하드 코팅액 및 하드 코팅 필름
    5.
    发明公开
    하드 코팅액 및 하드 코팅 필름 有权
    硬涂层液和薄膜

    公开(公告)号:KR1020110023362A

    公开(公告)日:2011-03-08

    申请号:KR1020090081193

    申请日:2009-08-31

    Abstract: PURPOSE: A hard coating film is provided to ensure high antistatic property and transmission without the formation of an antistatic layer on a hard coating ladyer. CONSTITUTION: A hard coating solution comprises zinc oxide nanorods doped with aluminum, and further one or more of heat or ultraviolet curable resin, curing initiators, and solvent. The zinc oxide nanorods doped with aluminum ensures conductivity and has the thickness of 2 nm ~ 1 μm and the length of 10 nm ~ 10 μm. A hard coating film(100) includes a base film(110), and a coating layer(120) formed with the antistatic hard coating solution.

    Abstract translation: 目的:提供硬涂层,以确保高抗静电性和透光性,而不会在硬涂层瓢虫上形成抗静电层。 构成:硬涂层溶液包含掺杂有铝的氧化锌纳米棒,还有一种或多种加热或紫外线固化树脂,固化引发剂和溶剂。 掺有铝的氧化锌纳米棒确保导电性,厚度为2nm〜1μm,长度为10nm〜10μm。 硬涂膜(100)包括基膜(110)和形成有抗静电硬涂层溶液的涂层(120)。

    산화아연 나노막대 제조 방법
    6.
    发明公开
    산화아연 나노막대 제조 방법 有权
    制备ZNO NANOROD的方法

    公开(公告)号:KR1020100065650A

    公开(公告)日:2010-06-17

    申请号:KR1020080124081

    申请日:2008-12-08

    Inventor: 임상규 황성호

    CPC classification number: C01G9/02 B82Y30/00 B82Y40/00 C01P2004/16

    Abstract: PURPOSE: A method for manufacturing zinc oxide nanorod is provided to dope a conductive metal atom to the zinc oxide nanorod by wet method using chemical characteristic. CONSTITUTION: A method for manufacturing zinc oxide nanorod comprises: a preparing a first emulsion solution containing zinc precursor, dopping metal precursor, emulsifier, and organic solvent; a step of inputting redundant to the first emulsion solution to prepare a second emulsion solution; a step of heating the second emulsion at 20-300°C to obtain a third emulsion solution; and a step of centrifuging or performing thermal treatment of the third emulsion solution.

    Abstract translation: 目的:提供一种制造氧化锌纳米棒的方法,通过使用化学特性的湿法将导电金属原子掺杂到氧化锌纳米棒上。 构成:制造氧化锌纳米棒的方法包括:制备含有锌前体,掺杂金属前体,乳化剂和有机溶剂的第一乳液; 向第一乳液溶液输入冗余以制备第二乳液的步骤; 在20-300℃下加热第二乳液以获得第三乳液的步骤; 以及对第三乳液溶液进行离心或进行热处理的步骤。

    기능성 고분자 소재 및 이의 제조 방법
    7.
    发明授权
    기능성 고분자 소재 및 이의 제조 방법 有权
    기능성고분자소재및이의제조방법

    公开(公告)号:KR100727086B1

    公开(公告)日:2007-06-13

    申请号:KR1020060066558

    申请日:2006-07-14

    Abstract: Provided are functional polymer materials, which are applicable to ultraviolet-blocking, electromagnetic-shielding, deodorant, and antibacterial products, and a manufacturing method thereof, whereby the functional polymer materials are stably produced. The functional polymer materials are manufactured by the steps of: mixing and kneading a semiconductive metal oxide with a polymeric resin to prepare a semiconductive metal oxide-containing polymeric resin composition; molding the polymeric resin composition into a polymer material having a predetermined shape; and photo-depositing metal nanoparticles on the polymer material to support the metal nanoparticles on the metal oxide particles distributed on the surface of the polymeric material.

