무기계 나노입자를 수계 매질에 분산시키는 생체적합성분산 안정화제
    1.
    发明公开
    무기계 나노입자를 수계 매질에 분산시키는 생체적합성분산 안정화제 无效
    用于将无机纳米颗粒分解成水溶液的生物可溶性悬浮稳定剂

    公开(公告)号:KR1020090038337A

    公开(公告)日:2009-04-20

    申请号:KR1020070103783

    申请日:2007-10-15

    CPC classification number: C07F9/2408 C07F9/2458

    Abstract: A bio-compatible suspension stabilizer for dispersing inorganic nano-particles in an aqueous medium is provided to modify surfaces of the inorganic nano-particles to have hydrophilic properties and easily allow ligand having in vivo activity to be accepted. A bio-compatible suspension stabilizer for dispersing inorganic nano-particles in an aqueous medium is phosphin oxide represented by the formula 1. A method for producing the phosphin oxide comprises the following steps of: dissolving a bio-compatible polymer in an organic solvent to prepare a bio-compatible polymer organic solvent; adding phosphin oxide having a leaving group into the prepared bio-compatible polymer organic solvent to bond the phosphin oxide with the bio-compatible polymer; reacting a compound having a functional group in order to induce the functional group which can be bonded with the functional ligand at a position of the leaving group of the bio-compatible polymer.

    Abstract translation: 提供了用于将无机纳米颗粒分散在水性介质中的生物相容性悬浮稳定剂,以将无机纳米颗粒的表面改性为具有亲水性,并容易地允许具有体内活性的配体。 用于将无机纳米颗粒分散在水性介质中的生物相容的悬浮稳定剂是由式1表示的氧化膦。氧化膦的制备方法包括以下步骤:将生物相容性聚合物溶解在有机溶剂中以制备 生物相容性聚合物有机溶剂; 在制备的生物相容性聚合物有机溶剂中加入具有离去基团的氧化膦,将氧化膦与生物相容的聚合物键合; 使具有官能团的化合物反应以诱导可在生物相容性聚合物的离去基团的位置处与官能配体结合的官能团。

    산화금속 중공 나노캡슐 및 이의 제조방법
    2.
    发明授权
    산화금속 중공 나노캡슐 및 이의 제조방법 失效
    金属氧化物空心纳米胶囊及其制备方法

    公开(公告)号:KR100846839B1

    公开(公告)日:2008-07-16

    申请号:KR1020060122077

    申请日:2006-12-05

    Abstract: 본 발명은 수계에 잘 분산되는 산화금속 중공 나노캡슐의 제조방법 및 이로부터 제조된 산화철 중공 나노캡슐에 관한 발명이다.
    본 발명에 따른 산화금속 중공 나노캡슐의 제조방법은 금속 옥시수산화물 입자를 수계에 분산시킨 후 상기 금속 옥시수산화물 입자 상에 실리카 코팅층을 형성한 후 이를 열처리하여 실리카 코팅층 내부에 중공형의 산화금속층이 형성한 후 실리카를 제거하는 과정을 통해 이루어지는 것을 특징으로 한다. 본 발명의 제조방법에 의해 제조된 산화금속 중공 나노캡슐은 수계 분산성이 우수하고 균일한 입도분포를 가질 뿐만아니라 내부 중공에 생리 활성 물질을 담지할 수 있는 효과가 있다.
    또한, 본 발명에 따른 산화철 나노캡슐은 100 m
    2 /g 이상의 큰 표면적과 좁은 분포의 중형 기공(meso pore)을 지니고 있어 생리 활성 물질의 담지가 가능하며, 약물전달 같은 생명의학적 응용, 가스센서(gas sensor), 리튬 이온전지(Li ion battery) 등 광범위한 산업적 응용의 가능성을 기대할 수 있다.
    금속 옥시수산화물, 중공 나노캡슐, 산화철

