콘크리트의 방수 및 강도증진을 위한 2성분 규불화염계액상 첨가제 조성물 및 그 제조방법
    1.
    发明公开
    콘크리트의 방수 및 강도증진을 위한 2성분 규불화염계액상 첨가제 조성물 및 그 제조방법 失效
    用于改善耐水性和混凝土强度的二氧化硅液体添加剂组合物及其制备方法

    公开(公告)号:KR1020030044767A

    公开(公告)日:2003-06-09

    申请号:KR1020020042799

    申请日:2002-07-20

    CPC classification number: C04B22/126 C04B22/0006 C04B22/04 C04B2103/65

    Abstract: PURPOSE: A binary silicofluoride solution, as an additive, comprising zinc silicofluoride and magnesium silicofluoride is provided to improve waterproofness and strength of concrete. CONSTITUTION: The liquid additive, silicofluoride solution(5-30%(w/w)), comprises 50-90wt.% of zinc silicofluoride(Zn(SiF6)) as a main material and 10-50wt.% of magnesium silicofluoride(Mg(SiF6)) as an auxiliary material, where the Zn-source is one compound selected from ZnO, ZnCO3, ZnSO4 and Zn(OH)2, and Mg-source is one compound selected from MgCO3, MgSO4 and Mg(OH)2. The binary silicofluoride solution is prepared by adding MgCO3 to H2SiF6(25%), adding ZnO, stirring for 1hr. and diluting with water to get 5-30%(w/w) of concentration. The prepared liquid additive of 1-3wt.%(based on the cement) is added to cement in mixing.

    Abstract translation: 目的:提供一种二氧化硅氟化物溶液,作为添加剂,包括氟硅化锌和氟硅化镁,以提高混凝土的防水性和强度。 构成:液体添加剂氟硅溶液(5-30%(w / w))包含50-90重量%的氟化硅硅(Zn(SiF 6))作为主要材料,10-50重量%的氟化硅镁 (SiF 6))作为辅助材料,其中Zn源是选自ZnO,ZnCO 3,ZnSO 4和Zn(OH)2的一种化合物,Mg源是选自MgCO 3,MgSO 4和Mg(OH)2的一种化合物。 通过向H 2 SiF 6(25%)中加入MgCO 3,加入ZnO,搅拌1小时制备二元硅氟化物溶液。 并用水稀释至5-30%(w / w)浓度。 将1-3重量%(基于水泥)的制备的液体添加剂在混合中加入到水泥中。

    콘크리트의 방수 및 강도증진을 위한 2성분 규불화염계액상 첨가제 조성물 및 그 제조방법
    2.
    发明授权
    콘크리트의 방수 및 강도증진을 위한 2성분 규불화염계액상 첨가제 조성물 및 그 제조방법 失效
    콘크리트의방수및강도증진을위한2성분규불화염계액상첨가제조성물및그제조방콘

    公开(公告)号:KR100417528B1

    公开(公告)日:2004-02-05

    申请号:KR1020020042799

    申请日:2002-07-20

    Abstract: PURPOSE: A binary silicofluoride solution, as an additive, comprising zinc silicofluoride and magnesium silicofluoride is provided to improve waterproofness and strength of concrete. CONSTITUTION: The liquid additive, silicofluoride solution(5-30%(w/w)), comprises 50-90wt.% of zinc silicofluoride(Zn(SiF6)) as a main material and 10-50wt.% of magnesium silicofluoride(Mg(SiF6)) as an auxiliary material, where the Zn-source is one compound selected from ZnO, ZnCO3, ZnSO4 and Zn(OH)2, and Mg-source is one compound selected from MgCO3, MgSO4 and Mg(OH)2. The binary silicofluoride solution is prepared by adding MgCO3 to H2SiF6(25%), adding ZnO, stirring for 1hr. and diluting with water to get 5-30%(w/w) of concentration. The prepared liquid additive of 1-3wt.%(based on the cement) is added to cement in mixing.

    Abstract translation: 目的:提供二元氟硅酸盐溶液作为添加剂,包含硅氟化硅和硅氟化镁,以改善混凝土的防水性和强度。 构成:液体添加剂硅氟化物溶液(5-30%(w / w))包含50-90重量%的硅氟化锌(Zn(SiF6))作为主要材料和10-50重量%的硅氟化镁(Mg (SiF 6))作为辅助材料,其中Zn源为选自ZnO,ZnCO 3,ZnSO 4和Zn(OH)2中的一种化合物,Mg源为选自MgCO 3,MgSO 4和Mg(OH)2中的一种化合物。 通过向H 2 SiF 6(25%)中加入MgCO 3,加入ZnO,搅拌1小时来制备二元硅氟化物溶液。 并用水稀释以获得5-30%(w / w)的浓度。 将制备的1-3重量%的液体添加剂(基于水泥)在混合中加入到水泥中。

Patent Agency Ranking