Abstract:
A film consisting essentially of a continuous phase linear polyester matrix having dispersed therein a non-crosslinked random SAN-polymer and dispersed or dissolved therein at least one ingredient from the group of ingredients consisting of inorganic opacifying pigments, whitening agents, colorants, UV-absorbers, light stabilizers, antioxidants and flame retardants, wherein the film is white, microvoided, non-transparent and axially stretched; the linear polyester matrix has monomer units consisting essentially of at least one aromatic dicarboxylic acid, at least one aliphatic diol and optionally at least one aliphatic dicarboxylic acid; and the weight ratio of the linear polyester to the non-crosslinked SAN-polymer is in the range of 2.0:1 to 19.0:1, wherein one of the said at least one aliphatic dimethylene monomer units is selected from the group consisting of neopentylene and 1, 4-cyclohexanedimethylene in a concentration of 30 mole % or less of all aliphatic dimethylene monomer units; the use of the film as or in synthetic paper; an image recording element comprising the film; a process for the preparing of the non-transparent microvoided axially stretched film; and a process for obtaining a transparent pattern therewith.
Abstract:
연속상으로서 선형 폴리에스테르 및 유리 전이 온도가 연속상의 유리 전이 온도보다 높은, 하나 이상의 사슬-중합 블록을 포함하고 상기 연속상에 균일하게 분산된 비결정질 고분자 및 이소태틱 폴리(4-메틸-1-펜텐) 을 포함하는 불투명한 미세기공 2축 연신 자가-지지성 비적층 중합체성 필름으로서, 상기 선형 폴리에스테르가 본질적으로 방향족 디카르복실레이트 및 지방족 디메틸렌 단량체 단위로 이루어져 있고, 상기 균일하게 분산된 비결정질 고분자와 이소태틱 폴리(4-메틸-1-펜텐) 의 필름 중의 조합 농도가 5 내지 35 중량%인 필름; 상기 불투명한 미세기공 2축 연신 필름의 합성지에서의 용도; 상기 불투명한 미세기공 2축 연신 필름을 포함하는 화상 기록 소자; 및 상기 불투명한 미세기공 2축 연신 필름에 압력을 가하여 임의로 보충된 열의 이미지 형성 방식 (image-wise) 적용 단계를 포함하는 투명 패턴의 제조 방법.
Abstract:
A non-transparent microvoided biaxially stretched self-supporting non-laminated polymeric film, the film comprising linear polyester as a continuous phase and dispersed uniformly therein an amorphous high polymer comprising at least one chain-polymerized block with a higher glass transition temperature than the glass transition temperature of the continuous phase and isotactic poly (4-methyl-1-pentene), wherein the linear polyester consists essentially of aromatic dicarboxylate and aliphatic dimethylene monomer units, wherein the combined concentration of the uniformly dispersed amorphous high polymer and isotactic poly (4-methyl-1-pentene) in the film is 5 to 35% by weight; the use of the above-described non-transparent microvoided biaxially stretched film in synthetic paper; an image recording element comprising the above-described non-transparent microvoided biaxially stretched film; and a process for producing a transparent pattern comprising the step of : image-wise application of heat optionally supplemented by the application of pressure to the above-described non-transparent microvoided biaxially stretched film.