    블록 공중합체를 이용한 팔라듐 나노 입자의 제조방법
    3.
    发明授权
    블록 공중합체를 이용한 팔라듐 나노 입자의 제조방법 有权
    使用三嵌段共聚物制备钯纳米粒子的方法

    公开(公告)号:KR100809056B1

    公开(公告)日:2008-03-03

    申请号:KR1020060066439

    申请日:2006-07-14

    Abstract: 본 발명은 수용액 상에서 블록 공중합체를 이용하여 균일한 팔라듐 나노 입자를 제조하는 방법에 관한 것이다.
    본 발명에 따른 제조방법에 의해 제조된 팔라듐 나노 입자는 그 조건에 따라서 몇 나노미터 에서 몇 십 나노미터 크기를 보이고 있으며, 입자의 크기 분포가 매우 균일하여 화학 반응의 촉매로 사용되어 높은 촉매 활성을 나타내는 장점이 있다.
    블록 공중합체, 팔라듐 나노입자, 촉매

    블록 공중합체를 이용한 팔라듐 나노 입자의 제조방법
    4.
    发明公开
    블록 공중합체를 이용한 팔라듐 나노 입자의 제조방법 有权
    使用三嵌段共聚物制备钯纳米微粒的方法

    公开(公告)号:KR1020080006996A

    公开(公告)日:2008-01-17

    申请号:KR1020060066439

    申请日:2006-07-14

    Abstract: A preparation method of palladium nanoparticles is provided to obtain uniform size nanoparticles through a simplified process and at the same time, to diversify size and shape of the nanoparticles. A preparation method of palladium nanoparticles includes the steps of: dissolving a polyethylene oxide polypropyleneoxide-polyethyleneoxide block copolymer in a distilled water to produce a triblock copolymer solution; and adding and stirring (or agitating) a palladium (Pd) precursor compound into the triblock copolymer solution at 0.2-1 mole ratio. Further, the palladium precursor compound is added additionally to adjust size and shape of particles, and, an acid or a base is added into the triblock copolymer solution to adjust pH thereof.

    Abstract translation: 提供钯纳米颗粒的制备方法以通过简化的方法获得均匀的尺寸的纳米颗粒,并且同时使纳米颗粒的尺寸和形状多样化。 钯纳米颗粒的制备方法包括以下步骤:将聚环氧乙烷聚环氧丙烷 - 聚环氧乙烷嵌段共聚物溶解在蒸馏水中以产生三嵌段共聚物溶液; 并以0.2-1摩尔比将钯(Pd)前体化合物加入并搅拌(或搅拌)到三嵌段共聚物溶液中。 此外,另外添加钯前体化合物以调节颗粒的尺寸和形状,并且在三嵌段共聚物溶液中加入酸或碱以调节其pH。

    기판상에 양자점을 배열하는 방법 및 장치
    5.
    发明公开
    기판상에 양자점을 배열하는 방법 및 장치 无效
    用于在基板上排列量子点的方法和装置

    公开(公告)号:KR1020020094479A

    公开(公告)日:2002-12-18

    申请号:KR1020010032716

    申请日:2001-06-12

    Abstract: PURPOSE: A method and an apparatus for arraying quantum dots on a substrate are provided to array uniformly the quantum dots on the substrate by using colloid solution with density of nanosphere. CONSTITUTION: A bath(1) is used for storing colloidal solution. The bath(1) is installed in the inside of a storage tank(7). The bath(1) is moved by vibration of a motor(2). A substrate(5) is dipped into the bath(1) when the storage tank(7) is moved to an upper direction. The substrate(5) is drawn from the bath(1) when the storage tank(7) is moved to a lower direction. A motor(2) has a speed range of 0.01 to 0.1 mm/sec. A rotator(3) is installed on a substrate holder in order to an angle of the substrate(5). A heating portion(6) such as a lamp is located beside the bath(1) in order to heat coated solution. A supplier(4) is used for applying an electric field or a magnetic field.

