비소제거를 통한 고순도 몰리브덴 산물 제조방법
    2.
    发明授权
    비소제거를 통한 고순도 몰리브덴 산물 제조방법 有权
    用于去除产生高纯度多晶硅的方法

    公开(公告)号:KR101048293B1

    公开(公告)日:2011-07-13

    申请号:KR1020100018443

    申请日:2010-03-02

    CPC classification number: C02F1/26 C02F1/5272 C02F1/54

    Abstract: PURPOSE: A method for manufacturing molybdenum is provided to obtain highly purified molybdenum by collecting molybdenum and eliminating arsenic from the molybdenum through a solvent extraction process. CONSTITUTION: An amine-based organic solvent is added in wastewater containing molybdenum and arsenic. Molybdenum ions are collected by the amine-based organic solvent. Ammonia water is added to back-extract the molybdenum ions(S20). Magnesium salt is added to precipitate an arsenic compound. A solid-liquid separating process is implemented. Acid is added to the liquid obtained through the solid-liquid separating process, and highly purified molybdenum is collected(S50).

    Abstract translation: 目的:提供钼的制造方法,通过收集钼并通过溶剂萃取方法从钼中除去砷来获得高纯度的钼。 构成:在含有钼和砷的废水中加入胺类有机溶剂。 钼离子由胺类有机溶剂收集。 加入氨水以提取钼离子(S20)。 加入镁盐以沉淀砷化合物。 实行固液分离处理。 将酸加入到通过固液分离过程获得的液体中,并收集高纯度的钼(S50)。

    몰리브덴 제조 공정에서 발생된 폐수에 잔류하는몰리브덴과 구리의 회수 방법
    3.
    发明公开
    몰리브덴 제조 공정에서 발생된 폐수에 잔류하는몰리브덴과 구리의 회수 방법 有权
    使用溶剂从废水中提取钼和铜产品的方法

    公开(公告)号:KR1020090090215A

    公开(公告)日:2009-08-25

    申请号:KR1020080015534

    申请日:2008-02-20

    CPC classification number: Y02P10/234 C22B7/00 C22B3/00 C22B15/00 C22B34/34

    Abstract: A method for collecting copper and molybdenum remaining in effluent generated in a manufacturing process is provided to reduce mineral import by recycling the copper and the molybdenum with a counter-current extraction mode. A method for collecting copper and molybdenum remaining in effluent generated in a manufacturing process includes the following steps of: collecting a molybdenum ion in an organic solvent by adding an Amine series organic solvent(S10); separating the collected organic solvent from the effluent(S20); performing a counter-current extraction process of the molybdenum ion by adding an ammonia solution(S30); and collecting molybdenum by adding acid on the ammonia solution(S40).

    Abstract translation: 提供一种用于收集在制造过程中产生的流出物中剩余的铜和钼的方法,以通过以逆流提取模式回收铜和钼来减少矿物进口。 在制造过程中产生的废水中残留的铜和钼的收集方法包括以下步骤:通过加入胺系列有机溶剂在有机溶剂中收集钼离子(S10); 从流出物中分离收集的有机溶剂(S20); 通过加入氨溶液进行钼离子的逆流提取处理(S30); 并通过在氨溶液中加酸收集钼(S40)。