧化硅和氧化铝; 在氮化物颗粒烧结体中填充混合粉末; 减少和加热填充有混合粉末的燃烧装置; 粉碎热处理后的粉末。
-
公开(公告)号:KR1020090083047A
公开(公告)日:2009-08-03
申请号:KR1020080008981
申请日:2008-01-29
Applicant: 삼성전기주식회사 , 성균관대학교산학협력단
CPC classification number: H05B33/10 , C09K11/574 , C09K11/595 , C09K11/7734 , C09K11/7738 , C09K11/7739 , C09K11/7774 , C09K11/7787 , C09K11/7794 , C09K11/7795 , C09K11/7797
Abstract: A method for preparing oxide nano phosphors is provided to ensure a simple and economical process because of not needing expensive materials and facilities, and to synthesize the oxide nano phosphors with uniform particle size distribution. A method for preparing oxide nano phosphors comprises the steps of preparing a metal precursor solution; impregnating porous polymer materials in the metal precursor solution; and heat-treating the porous polymer material containing the metal precursor solution. The heating process heats the porous polymer material containing the metal precursor solution at a heating rate of 100 ‹C or more per minute to 500 ‹C or more.
Abstract translation: 提供一种制备氧化物纳米磷光体的方法,以确保简单和经济的工艺,因为不需要昂贵的材料和设备,并且合成具有均匀粒度分布的氧化物纳米磷光体。 制备氧化物纳米磷光体的方法包括制备金属前体溶液的步骤; 在金属前体溶液中浸渍多孔聚合物材料; 并对含有金属前体溶液的多孔聚合物材料进行热处理。 加热过程以100℃或更高/分钟的加热速率加热含有金属前体溶液的多孔聚合物材料至500℃以上。
-
公开(公告)号:KR100912176B1
公开(公告)日:2009-08-14
申请号:KR1020070109859
申请日:2007-10-30
Applicant: 성균관대학교산학협력단
Abstract: 본 발명은 PDP(Plasma Display Panel) 보호막용 나노분말의 제조방법에 관한 것으로서, 질산칼슘(Ca(NO
3 )
2 4H
2 O) 및 질산알루미늄(Al(NO
3 )
3 9H
2 O)를 혼합한 금속염 수용액(몰비, 9≤Ca(NO
3 )
2 4H
2 O≤13 : 5≤Al(NO
3 )
3 9H
2 O≤9)을 고분자 소재에 함침시키는 단계; 상기 금속염 수용액이 함침된 고분자 소재를 건조한 후, 열처리하는 단계; 및 열처리하여 수득한 고분자 소재를 분쇄하여, 분말을 수득하는 단계를 포함하는 방법에 관한 것이다.
PDP(Plasma Display Panel), 유전체 보호막 분말, 질산칼슘, 질산알루미늄-
公开(公告)号:KR1020090080680A
公开(公告)日:2009-07-27
申请号:KR1020080006575
申请日:2008-01-22
Applicant: 성균관대학교산학협력단
CPC classification number: C01G23/006 , B82Y30/00 , B82Y40/00 , C01P2004/64
Abstract: Provided is a method for preparing barium titanate nano powder for MLCC(multi layer ceramic capacity) in no need of time-consuming processes such as a mixing, drying, calcining and crushing process. A method for preparing barium titanate nano powder for MLCC(multi layer ceramic capacity) comprises: a first step of preparing a mixed solution of barium metal salt solution and a titanium metal salt solution and dipping into a polymer; a second step of drying the polymer and thermally treating it; and a third step of crushing the thermally treated polymer to obtain powder. The barium metal salt solution represents one material selected from the group consisting of BaCl2, Ba(OH)2, Ba(ClO3)2 and Ba(NO3)2.
Abstract translation: 提供了一种不需要诸如混合,干燥,煅烧和破碎过程的耗时的方法制备用于MLCC的钛酸钡纳米粉末(多层陶瓷容量)的方法。 一种制备用于MLCC的钛酸钡纳米粉末(多层陶瓷容量)的方法包括:制备钡金属盐溶液和钛金属盐溶液的混合溶液并浸渍到聚合物中的第一步骤; 干燥聚合物并对其进行热处理的第二步骤; 以及粉碎所述热处理聚合物以获得粉末的第三步骤。 钡金属盐溶液代表选自BaCl 2,Ba(OH)2,Ba(ClO 3)2和Ba(NO 3)2的一种材料。
-
公开(公告)号:KR101141864B1
公开(公告)日:2012-05-08
申请号:KR1020080024834
申请日:2008-03-18
Applicant: 성균관대학교산학협력단
CPC classification number: Y02B20/181
Abstract: 본 발명은 청색 발광 다이오드 또는 자외선 발광 다이오드를 광원으로 하는 백색 발광 다이오드의 형광체에 적용할 수 있는 산질화물 분말의 제조를 위한 소성 장치를 이용한 산질화물 분말의 제조 방법에 관한 것이다. 본 발명에 따른 소성 장치는 안정적인 재현성과 양산성이 우수한 산질화물 분말의 제조가 가능하다. 또한 본 발명의 제조 방법에 따라 제조된 산질화물 분말은 백색 발광 다이오드의 형광체에 적용 가능한 적당한 입도를 지니며, 표면 결함이 없고, 발광 특성이 우수한 장점을 지닌다.
산질화물 형광체, 소성장치, 사이알론, 발광특성-
公开(公告)号:KR1020090044012A
公开(公告)日:2009-05-07
申请号:KR1020070109859
申请日:2007-10-30
Applicant: 성균관대학교산학협력단
Abstract: 본 발명은 PDP(Plasma Display Panel) 보호막용 나노분말의 제조방법에 관한 것으로서, 질산칼슘(Ca(NO
3 )
2 4H
2 O) 및 질산알루미늄(Al(NO
3 )
3 9H
2 O)를 혼합한 금속염 수용액(몰비, 9≤Ca(NO
3 )
2 4H
2 O≤13 : 5≤Al(NO
3 )
3 9H
2 O≤9)을 고분자 소재에 함침시키는 단계; 상기 금속염 수용액이 함침된 고분자 소재를 건조한 후, 열처리하는 단계; 및 열처리하여 수득한 고분자 소재를 분쇄하여, 분말을 수득하는 단계를 포함하는 방법에 관한 것이다.
PDP(Plasma Display Panel), 유전체 보호막 분말, 질산칼슘, 질산알루미늄-
公开(公告)号:KR101530671B1
公开(公告)日:2015-06-23
申请号:KR1020080008981
申请日:2008-01-29
Applicant: 삼성전기주식회사 , 성균관대학교산학협력단
CPC classification number: H05B33/10 , C09K11/574 , C09K11/595 , C09K11/7734 , C09K11/7738 , C09K11/7739 , C09K11/7774 , C09K11/7787 , C09K11/7794 , C09K11/7795 , C09K11/7797
Abstract: (c) 상기금속전구체용액을머금은다공성고분자물질을열처리하는단계를포함하는산화물나노형광체제조방법으로서, 상기 (c) 단계의열처리는상기금속전구체용액을머금은다공성고분자물질을분당 100℃이상의고속의승온속도로 500℃이상으로가열하여열처리하는것을특징으로하는산화물나노형광체제조방법을제공한다.
-
-
-
-
-
-