    Abstract translation: 提供适用于紫外线阻断,电磁屏蔽,除臭和​​抗菌产品的功能性高分子材料及其制造方法,由此稳定地制造功能性高分子材料。 功能性高分子材料通过以下步骤制造:将半导体金属氧化物与聚合物树脂混合并捏合以制备含半导体金属氧化物的聚合物树脂组合物; 将聚合物树脂组合物模塑成具有预定形状的聚合物材料; 以及在聚合物材料上光沉积金属纳米粒子以将金属纳米粒子支撑在分布在聚合物材料表面上的金属氧化物粒子上。

    산화인듐주석 로드의 제조방법
    9.
    发明授权
    산화인듐주석 로드의 제조방법 有权
    氧化铅填料的制备方法

    公开(公告)号:KR101401089B1

    公开(公告)日:2014-05-30

    申请号:KR1020110120034

    申请日:2011-11-17

    Abstract: 본 발명의 일 측에 따른 산화인듐주석 로드의 제조방법은 디메틸포름아미드(dimethylformamide) 및 알콜의 혼합비율을 달리함으로써 길이와 두께의 비인 어스펙트비(aspect ratio)가 조절된 산화인듐주석 로드를 제조할 수 있다. 즉, 산화인듐주석 로드 제조시, 디메틸포름아미드와 알콜을 특정 비율로 혼합함으로써 제조되는 산화인듐주석의 두께와 길이를 쉽게 조절할 수 있다. 또한, 본 발명의 일 측에 따라 인듐과 주석에 고분자를 배위시킨 화합물로부터 제조되는 산화인듐주석 로드는 전자 재료, 센서 소재 등 다양한 소재 분야에 적용될 수 있다.

    구리 프탈로시아닌이 부착된 나노구조체의 제조방법 및 산화 구리 입자가 부착된 나노구조체의 제조방법
    10.
    发明授权
    구리 프탈로시아닌이 부착된 나노구조체의 제조방법 및 산화 구리 입자가 부착된 나노구조체의 제조방법 有权
    铜酞菁涂层纳米结构材料和氧化铜涂层纳米结构材料的制造方法

    公开(公告)号:KR101314744B1

    公开(公告)日:2013-10-08

    申请号:KR1020110120182

    申请日:2011-11-17

    Abstract: 본 발명은 구리 프탈로시아닌 또는 산화구리 입자가 부착된 나노구조체 분말 제조방법에 관한 것으로, (a) 합성반응기에 에틸렌 글리콜 용매와 금속, 금속산화물 및 반도체 나노구조체 중 적어도 어느 하나를 투입하여 교반하는 단계; (b) 4-nitrophthalonitrile, copper(II) acetate monohydrate 및 ammonium molybdate을 순서대로 상기 합성반응기에 투입하여 교반하는 단계; (c) 상기 (b) 단계의 용액을 교반하면서, 상기 용액을 가열하여 구리 프탈로시아닌이 부착된 나노구조체를 포함하는 용액을 형성하는 단계; (d) 상기 (c) 단계에서 형성된 용액을 원심분리 및 수세건조하여 구리 프탈로시아닌이 부착된 나노구조체 분말을 형성하는 단계; 및 (e) 구리 프탈로시아닌이 부착된 나노구조체 분말을 소성하여 산화구리 입자가 부착된 나노구조체 분말을 형성하는 단계를 포함한다.
    이와 같은 본 발명은 구리 프탈로시아닌 및 산화구리 입자가 피복된 나노구조체의 제조방법은 센서 소재 및 전자재료 등에 적용될 수 있는 합성방법을 제공할 수 있고, 합성시 구리 프탈로시아닌 전구체의 양을 조절함으로 구리 프탈로시아닌 및 산화구리 입자의 피복양을 쉽게 조절할 수 있는 합성법으로 발명의 효과를 제공한다.