    Abstract translation: 目的:提供一种在基板上排列量子点的方法和装置,通过使用纳米球密度的胶体溶液均匀地排列在基板上的量子点。 规定:使用浴(1)保存胶体溶液。 浴(1)安装在储罐(7)的内部。 浴缸(1)通过电动机(2)的振动而移动。 当储存箱(7)向上方移动时,将基板(5)浸入槽(1)中。 当储存罐(7)向下方移动时,基板(5)从槽(1)中被拉出。 电机(2)的转速范围为0.01〜0.1mm / sec。 旋转体(3)以基板(5)的角度安装在基板支架上。 为了加热涂布的溶液,诸如灯的加热部分(6)位于浴(1)旁边。 供应商(4)用于施加电场或磁场。

    세륨 산화물 나노 입자 제조 방법
    8.
    发明授权
    세륨 산화물 나노 입자 제조 방법 有权
    制备氧化铈纳米粒子的方法

    公开(公告)号:KR101356870B1

    公开(公告)日:2014-01-29

    申请号:KR1020060096792

    申请日:2006-09-30

    Inventor: 현택환 유태경

    Abstract: 본 발명은 유수성 또는 무수성 졸-겔 반응을 통하여 세륨산화물(CeO
    2 ) 나노 입자를 제조하는 새로운 방법에 관한 것이다. 보다 구체적으로는, 본 발명은 졸-겔 반응을 통하여 세륨산화물(CeO
    2 ) 나노 입자를 제조함에 있어서, i) 세륨 전구체와 계면활성제 혼합물 또는 세륨전구체와 계면활성제 및 유기 용매의 혼합물을 가열하여 세륨-계면활성제 복합체를 생성시키는 단계; 그리고 ii) 상기 세륨-계면활성제 복합체 혼합물에 에테르계 화합물을 첨가하고 가열하여 혼합물의 온도를 100℃ 내지 360℃ 범위로 유지하는 단계를 포함하는 것을 특징으로 하는 세륨 산화물 나노 입자 제조 방법에 대한 것이다.
    세리아, 나노입자

    금속-금속산화물 이종접합 나노입자 제조 방법
    10.
    发明公开
    금속-금속산화물 이종접합 나노입자 제조 방법 无效
    合成金属氧化物异构体纳米粒子的方法

    公开(公告)号:KR1020090093702A

    公开(公告)日:2009-09-02

    申请号:KR1020080019389

    申请日:2008-02-29

    Abstract: A method for manufacturing a metal oxide-metal heterojunction nanoparticle is provided to vary the shapes of metal oxide-metal heterojunction nanoparticles such as a dumbbell shape and a flower shape. A method for manufacturing a metal oxide-metal heterojunction nanoparticle comprises the following steps of: mixing a metal precursor solution and an organic acid metal salt composite solution, wherein the metal precursor solution consists of a metal precursor, a surfactant and an organic solvent and the organic acid metal salt composite solution consists of an organic acid metal salt composite, the surfactant and the organic solvent; and pyrolyzing the mixture. The metal precursor is selected from the group consisting of HAuCl4.nH2O, H2PtCl6.nH2O, NiCl2 and AgNO3. The surfactant is selected among C1-C18 alkyl amines.

    Abstract translation: 提供金属氧化物 - 金属异质结纳米颗粒的制造方法,以改变金属氧化物 - 金属异质结纳米颗粒的形状,例如哑铃形状和花形状。 金属氧化物 - 金属异质结纳米颗粒的制造方法包括以下步骤:将金属前体溶液和有机酸金属盐复合溶液混合,其中金属前体溶液由金属前体,表面活性剂和有机溶剂组成, 有机酸金属盐复合溶液由有机酸金属盐复合物,表面活性剂和有机溶剂组成; 并热解混合物。 金属前体选自HAuCl4.nH2O,H2PtCl6·6H2O,NiCl2和AgNO3。 表面活性剂选自C1-C18烷基胺。